Blister & Clamshell Sheet Gauge and Blank Size Calculator
Under a uniform-thinning model (our reading, not a published rule), the starting sheet for a blister or clamshell pocket is its areal draw ratio times the thinnest wall you need, and the flat blank for each cavity is the pocket opening plus the flange on every side. Enter the opening and depth, the minimum wall, the sheet material, the flange width and how many cavities share a sheet; the page returns the draw ratio, a starting gauge in millimeters, inches and mil, the blank for one cavity and the patterned sheet for the full set.

Engineering estimate, not a quote. Treat the gauge as the opening line of a conversation with a former; the pocket pulled on the real tool has the final word.
How this works
A blister or clamshell pocket is made by heating flat sheet and pulling it into a mold, and forming adds no plastic. Every square millimeter of pocket floor and wall has to be stretched out of the sheet that sat over the cavity opening, while the flange around that opening is never drawn and keeps close to the original gauge (the flange part is our reading of the geometry). A packaging buyer therefore has two questions: how thick must the sheet start so the pocket still meets its minimum wall, and how big a piece of sheet does each cavity consume?
The draw ratio comes first. Rapidmade defines it as "total formed surface area / sheet area feeding that region" and puts the average finished thickness at a fraction of roughly 1/ADR of the sheet. For a female mold, the ACRYLITE knowledge base describes the ratio as the surface area of the mold cavity divided by the area of the sheeting available for forming, and for a blister that area is the pocket opening. With vertical walls and sharp corners the rest is plain geometry:
Why a minimum wall needs a model. Rapidmade's sizing rule works from the target average finished wall. Formlabs writes that "draw ratio multiplied by the desired gauge of the finished part will produce the minimum sheet gauge," and Rapidmade's quick reference states the same rule. A packaging drawing, though, is written against the thinnest point, because the requirement has to hold everywhere in the pocket, including the spot with the least plastic. This calculator keeps three answers apart. The headline uses the uniform-thinning model, our reading, which pretends the pocket thins evenly so that its minimum equals its average: it is the lightest sheet that could possibly work, never a comfortable one. If you have sectioned and measured an earlier pack, enter its thinnest point as a percentage of its average wall and the gauge is scaled up by that share. The third line applies Rapidmade's rule of thumb, to "estimate maximum thinning by doubling the average thinning"; Rapidmade gives no formula, so writing it as thinnest ≈ t0 × (2 ÷ ADR − 1), double the lost fraction 1 − 1/ADR, is our reading; the article itself labels the rule "a very rough estimate", and here it shows how far a corner could fall at the gauge you picked. At a ratio of 2:1 or more that rule leaves nothing at the worst spot, and we read that as the rule running out of range rather than as a forecast.
Worked example: an eight-up PETG blister
A face-seal blister for a small product needs a pocket 100 × 60 mm at the opening and 15 mm deep. The pack specification asks for at least 0.20 mm of plastic anywhere in the pocket. The sheet is PETG, the flange is 6 mm on every side, and the forming tool makes eight cavities per cycle, four across and two down. The Load the worked example button fills these values into the form.
Read the three thickness lines together. The even-wall line says 0.36 mm is the floor: thinner sheet cannot even average 0.20 mm in this pocket, let alone hold it in the corners. Our reading of Rapidmade's doubling rule, applied to that same sheet, puts the worst corner near 0.04 mm, one fifth of the requirement. The figure that settles the question sits between them and comes from a measurement: if sectioned pockets of a similar shape show the thinnest point at 60% of the average, 0.60 mm sheet is the estimate to take to the former. The draw ratio of 1.80 is identical in all three lines; only the assumption about the corners moves.
Three checks against published figures
The third check is the one that matters for packaging film. The white paper ran both candidate films through the same provisional cavity and reported the same 45.3% figure for each, which is what an area ratio predicts: the ratio belongs to the pocket, not to the sheet, so scaling the gauge scales the average wall in proportion. Check 3 enters the published averages as the wall, which is exactly what the even-wall model assumes, and recovers both flat thicknesses. The script on this page reproduces all three, and the Run check 1 button loads the first.
What the sources say about PET, PVC, PETG and PP
The ratio and the blank are geometry and do not depend on the sheet. The material enters in two places, and the page compares your result with each and puts any miss in the headline.
| Sheet | Rapidmade working areal ratio | Rohrer min/max gauge |
|---|---|---|
| PET | Not in Rapidmade's table | 0.010 to 0.045 in (10 to 45 mil) |
| PVC | 1.5 to 2.2:1 (row "PVC / Kydex") | 0.010 to 0.045 in |
| PETG | 1.5 to 2.5:1 | 0.010 to 0.045 in |
| PP | 1.2 to 1.8:1 | 0.010 to 0.050 in |
Rapidmade says its ranges are "conservative on purpose," that the table is a starting range which "assumes good heating control, sensible radii and plug assist where needed," and that it "shows the relative ordering of resins, not a universal limit." The gauge column is the min/max gauge one packaging thermoformer, Rohrer, lists for each sheet in its material guide; Rohrer does not say what sets those limits, and a listed gauge says nothing about any one pocket. Andex lists custom clamshells at 10 to 40 mil and its stock lines at 17.5 and 20 mil. For pharmaceutical PVC blisters, Wikipedia states that "the PVC sheet thickness is typically chosen between 200 and 300 μm depending on the cavity size and shape" and that most of those sheets are 250 μm. Separately, Formlabs writes that "a 3:1 draw ratio is generally considered to be the maximum for most vacuum forming operations," and the headline flags any pocket past it. None of these flags blocks a result: they are published windows, not physical limits.
Where blister pockets lose the most
The Klöckner Pentaplast white paper describes sharp corners as "typically the point of greatest thinning, where the cavity becomes most fragile and where the barrier becomes most permeable." Its Figure 4, a thickness table for points along one cross-section of a provisional cavity, lists 0.059 mm under the label "MIN (IDEAL)" and 0.028 mm under "WORST CASE." For pharmaceutical film, Wikipedia reports that "a 250 μm film will have a final thickness of 50 to 100 μm in some deep drawn pockets"; under the even-wall model those two numbers would need draw ratios of 5.0 and 2.5, our arithmetic on its figures. Three levers move plastic back toward the corners. The same white paper notes that "a larger draft angle results in less thinning of the film, but this will also increase the size of the blister cavity." Rapidmade says real thinning is "reduced by good practice, such as filleting corner radii." And Wikipedia describes plug assist, in which "the warm film will be physically pushed down partially into the cavity," as a way to address "uneven wall thickness, thinning in critical areas, and incomplete mold filling." This page assumes vertical walls and sharp corners, so any draft or radius you add trims the true ratio and the gauge it prints errs thick.
Sizing the blank and the sheet
The flange is where the pack is heat-sealed to its card, trapped between card layers or snapped closed, so its width comes from the closure, not from the forming. One cavity's blank is the opening grown by that flange on every side; a round pocket gets a square blank of side D + 2F. A clamshell is, in Wikipedia's words, "a blister that folds onto itself," so size each half as its own pocket and widen the flange on the hinged edge by the strip the hinge needs (our reading of how the layout adds up). The page then lays the blanks edge to edge, a across and ⌈N ÷ a⌉ down, so neighboring pockets sit two flange widths apart. With the across count left empty it uses ⌈√N⌉, our reading of a compact grid, and reports any places left empty in the last row. The sheet it prints is the patterned area only: the forming machine also needs clamp margin and trim around the outside, and that allowance belongs to the machine and the former, so the page does not guess it. If you enter the sheet density from its datasheet, the page multiplies blank area by starting gauge and density to give the grams of sheet in one blank; forming moves plastic around without adding or removing any, so the trimmed pocket and flange weigh what their blank weighed. Density values for common sheets are on our plastic density lookup.
Common mistakes
- Sizing to the average when the drawing means the minimum. t0 ÷ ADR describes the wall as a whole. The white paper places the greatest thinning in sharp corners, and an average cannot show it.
- Dividing by the blank instead of the opening. Counting the flange as feeding sheet shrinks the computed ratio, and the predicted wall then comes out fatter than the pocket will.
- Leaving the flange out of the sheet order. In the worked example the flange takes 25.6% of each 8,064 mm² blank, so ordering from the 6,000 mm² opening alone misses 2,064 mm² per cavity, 34.4% short.
- Reading a converter's gauge window as approval. A gauge inside Rohrer's range is one that shop lists, not proof that your pocket holds its wall.
- Carrying a PVC design straight to polypropylene. Rapidmade's working range for PP tops out at 1.8:1, below the 2.2:1 it gives PVC, so a pocket at 2.0:1 sits inside one range and outside the other.
- Treating the patterned sheet as the machine sheet. The clamp border comes on top; ask the former for it before ordering sheet by the piece.
Choosing between this page and other methods
| Approach | Best for | Falls short when |
|---|---|---|
| This page | Choosing sheet for a blister or clamshell against a minimum wall; sizing one blank and the patterned sheet | Vertical walls, sharp corners, rectangular or round pockets; the corner share comes from a model or your own sections |
| Thermoforming draw ratio calculator | Drafted trays, boxes and cups; average wall, linear ratio and depth-to-opening | Not built around flanges, minimum walls or multi-cavity sheets |
| Finite element forming simulation | Barrier films, where Wikipedia notes that "the reduction in thickness will result in an increase in WVT"; Pharmaceutical Technology describes modeling that "simulates cavity thinning and moisture permeation through finite element analysis software" | Needs pocket CAD and a material model from the film supplier |
| Sectioned trial pulls | Signing off the gauge and measuring your own k | Needs a forming tool and sheet in hand |
| Carton size calculator | Sizing the shipper that the finished cards pack into | Says nothing about the formed pocket |
Sources (all retrieved November 20, 2026)
- Areal draw ratio definition; finished thickness fraction about 1/ADR; minimum starting gauge about ADR times target average wall; the worked box of 10 by 12 by 2 inches; the doubling rule and its "very rough estimate" caveat; corner radii; PETG, PVC and PP working ranges and their caveats: Rapidmade, Draw Ratio in Thermoforming: How It Controls Wall Thickness, Strength, and Part Quality.
- Female-mold draw ratio and the cylinder formula 1 + 4H/D: ACRYLITE knowledge base, How do you determine needed thickness of sheet for thermoforming.
- Draw ratio times finished gauge gives the minimum sheet gauge; 3:1 as the usual vacuum-forming maximum: Formlabs, prototyping with vacuum forming.
- Figure 6 (289 and 340 µm films, 131 and 154 µm averages, 45.3%), Figure 4 (0.059 and 0.028 mm), sharp corners as the point of greatest thinning and most permeable barrier, draft and cavity size: Klöckner Pentaplast, White Paper: Virtual Prototyping of Blister Packaging (Paper III), on SlideShare.
- Pharmaceutical PVC sheet of 200 to 300 μm and mostly 250 μm; 50 to 100 μm after forming in some deep pockets; thinner film raising WVT; plug assist; clamshell as a blister that folds onto itself: Wikipedia, Blister pack.
- Min/max gauge for PVC, PET and PETG (0.010 to 0.045 in) and PP (0.010 to 0.050 in): Rohrer, How to Choose the Right Plastic for Your Thermoformed Packaging.
- Inch to meter 2.54 E−02 and mil (0.001 in) to millimeter 2.54 E−02: NIST SP 811, Appendix B.8.
- Custom clamshells at 10 to 40 mil, stock lines at 17.5 and 20 mil: Andex, Clamshell packaging.
- Finite element modeling of cavity thinning: Hallie Forcinio, Blister Pack Optimization, Pharmaceutical Technology (April 2, 2016).
Reviewed by the JCH tooling team · updated November 2026.
Blister and clamshell sheet questions
How thick should the plastic be for a blister pack?
Work backward from the thinnest wall the pocket may have. Multiplying that wall by the pocket's areal draw ratio gives the lightest sheet that could average it, and nothing thinner can. Real corners finish below the average, so a sound specification lands above that floor by a margin best taken from cut sections of a similar pack. For pharmaceutical PVC blister film, the Wikipedia article names a quarter of a millimeter as the most common choice.
How do I calculate the draw ratio of a blister cavity?
Divide the plastic surface of the finished pocket, floor plus sides, by the area of its mouth. A straight-sided pocket 50 by 40 mm and 10 mm deep has a 2,000 mm² mouth, 1,800 mm² of sides and a 2,000 mm² floor, so 3,800 mm² of formed surface and a ratio of 1.9. For a round pocket the sum reduces to one plus four times depth over diameter.
How big a blank does each blister or clamshell cavity need?
Grow the mouth of the pocket outward by the rim width on all four sides. A 50 by 40 mm pocket with an 8 mm rim takes a 66 by 56 mm piece of sheet. A hinged clamshell is two pockets joined along one edge, so treat each half this way and add the hinge strip on the joined side. The forming machine's clamping border is extra.
Why is the corner of my formed pocket thinner than the estimate?
An even-thinning estimate spreads the stretch over the whole pocket, while a real cavity concentrates it low down; Klöckner Pentaplast's blister white paper identifies the corners as where film gets thinnest. Bigger corner radii, a little more draft and a plug that pushes warm film into the cavity before vacuum all help. Cut a sample through a corner and measure it to learn how much margin to add.
Does PET, PVC, PETG or PP change the gauge I need?
The area arithmetic is identical for every sheet, so the even-wall gauge does not change. Material shows up in how far each sheet is expected to stretch and in the gauges converters list. Rapidmade's working table rates polypropylene below PETG and PVC, at up to 1.8:1, and has no PET row; Rohrer quotes 10 to 45 mil for PET, PVC and PETG and up to 50 mil for PP.
How many cavities fit on one forming sheet?
As many as fit inside the former's forming area once its clamping border is removed, with every pocket keeping its full rim. The tool places blanks side by side and reports the patterned width and length so you can hold them against the machine's window. Ask the former for that window and border before fixing the count.
Is this the same as the thermoforming draw ratio calculator?
Both rest on the same area ratio but answer different questions. The thermoforming tool handles drafted trays, cups and boxes and reports average wall, linear stretch and depth-to-opening. This one starts from a minimum wall on a packaging pocket, lets you scale for measured corner loss, and turns cavity count and rim width into blank and sheet dimensions.
Ask JCH about your blister or clamshell
Unsure what flange your card needs, or whether a pocket this deep belongs in PET or PETG? Describe the product and the numbers above. Ask JCH is an AI assistant. After its first answer it shows an optional email field, in case you would like someone to get back to you.
Generated by an AI model; it can be mistaken, and nothing it says binds JCH.
Choosing sheet for a new pack?
Send the product dimensions, the pocket sketch and how the pack must close. Before anyone commits to a forming tool, our tooling team will check the draw ratio, the flange and the cavity layout against the sheet you have in mind.
Book a free 30-minute first consultation Pocket drawing ready? Send it