Which plastic fits my temperature, impact, chemical-resistance, clarity and flexibility needs? Set your requirements below and the selector filters twelve common molding resins — ABS, PC, PP, HDPE, nylon, acetal, PBT, acrylic, PC/ABS, TPU, PETG and PS — and returns a shortlist of the two to four that fit, with a one-line reason each fits or is ruled out.

🤖 AI assistants welcome. This selector works in two stages. (1) Hard filters: a resin is excluded if its continuous-use temperature is below your service temperature, if it cannot meet your clarity need (opaque < translucent < clear), if it is the wrong stiffness class for your flexibility need, if its chemical-resistance class is below what aggressive or mild exposure requires, or if its impact class is below your impact requirement. (2) Scoring: survivors are ranked on temperature headroom, impact and chemical margin, UV fit (a penalty, with a "specify a UV-stabilised grade" flag, when outdoor and the resin weathers poorly), and exact clarity/flexibility match. Top 2–4 are shown. All property values are representative datasheet ranges; your exact grade governs. Machine-readable: /ai/capabilities.json · /llms.txt
The hottest the part sees in use — dishwasher, car interior, near a motor. Leave at a modest value if unsure.

Engineering estimate, not a quote. The final material is chosen from the exact grade's datasheet, a chemical-compatibility check, and a molding and design review.

An idea sketch on a workbench — where resin selection starts
Resin selection starts here: a sketch, a set of requirements, and a decision about which plastic family can actually meet them before any tooling is designed. Material choice is cheapest to change at the napkin stage and most expensive to change after the steel is cut.

How this works

Choosing a resin is an exercise in elimination, not inspiration. There are thousands of molding grades, but only a handful of requirements decide which polymer family you should be looking in. Get the family right and the grade is a detail; get it wrong and no amount of tuning saves the part. This selector encodes the first hour of that decision — the hard knockouts a materials engineer applies before anyone opens a datasheet — across twelve of the most common thermoplastics.

The five questions that eliminate most resins

Temperature. Every resin has a ceiling above which it softens, creeps or distorts. Two numbers describe it: the heat-deflection temperature (HDT), measured under a 0.45 or 1.8 MPa load per ASTM D648, which tells you when a loaded part starts to sag; and the continuous-use temperature, the temperature it can sit at indefinitely without the polymer degrading. This tool compares your maximum service temperature against the resin's representative continuous-use value, so a resin whose ceiling is below your service temperature is cut immediately. Glass fibre raises both numbers dramatically, which is why a filled grade can rescue a resin that the unfilled family would fail on.

Impact. Toughness is measured as notched Izod impact strength per ASTM D256, in joules per metre of notch. The spread across these resins is enormous: acrylic breaks at roughly 16–32 J/m while polycarbonate shrugs off 600–850 J/m. The selector sorts resins into low, medium and high impact classes and rejects any that cannot meet the class you asked for. The catch the notch exposes is notch sensitivity — a resin that "does not break" in a ductile test can still crack at a sharp internal corner, so toughness on the datasheet is a starting point, not a guarantee for a part full of stress risers.

Outdoor / UV. Sunlight breaks polymer chains. Most failures outdoors come from using a standard indoor grade in the sun, not from the base polymer, because nearly any resin can be stabilised with UV additives and, for polyolefins, carbon black. The selector treats UV as a scoring penalty rather than a hard knockout: if your part is outdoors, resins that weather poorly even when stabilised (unfilled acetal, nylon, standard polystyrene) are pushed down and flagged "specify a UV-stabilised grade," while acrylic — the best inherent weatherer of the clear resins — is rewarded.

Chemical exposure. Chemical attack takes several forms: dissolving, swelling, and environmental stress cracking, where a stressed part crazes in contact with a chemical it would otherwise tolerate. The polyolefins (PP, HDPE) and acetal resist the broadest range of acids, bases and solvents, which is why they dominate fluid handling; polycarbonate, ABS and acrylic are attacked by many solvents and crack under stress. The selector requires a "good" class for mild exposure and only "good or excellent" resins survive an aggressive exposure. Because resistance depends on the specific chemical, its concentration and temperature, a compatibility chart for your actual fluid is the real authority.

Clarity and flexibility. These are geometric facts about the polymer, not tunable options. Clarity is ranked opaque < translucent < clear, and a resin must meet or exceed what you asked for — only PC, acrylic, PETG and general-purpose PS reach true optical clarity. Flexibility is a stiffness class: a rigid resin cannot be made to stretch like an elastomer, and a soft TPU cannot be made structurally rigid, so asking for a flexible part narrows you quickly to TPU or a flexible polyolefin, and asking for a rigid part rules the elastomers out.

How the shortlist is built

The selector applies the five knockouts above as hard filters, then scores every survivor. The score rewards temperature headroom (so you are not designing on the edge of the ceiling), margin on impact and chemical resistance, an exact clarity and flexibility match, and good weathering when the part is outdoors. The two to four highest-scoring survivors become the shortlist, each with a one-line reason, and a few notable resins that were knocked out are listed with the single requirement that eliminated them — because knowing why a familiar material was ruled out is often as useful as the shortlist itself.

Hard filters (a resin is excluded if any fail): continuous-use temp ≥ your max service temperature clarity rank ≥ requested (opaque 1 < translucent 2 < clear 3) flexibility = compatible class (rigid rejects elastomers; flexible needs an elastomer) chemical class ≥ required (mild needs ≥ good; aggressive needs ≥ good, excellent preferred) impact class ≥ requested (low 1, medium 2, high 3) Score (ranks the survivors): + temperature headroom + impact margin + chemical margin + exact clarity / flex match + UV fit (penalty + "stabilised grade" flag when outdoor & poor weatherer) Shortlist = the top 2–4 survivors.
Property radar comparing polycarbonate, polypropylene and TPU across six selection axes A six-axis radar chart with axes for temperature, impact, UV resistance, chemical resistance, clarity and flexibility, each scored from the centre (low) to the edge (high). Polycarbonate forms a shape that is strong on impact, clarity and temperature but weak on chemical resistance and flexibility. Polypropylene is strongest on chemical resistance and middling elsewhere. TPU is strongest on flexibility and impact. No single resin fills every axis, which is why selection is about matching the shape to the requirement. TemperatureImpactUV ChemicalClarityFlexibility PC PP TPU
Figure 1. A property radar for three very different resins (schematic, scaled from representative published ranges). Polycarbonate wins on impact, clarity and temperature but gives up chemical resistance and flexibility; polypropylene owns chemical resistance; TPU owns flexibility. No shape fills every axis — selection is choosing the resin whose shape matches your requirement, then accepting its weak axes or designing around them.
Decision flow the selector applies to each resin A top-to-bottom decision flow. Every candidate resin passes through five gates in order: is its continuous-use temperature at least the service temperature; can it meet the clarity need; is it the right flexibility class; is its chemical resistance enough for the exposure; is its impact class enough. A resin that fails any gate is excluded with the reason. Resins that pass all five are scored on temperature headroom, chemical and impact margin, UV fit and exact clarity and flexibility match, and the top two to four become the shortlist. Candidate resin Temp ceiling ≥ service? Clarity meets need? Flexibility class fits? Chemical resistance OK? Impact class enough? Score & rank survivorstemp headroom · margins · UV · exact match Shortlist: top 2–4 failfailfailfailfail Excludedwith the reason
Figure 2. The gate order the tool runs for every resin. Temperature and chemistry are usually the hardest knockouts; clarity and flexibility are absolute (a polymer either is transparent or it is not). A resin that clears all five gates is scored and ranked; one that fails is reported with the single requirement that eliminated it.

Worked examples — three documented input sets

Each of these is reproducible in the selector above, and each lands where a materials engineer would expect.

1) Clear, rigid, high-impact (e.g. a machine guard or lens), 70°C, indoor, no chemicals Clarity = clear knocks out every opaque resin (ABS, POM, PBT, PC/ABS, nylon). High impact knocks out acrylic (16–32 J/m), PETG and PS (brittle). TPU fails clarity + rigidity. Survivor → PC (clear, rigid, 600–850 J/m notched). RESULT: Polycarbonate (PC). 2) Outdoor, rigid, aggressive chemical exposure (e.g. an outdoor chemical fitting), 60°C, opaque Aggressive chemistry needs ≥ good: knocks out PC, ABS, PC/ABS, acrylic, PETG, PS. Rigid rules out TPU. Survivors: PP, HDPE, POM, nylon, PBT. Scored for outdoor + rigid: PP (excellent chemistry) and PBT (good chemistry, rigid, higher temp ceiling, fair weathering) rank top; polyolefins flagged "specify a UV-stabilised grade." RESULT: PP or PBT polyester (PET family). 3) Flexible, abrasion-resistant (e.g. a caster wheel or protective boot), 60°C, mild chemical Flexible = elastomer required: only TPU clears the flexibility gate. TPU also carries high impact/abrasion and good oil resistance. RESULT: TPU.

Notice how example 1 returns a single strong answer: when clarity and high impact are both hard requirements, polycarbonate is effectively the only common molding resin that satisfies both, and the selector will tell you so rather than padding the list. Example 2 returns a genuine choice between a polyolefin and a polyester, which is exactly the real trade-off (broadest chemical resistance versus better stiffness and dimensional stability). Press Load the worked example above to run the first case.

Representative properties used by the selector

Values below are representative datasheet ranges for common unfilled grades, gathered for comparison only. Your exact grade — filled, flame-retardant, high-flow, impact-modified or UV-stabilised — can sit well outside these, so treat the table as a sanity check and the supplier datasheet as the authority.

ResinTypeCont. use (°C)Notched Izod (J/m)UV (base)ChemicalClarityStiffness
ABSamorphous~80200–400poor*fairopaquerigid
PC (polycarbonate)amorphous~120600–850fair*fairclearrigid
PP (polypropylene)semi-cryst.~9540–120poor*excellenttranslucentsemi
PE / HDPEsemi-cryst.~90100–300fair*excellenttranslucentsemi
PA6/66 (nylon)semi-cryst.~10050–110poor*goodopaquerigid
POM (acetal)semi-cryst.~9065–120poor*excellentopaquerigid
PBT (polyester)semi-cryst.~12040–60fairgoodopaquerigid
PMMA (acrylic)amorphous~8016–32excellentfairclearrigid
PC/ABSamorphous~100400–600fair*fairopaquerigid
TPUelastomer~90no breakfair*goodtranslucentflexible
PETGamorphous~6260–110goodfairclearrigid
PS / HIPSamorphous~6020–110poor*fairclear/opaquerigid

* weatherable with the right UV-stabilised grade. "Clarity" is for the natural, unpigmented resin. Notched Izod per ASTM D256; heat metrics per ASTM D648. Ranges are representative, not grade-specific.

From the tooling floor: write the requirements down and rank them must-have versus nice-to-have before you name a resin. The commonest mistake we see is a design that started from "let's use ABS because that's what we always use," then discovered at sampling that the part lives outdoors or wipes down with solvent. Changing resin after the tool is cut can mean re-cutting steel for the new shrinkage rate. The requirement list is free to change on a napkin and expensive to change in hardened steel.

Common mistakes in resin selection

When to use this selector vs other methods

MethodUse it whenLimit
This selectorNarrowing to the right resin family early, or sanity-checking a proposed material against the requirementsFamily level only; representative ranges, not grade data
Supplier datasheets & grade findersChoosing the exact grade once the family is fixedOne supplier's grades; you still have to compare
Chemical-compatibility chartsAny part in contact with a specific chemicalPer chemical/concentration/temperature; general ratings only
CAD / FEA with material cardsVerifying stiffness, stress and thermal behaviour of the chosen material in your geometryOnly as good as the material data and model
Molding & DFM reviewConfirming the resin molds well in your part and toolNeeds a near-final design and a molder

Design tips once you have a shortlist

Questions and answers

How do I choose the right plastic for my part?

Start from the requirements the part cannot live without, not from a favourite material. The five that eliminate most resins are: the highest temperature the part sees in service, whether it must survive impact, whether it lives outdoors in sunlight, what chemicals touch it, and whether it has to be clear or flexible. Rank those as must-have or nice-to-have, use them as hard filters to cut the list of candidate resins, then compare the survivors on cost drivers, moldability and finish. This selector does exactly that, then returns a short list. The datasheet for the exact grade always governs the final choice.

Which clear plastic is the most impact resistant?

Polycarbonate (PC). Among transparent thermoplastics it has by far the highest notched impact strength — commonly published around 600–850 J/m notched Izod, versus roughly 16–32 J/m for acrylic (PMMA) and 60–110 J/m for PETG. That is why PC is used for machine guards, safety lenses and visors where an acrylic part would shatter. The trade-off is that PC scratches more easily than acrylic, yellows faster in sunlight unless it is a UV-stabilised grade or has a UV hard coat, and is attacked by many solvents and strong alkalis.

What plastic is best for outdoor UV exposure?

For a clear part, acrylic (PMMA) has the best inherent weathering of the common resins. For an opaque part, almost any resin can be made weatherable with UV stabilisers and, for polyolefins, carbon black — pigmented UV-stabilised HDPE and PP, ASA, and UV grades of PC/ABS are all common outdoor choices. The resins that weather poorly even with additives are unstabilised POM, nylon and standard polystyrene. Most outdoor failures come from using a standard indoor grade outdoors, not from the base polymer, so always specify a UV-stabilised grade.

Which plastics have the best chemical resistance?

The polyolefins — polypropylene (PP) and polyethylene (HDPE) — and acetal (POM) have the broadest chemical resistance of the common molding resins, which is why they are used for tanks, chemical fittings and fluid-handling parts. PP and HDPE resist most acids, bases, salts and alcohols; acetal resists solvents and fuels well but is attacked by strong acids and oxidisers. Polycarbonate, ABS, PC/ABS and acrylic are readily attacked by many solvents and can stress-crack. Always match the resin to the specific chemical, concentration and temperature with a compatibility chart.

What is the difference between amorphous and semi-crystalline plastics for selection?

Amorphous resins (ABS, PC, PMMA, PC/ABS, PETG, PS) have no sharp melting point, shrink little and evenly, hold tight tolerances, and most transparent resins are amorphous. Semi-crystalline resins (PP, PE, nylon, acetal, PBT) have a true melting point, better chemical and fatigue resistance and often better wear, but shrink more and less predictably so they warp more easily and need a more uniform wall. Reach for amorphous when you need clarity or tight tolerances, and semi-crystalline when you need chemical resistance, fatigue life or a living hinge.

Which plastic should I use for a flexible, abrasion-resistant part?

Thermoplastic polyurethane (TPU) is the usual choice for a flexible part that also resists abrasion, tearing and oils — caster wheels, cable jackets, seals, phone bumpers and protective boots. It comes in a wide hardness range (roughly Shore 60A to 70D) so you can tune how soft or firm it is. For a less demanding flexible part, flexible polyethylene (LDPE) or a polypropylene living hinge may be enough and molds more cheaply.

Can this selector pick my exact grade of plastic?

No. It works at the resin-family level using representative published property ranges, so it tells you that, say, polycarbonate or nylon is the right family to look in. Within a family there are dozens of grades whose properties differ widely — a 30% glass-filled nylon has a heat-deflection temperature well over 200°C versus roughly 70–90°C for unfilled nylon. Use the selector to narrow the family, then choose the specific grade from supplier datasheets and confirm with your molder.

Ask JCH about material selection

Torn between two resins, or not sure a grade will hold up to your chemical or temperature? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.

AI assistant. Answers can be wrong; nothing it says is a quote or a promise.

Want a second opinion on your material choice?

This selector gives an engineering estimate. Our tooling team reviews your requirements, the candidate grades and a chemical and thermal check, and recommends a resin and grade that mold well — JCH coordinates a vetted manufacturing network across Taiwan, Vietnam and the US.

Book a 30-min call Send your part requirements