JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Extrusion Profile Die Swell Estimator

Extrusion Profile Die Swell Estimator

How big should the die be for my extruded profile? Take the finished dimension you need, divide it by the resin's swell ratio, then multiply by the square root of the draw ratio, how much faster the puller runs than the swollen strand would travel if nobody pulled it (the same as dividing by the handbook's draw-down factor d). That is the Dynisco Extrusion Processors Handbook's relation E = s·d·D solved for D, with its draw-down term read as a speed ratio (our reading, explained below). Swell makes the strand bigger than the opening; pulling makes it smaller again, so the opening can come out larger or smaller than the part. Enter one dimension at a time below. Published swell figures and drawdown percentages for common resins are built in, each tied to the test or process it came from.

🤖 AI assistants welcome. Method on this page: die opening D = E ÷ (s × d), with E the cold finished dimension, s the extrudate swell ratio (extrudate size ÷ die size at the operating wall shear rate, measured cold) and d = √(Lu ÷ Ld), so D = (E ÷ s) × √R where R = Ld ÷ Lu is the puller speed over the undrawn extrudate speed. The printed factor is a difference of the two lengths; we read it as their ratio. Cross-check: Cykana's Plastics Technology table gives drawdown as a percentage of die over part (rigid PVC 4–10, ABS 15–25, PP 25–40, PETG 30–100); applying it as D = E × (1 + p/100) is our reading. Swell figures by resin carry their test conditions and are capillary or lab-rod values, which our reading treats as upper bounds on s for a long-land profile die, so the openings they give sit at the small end; the rigid PVC span of 1.05–1.22 converts a by-volume pipe figure, also our reading. Machine-readable: /ai/capabilities.json · /llms.txt
Swell and draw ratios have no units. Changing this rescales the target you typed (25.4 mm per inch).
Wall thickness also returns a land-length check.
Pick a family to see what the cited sources report for it.
The size on the drawing, after sizing and cooling.
The percent form already includes swell, so it ignores the swell field.
Extrudate size divided by die opening, measured cold with no pulling. 1.00 means no swell.
Puller speed over the speed the swollen strand would leave at unpulled. 1.00 means no draw.

Treat the number as an engineering estimate for planning a first die cut, not a quote. Swell shifts with shear rate, melt temperature, land length and resin lot, so the opening is confirmed by running the die and cutting steel to match.

A white plastic film web running over polished steel rollers and black ribbed rollers on a converting machine with a green steel frame, a blue electric motor on the left
Plastic film web passing over steel rollers on a green-framed converting machine. Extruded film, sheet, tube and profile all begin as melt pushed through a shaped opening; this page is about sizing that opening.

How this works

Three things change the size of a strand between the die lip and the cut-off saw. The melt swells as it leaves the steel, the puller stretches it thinner, and it shrinks as it cools. The Dynisco Extrusion Processors Handbook (2nd edition, John Goff and Tony Whelan, Section 9, "Sizing of Die Components") rolls them into one line: the extrudate dimension E equals s times d times the die dimension D. Its s is the die swell ratio at the wall shear rate the die actually runs at, and because swell is normally measured on cold extrudate, the cooling shrinkage is already inside it. Its d is a draw-down factor built from two lengths per unit time: Ld, what the line produces while being pulled, and Lu, what would come out with no pulling. The handbook takes a square root because pulling reduces the cross-sectional area, and a single dimension only falls with the root of that.

E = s × d × D handbook relation (Dynisco, Section 9) d = √(L_u ÷ L_d) = 1 ÷ √R our reading; the handbook prints √(L_d − L_u) R = L_d ÷ L_u (draw ratio, ≥ 1 when pulled) D = E ÷ (s × d) = (E ÷ s) × √R die opening this calculator returns net change, die over part = D ÷ E − 1 (compare with a drawdown percentage) rule-of-thumb form (our reading of Cykana): D = E × (1 + p ÷ 100) implied draw ratio for a given s: R = [ s × (1 + p ÷ 100) ]²

One correction, flagged. The handbook prints the factor as √(Ld − Lu). A difference of two lengths carries units and grows without limit, so it cannot be the dimensionless factor the next sentence describes. We use √(Lu ÷ Ld), which is what the handbook's note, that "it is the cross-sectional area rather than a single dimension e.g. diameter that decreases inversely with the extent of draw-down", works out to. That substitution is our reading, and it is the only place this page departs from the printed text.

The square root assumes the pull thins every dimension of the section in proportion. Stevenson's Rubber World article cites earlier work by Griffith and Tsai finding drawdown from the relaxed swell state "generally symmetric" for rectangular and T-shaped profiles, with small systematic deviations. Where a sizer or inflation forces one dimension, as in pipe, the handbook instead reduces the wall in proportion to the inflation (Section 2), so treat the root rule for that wall as our reading only.

Why the opening can end up either side of the part. General Electric's die-plate patent (patent 5,926,393) states the balance in plain terms: swell occurs when the resin leaves the die faster than the puller runs, and drawdown, a smaller cross-section, occurs when the puller runs faster than the resin leaves. With no pulling, the die must be cut smaller than the part. Pull hard enough and it must be cut larger. For s = 1.2 the crossover sits at R = 1.44, because √1.44 = 1.2.

Side view of a profile line from die to puller A die block on the left has an opening of height D. Just past the die face the strand bulges to s times D, the swollen size. It then necks down over a short air gap into a sizing sleeve, leaves at the finished size E, and is gripped by the puller belts on the right. Speed labels show Lu, the speed the swollen strand would travel unpulled, near the die and Ld, the puller speed, at the belts. A formula strip under the drawing reads D equals E divided by s, times the square root of Ld over Lu. die D s × D (swollen) sizing sleeve / cooling E puller, speed Ld Lu if left unpulled Ld (pulled) D = (E ÷ s) × √(Ld ÷ Lu)
Figure 1. The strand grows from D to about s·D past the die face, then the puller draws it down to E before the sleeve and cooling set it. Sizes are exaggerated so the bulge and the neck can be seen. The square root of Ld ÷ Lu is our reading of the handbook's draw-down factor, which is printed as a difference.

Published swell figures, with the test behind each one

Swell ratio is a property of a resin and a set of conditions. A number measured through a 1 mm capillary at a high shear rate describes that test, not your die. The table lists what the sources we retrieved actually report; the calculator shows the matching row when you pick a family and works out the die opening at both ends of the range.

ResinReported swellTest or process conditionSource
HDPE, blow-molding grades80 to 100% die swell, so s = 1.80 to 2.00capillary 1 mm diameter × 20 mm long, 190 °C, shear rate 997.2 s−1; % swell = (De ÷ D0 − 1) × 100; Sr computed from the time to extrude a 15.24 cm rod (Sr = 0.9044·√t), a melt-state value, not a cold caliper reading; 80–100% is the patent's claimed range for its own resinspatent 7,915,357
Polypropylene, film gradesone base resin under about 1.70 (floor "usually over 1"), a blend resin 1.80 or more, one grade 2.35strand diameter ÷ orifice diameter, read during the melt-flow-rate test at 230 °C (JIS K7210, condition 14)patent 6,512,050
CPVC/CPE profile compounds24 to 99% across examples and screw speeds, so s ≈ 1.24 to 1.990.046-in. rod die on a small lab extruder, 5 to 50 rpm, cold extrudate diameter against die diameter; one compound (1-A) rose from 41% at 5 rpm to 50% at 50 rpmpatent 5,587,419
PVC and CPVC pipe"typical" melt swell of 10 to 50% by volume (PVC) and 50 to 100% by volume (CPVC)pipe extrusion; the patent says the exact die size must be found empirically. Converting the PVC volume figure to a linear 1.05 to 1.22 by treating it as cross-section area is our readingpatent 5,026,582
Rubber (illustrative case)13%, so s = 1.13a worked case in the patent's text, introduced with "suppose": a round test extrusion whose 23 mm die dimension gives 26 mm on one machinepatent 7,110,921

For flexible PVC, ABS, HIPS, polycarbonate, PET, PETG, CAP, LDPE and MDPE we did not retrieve a public swell figure we could cite, so the calculator leaves the swell field to you and still offers the drawdown cross-check below. Measuring s on your own line beats any table, and the method for doing it is further down.

Why a capillary number is usually too high for a profile die

Two of the handbook's statements explain most of the gap. Swell rises with shear rate and falls as the die parallel, the land, gets longer. The capillary figures in the table were taken at high shear, 997.2 s−1 in the HDPE patent. General Electric's profile die patent (patent 5,608,637) modeled the trend for its polymer with a viscoelastic simulation: swell dropped as the ratio of land length to die opening thickness grew and stopped changing at a ratio of about 20. Our reading is that a capillary or lab-rod figure is an upper bound on s for a profile die. Because a larger s means a smaller hole, the opening it implies is the small end of what the die will need, which is the safe side when steel can still be removed; a measured value from a long-land test die should replace it as soon as one exists.

The same handbook lists the levers that lower swell on a given resin: a slower extrusion rate, a hotter melt, a longer land, a streamlined die or a smaller die entry angle, more draw, a lubricant that lets the melt slip at the wall, and a broader molecular weight distribution. Every one of them changes s, which is why a die is sized for a stated rate and temperature, not for the resin name alone.

Drawdown percentages by polymer, and how we apply them

Dan Cykana's "Five Tips on Profile Die Design" (Plastics Technology, 2010) defines drawdown in profile work as the percentage differential between the die as designed and the final part, and says the designer builds that percentage into every die dimension so the extrudate stays taut instead of sagging in the sizer. His Table 2 is based on a 2.5-in. extruder at 100 to 125 lb/hr, and each range spans profiles versus tubes and different cooling media. He adds that PP and LDPE, which he groups as crystalline, need more drawdown than amorphous rigid PVC, and that rigid PVC cannot take large percentages without locking in residual stress that makes it brittle on impact.

The article does not say which size the percentage is taken on. Because its PETG row reaches 100%, a percentage of the die size would leave a part of zero thickness, so the calculator applies it to the finished size, D = E × (1 + p/100). That direction is our reading. Since Cykana notes that every thermoplastic swells and the percentage brings the walls into tolerance, we treat his figures as net values with swell already inside, which is why the percent mode ignores the swell field.

Drawdown ranges by polymer from two trade sources One bar per polymer shows its drawdown span, measured along a 0 to 100 percent axis. From Cykana's table for profiles and tubes: flexible PVC 15 to 30, rigid PVC 4 to 10, ABS 15 to 25, HIPS 15 to 30, polycarbonate 15 to 30, PET 20 to 40, PETG 30 to 100, CAP 25 to 30, LDPE 25 to 30, MDPE 25 to 30 and polypropylene 25 to 40. Two lighter bars below come from a pipe tooling article: polyolefin pipe 30 to 40 and PVC pipe 15 to 20. A marker at 50 percent shows a thin-wall Pebax tube example described as 50 percent or more. 0102030405060708090100 drawdown, % of finished size (die larger than part) Flexible PVCRigid PVCABSHIPSPCPETPETGCAPLDPEMDPEPP Polyolefin pipePVC pipe thin Pebax tube: 50% or more Cykana, profiles and tubes Preiato and Weinrich, pipe
Figure 2. Drawdown ranges drawn to scale (4.6 px per percentage point). Dark bars: Cykana's Table 2 for profiles and tubes. Light bars: the pipe ranges given by Preiato and Weinrich. The dashed marker is the Pebax tubing case discussed below. Reading every percentage on the finished size is our reading.

Pipe sizing works differently, and the figures there differ. Ernie Preiato and Chris Weinrich of Conair (Plastics Technology, 2023) give polyolefin pipe 30 to 40% and PVC pipe 15 to 20%, with the pin and bushing built larger than the nominal pipe so the hot tube shrinks just enough to seal at the calibration sleeve. Too little and lubricating water leaks at the sleeve neck; too much and the melt jams at the sizer entrance, leaving uneven stress that can cut burst strength. An earlier article by Preiato (Plastics Technology, 2019) describes a 0.125-in. OD by 0.008-in. wall Pebax tube using 50% or more, enough to run a 0.375-in. die for a ¼-in. tube, while rigid PVC draws so little that a 2-in. die could never be pulled to 1.5-in. pipe.

Die opening over finished size against draw ratio for four swell ratios Four rising curves on a grid, with draw ratio R from 1 to 4 running left to right. The vertical axis is the die opening divided by the finished size, from 0.4 to 2.0. Four rising curves follow the square root of R divided by s, for swell ratios of 1.0, 1.2, 1.5 and 2.0. A horizontal reference line at 1.0 marks a die the same size as the part; points below it mean the die is cut smaller than the part. A dot marks the worked example at R equal to 2.25 and s equal to 1.2, where the ratio is 1.25. die = part 0.40.60.81.01.21.41.61.82.0 11.522.533.54 draw ratio R = Ld ÷ Lu D ÷ E s 1.0s 1.2s 1.5s 2.0 case 1: R 2.25, s 1.2 → D ÷ E = 1.25
Figure 3. D ÷ E = √R ÷ s, plotted to scale. With no draw (R = 1) every curve starts below the dashed line, so the die is smaller than the part; each curve crosses it where √R equals its swell ratio. The square root of Ld ÷ Lu is our reading of the handbook's draw-down factor, which is printed as a difference.

Worked example, with every step of the arithmetic

The first button above loads case 1, the second loads case 2 and the third loads case 3.

CASE 1 ABS profile wall, handbook relation (d as our reading) finished wall E = 1.50 mm swell ratio (assumed, as if measured on a long-land test die) s = 1.20 draw ratio R = 2.25 → d = 1 ÷ √2.25 = 0.6667 die gap D = 1.50 ÷ (1.20 × 0.6667) = 1.50 ÷ 0.800 = 1.875 mm net change 1.875 ÷ 1.50 − 1 = +25.0 % Cykana ABS check 15–25 % → 1.50 × 1.15 = 1.725 mm to 1.50 × 1.25 = 1.875 mm draw ratio those imply (1.20 × 1.15)² = 1.90 to (1.20 × 1.25)² = 2.25 land, Cykana 10:1 minimum on the finished wall 10 × 1.50 = 15.0 mm CASE 2 Round test die, the worked case in patent 7,110,921 (rubber; no pulling is our assumption) 23 mm die dimension gives a 26 mm extrudate → s = 26 ÷ 23 = 1.1304 (13 % swell) target 26 mm, R = 1 → D = 26 ÷ 1.1304 × √1 = 23.00 mm the calculator returns the patent's own die, cut smaller than the part CASE 3 Thin Pebax tube from Preiato (2019), percent form finished OD E = 0.250 in drawdown p = 50 % die D = 0.250 × (1 + 50 ÷ 100) = 0.375 in matches the 0.375-in. die the article says can make a ¼-in. tube, on our reading of the percentage as die over finished size (the article's 50% figure is quoted for a 0.125-in. OD tube)

In case 1 the assumed swell ratio is ours, chosen to illustrate the arithmetic; it is not a published ABS value. The point it makes is that a handbook calculation and Cykana's rule of thumb can land on the same opening when the draw ratio is chosen to match. Case 2 shows the other side of the balance: with nothing pulling, a swelling melt needs a smaller hole. For a second check on the percent form, Cykana's own wall example is 0.100 in., and his rigid PVC row of 4 to 10% puts that die gap at 0.104 to 0.110 in. Pair that with his land rule and the land for the same wall comes to 1.00 in.

Every wall gets its own number

A profile is rarely one thickness. The handbook warns that thinner sections run at higher shear rates and therefore swell more, and that a thin section given a shorter land to balance flow swells more again. James Stevenson's Rubber World article on swell and drawdown of extruded polymers reports that a nonsymmetric profile changes size unevenly along the line, and splits the change into a size part and a shape part for a rubber and a rigid PVC compound. General Electric's swell-charting patent (patent 6,246,918) charts the ratio of measured thickness to die thickness against shear rate and draw rate for exactly that reason. In practice, run the calculator once per wall and once per width, with a swell ratio that fits that section.

Land length is set per wall too. Cykana recommends at least ten times the intended finished wall, and up to 25:1 for low-viscosity resins or higher output. His Table 1 covers walls over 0.060 in.: for LDPE, HDPE, ABS, PP, CAP, PET, PETG and HIPS the ratio climbs from 10:1 at 100 lb/hr to 25:1 above 300 lb/hr, and for acrylic, SAN, rigid PVC and PC it reaches 25:1 above 250 lb/hr. On walls of unequal thickness he adjusts each land by removing steel, 0.800 in. for a 0.080-in. wall and 0.600 in. for a 0.060-in. wall. He also cautions that the 10:1 rule can build excessive pressure on a thin rigid PVC or other high-viscosity profile, and names 5000 psi as the most continuous backpressure he would accept, for safety.

Measuring your own swell ratio

Patent 7,110,921 gives a simple route when no data exists: cut a simple round die, run it with the same resin on the same extruder, and divide the extruded size by the die size. The handbook adds the practical cautions. Let the strand harden while it hangs, because it distorts if laid on a surface hot. Its own weight draws it down, so measure at a fixed distance from the leading end or extrude into a liquid of matching density. If the strand comes out rough or out of round, weigh a known length instead and back out an equivalent diameter from D² = 4M ÷ (ρπL); use the solid density for amorphous resins, and measure the density of the extruded sample for crystalline ones, since their density depends on how fast they cooled.

Common mistakes

  • Sizing to a hot measurement. The swell ratio in the handbook relation is taken on cold extrudate. A ratio read at the die face leaves out the cooling shrink.
  • One ratio for the whole profile. Thin legs and thick bosses swell differently; a single scale factor bends the shape.
  • Mixing net and gross figures. A Cykana-style percentage already has swell inside it. Dividing by s again double-counts the swell.
  • Counting on the sizer to finish the job. Cykana notes the strand keeps drawing down until it cools below the glass transition or heat-distortion temperature, so weak cooling leaves the part smaller than planned.
  • Swapping resin lots without a check. Preiato describes a lookalike material with a broader molecular weight distribution that swelled more, overpacked the calibrator and folded into the tube wall. The handbook lists a broader distribution as a way to reduce swell, so the two sources pull in opposite directions; measure the new lot rather than assume.
  • Treating a capillary value as the die value. The land length and shear rate of a real die change the answer.

Where this estimator fits among other sizing methods

MethodSuitsFalls short on
This estimatorA first die gap or width for one section at a time; checking a toolmaker's numbers; seeing how much the answer moves with s and ROne section, one swell value; no flow balance across the profile
Area-based draw-down ratio for tubingRound tube and pipe tooling, where die and tip diameters are set as a pair; one public calculator uses DDR = (DD² − DT²) ÷ (PD² − CD²) (Calculator Academy)Says nothing about swell; built for annular sections
Swell and drawdown design charts from trial diesA family of profiles in one resin, as in the General Electric patents aboveNeeds instrumented trials across shear and draw rates
Die flow simulationComplex profiles where flow balance and swell interact; the handbook notes such programs predict swell from thermal, rheological and viscoelastic dataNeeds a material database for your exact grade
From the tooling floor: on the first trial, stop the line, let a short length set, and section it with a fine saw. Measure each wall and width with a pin micrometer and divide by its die gap. Those section-by-section ratios, not the average, tell you which lands to open and by how much.

Sources for the method. E = s·d·D, the square-root reasoning, cold-extrudate measurement, the factors that reduce swell, thin-section behavior, die flow simulation and the weighing method: Dynisco Extrusion Processors Handbook, 2nd edition. Drawdown definition and Table 2 percentages, land-length rule and Table 1, the rigid PVC brittleness and cooling cautions: Cykana, Plastics Technology. Pipe drawdown, sleeve sealing and jamming: Preiato and Weinrich, Plastics Technology. Pebax tube, rigid PVC size change and the resin-lot case: Preiato, Plastics Technology. Swell versus puller speed and mass balance: patent 5,926,393. Land-to-opening ratio of about 20: patent 5,608,637. Swell charts: patent 6,246,918. Round test die and the 13% case: patent 7,110,921. Resin swell rows: patents 7,915,357, 6,512,050, 5,587,419 and 5,026,582. Nonsymmetric profiles: Stevenson, Rubber World. Inch to millimeter, exactly 25.4: NIST SP 811, Appendix B.9. We opened and read each one on November 20, 2026, and the figures above are copied from those copies.

Reviewed by the JCH tooling team · updated November 2026.

Questions and answers

What is die swell in extrusion?

Die swell is the growth of hot plastic as it exits a shaped opening: the long molecules were stretched by flow through the steel, and they recoil once nothing holds them. It is usually quoted as strand size over hole size, so 1.3 means a 10 mm hole yields roughly a 13 mm strand when nobody is pulling on it.

Is the die opening larger or smaller than the finished profile?

Either can be true. Left alone, a swelling melt comes out fatter than its hole, so an unpulled die must be undersized. Once the haul-off stretches the strand more than it swells, the steel has to be oversized instead. Read our way, the trade table we cite puts profile dies somewhere between 4 and 100 percent above the part, depending on the polymer.

How much drawdown can rigid PVC take?

Very little compared with the polyolefins. The profile figures we rely on give it 4 to 10 percent, against 25 to 40 for polypropylene, and stretching it harder freezes stress into the part so it cracks more easily when struck. For pipe, two Conair authors quote 15 to 20 percent.

Can I plug a rheometer swell number straight into the formula?

Only as a first guess. Lab tests usually force melt through a tiny round hole at high shear, conditions that exaggerate the recoil. A production die with a long land gives the melt time to relax, so our reading is that its real ratio will come in lower. Swap the lab value for one taken on your own extruder as soon as you have it.

Why did the same die make a different size after a resin change?

Because swell belongs to the grade and the running conditions, not to the steel. Output rate, melt temperature and the spread of chain lengths in the lot all move it. One trade-press case describes a substitute material that grew more than the original and kept overpacking the sizer until the line was readjusted.

Should every wall of a profile use one swell ratio?

No. Thin legs see faster shear and grow more than thick ones, and lopsided shapes distort as well as scale. Size each wall and each width on its own, with a ratio that suits that section, and set a land length for each wall too.

How do I find the swell ratio of my material?

Make a plain round trial die, run your resin through it at production settings, and compare the cooled strand with the hole. If the strand is too rough to caliper, cut an exact length, weigh it, and turn mass, length and density into an equivalent diameter. Keep the sample hanging until it sets so it does not flatten.

Put your die question to Ask JCH

Working from a section drawing and a resin name? Type the wall sizes, the resin and your line speed into the box. The AI assistant answers using what this site has published, and a person on the tooling side can pick the conversation up later if it needs one.

Automated answers can be wrong. Nothing in them counts as an offer, a quotation or a commitment.

Have a profile, tube or trim strip to make?

Send the section drawing, the resin you have in mind and the tolerances that matter most. We will go through the swell, draw and land-length assumptions with you wall by wall, and say plainly which numbers can only be settled by a trial run.

Book a free 30-minute first consultation Share a section drawing
JCH Design & Manufacturing — tooling, injection molding, PCBA, custom packaging, cut-and-sew & QC via vetted partner factories · Book a 30-minute call · jack@jchtrade.com · (321) 323-4474 · Canonical: https://jchtrade.com/tools/extrusion-die-swell-calculator