What size should the mold be so the part shrinks to the number on your drawing? Enter the part dimension and resin. The calculator applies mold dimension = part ÷ (1 − S), gives a steel-safe cut size for cavity or core features, and checks whether the resin's shrink range alone could push the part outside your tolerance.
Engineering estimate, not a quote. Final steel sizes come from the grade's datasheet, your molder's experience with that grade, and a trial shot.
Molten plastic fills the mold at the mold's size, then contracts as it cools and solidifies. The part that comes out is smaller than the steel that formed it. The standard test methods for this, ASTM D955 and ISO 294-4, define mold shrinkage as the difference between the mold dimension and the part dimension, divided by the mold dimension. Rearranging that definition gives the size to cut the steel:
Shrink rates on datasheets are given in percent or in thousandths per unit length (in/in or mm/mm). 0.5% equals 0.005 in/in, which is the same as 5 thousandths of an inch per inch. Enter percent here.
| Resin | Structure | Typical shrink (%) | Midpoint |
|---|---|---|---|
| ABS | amorphous | 0.4 – 0.7 | 0.55 |
| PC (polycarbonate) | amorphous | 0.5 – 0.7 | 0.60 |
| PC/ABS | amorphous | 0.5 – 0.7 | 0.60 |
| PS (general purpose) | amorphous | 0.3 – 0.6 | 0.45 |
| HIPS | amorphous | 0.4 – 0.7 | 0.55 |
| PMMA (acrylic) | amorphous | 0.2 – 0.8 | 0.50 |
| SAN | amorphous | 0.3 – 0.5 | 0.40 |
| Rigid PVC | amorphous | 0.2 – 0.5 | 0.35 |
| PP (polypropylene) | semi-crystalline | 1.0 – 2.5 | 1.75 |
| HDPE | semi-crystalline | 1.5 – 3.0 | 2.25 |
| LDPE | semi-crystalline | 1.5 – 3.0 | 2.25 |
| POM (acetal) | semi-crystalline | 1.8 – 2.5 | 2.15 |
| PA6 (nylon 6) | semi-crystalline | 0.7 – 1.5 | 1.10 |
| PA66 (nylon 66) | semi-crystalline | 1.0 – 2.0 | 1.50 |
| PA66 30% glass | filled, anisotropic | 0.3 – 0.8 | 0.55 |
| PBT | semi-crystalline | 1.5 – 2.0 | 1.75 |
| PBT 30% glass | filled, anisotropic | 0.3 – 0.8 | 0.55 |
| TPE / TPU | varies by family | 0.5 – 2.0 | 1.25 |
Generic ranges as typically published on resin datasheets (measured per ASTM D955 or ISO 294-4). Individual grades sit anywhere in, and sometimes outside, these ranges. The datasheet for the exact grade you will mold governs.
An ABS housing has an outside length of 100.00 mm ±0.10 mm on the drawing. The ABS range is 0.4–0.7%, so we design to the 0.55% midpoint.
The lesson: for ABS the generic shrink range alone is wider than a ±0.10 mm band on a 100 mm dimension. The tool should be cut steel-safe, a trial shot measured, and the cavity opened to the measured shrink. Press Load the worked example above to see the calculator reproduce these numbers.
For comparison, a 50.00 mm polypropylene dimension at 1.75% needs 50.00 / 0.9825 = 50.891 mm of steel. The (1 + S) shortcut gives 50.875 mm, 0.016 mm small. The shortcut error grows with the square of the shrink rate, which is why it matters most for PP, PE and acetal.
Removing steel from a mold is routine machining. Adding steel back means welding, re-machining and re-polishing, with a risk of visible weld lines on cosmetic surfaces. So toolmakers cut critical features so the first trial lands on the side that can be fixed by removing metal.
For an outside dimension, the cavity forms the part, so the cavity is sized with the low end of the shrink range: the part may come out slightly small, and the cavity is opened up. For a hole, slot or inside diameter, a core forms the feature, so the core is sized with the high end: the hole may come out slightly large, and the core is ground down. The calculator gives you both the nominal and the steel-safe number.
| Method | Use it when | Limit |
|---|---|---|
| This calculator with the generic range | Early design, first tool sizing, checking whether a tolerance is realistic for a resin family | Range width is the generic spread; one rate per dimension |
| Grade datasheet value (custom input) | The grade is chosen and the part is simple with uniform walls | Datasheet plaques are a fixed thickness; your wall may differ |
| Mold-flow simulation | Fiber-filled resins, uneven walls, long parts, tight tolerances | Needs a near-final CAD model and accurate material data |
| Data from a previous tool in the same grade | A family of similar parts already in production | Only valid for similar wall, gate and processing |
| Prototype or bridge tool | Critical fits where a production tool correction would be costly | An extra tool and trial loop |
Divide the part dimension by (1 minus the shrink rate as a decimal). This follows the ASTM D955 definition, where shrinkage is measured as a fraction of the mold dimension. Example: a 100.00 mm ABS dimension at 0.55 percent shrink needs a mold dimension of 100.00 / 0.9945 = 100.553 mm.
Divide by (1 − S) when the shrink rate is defined the ASTM D955 way, as a fraction of the mold dimension, which is how resin datasheets report it. Multiplying by (1 + S) is a common shortcut that comes out slightly small; the error is about S squared times the dimension. At 0.5 percent on 100 mm it is 0.0025 mm, but at 2 percent on 300 mm it is about 0.12 mm, which can exceed a tight tolerance.
Typical datasheet ranges are: ABS 0.4 to 0.7 percent, polycarbonate 0.5 to 0.7 percent, polystyrene 0.3 to 0.6 percent, acrylic 0.2 to 0.8 percent, polypropylene 1.0 to 2.5 percent, HDPE 1.5 to 3.0 percent, acetal 1.8 to 2.5 percent, nylon 66 1.0 to 2.0 percent and 30 percent glass-filled nylon 0.3 to 0.8 percent depending on direction. The datasheet for the exact grade governs.
Semi-crystalline resins such as polypropylene, polyethylene, acetal and nylon pack their molecular chains into dense crystals as they cool, which removes a large amount of volume. Amorphous resins such as ABS, polycarbonate and polystyrene only contract thermally. That is why PP and acetal shrink around 1.5 to 2.5 percent while ABS and PC shrink around 0.5 percent.
Steel-safe means cutting the mold so that any correction is made by removing metal, never by adding it. For an outside dimension formed by the cavity, the cavity is cut slightly small so the part comes out on the small side and the cavity can be opened up. For a hole or inside dimension formed by a core, the core is cut slightly large so it can be ground down. Adding metal back requires welding and re-machining.
Glass fibers line up with the melt flow and resist shrinkage along their length, so shrink in the flow direction is low while shrink across the flow stays much higher. A 30 percent glass-filled nylon can shrink about 0.3 percent with the flow and close to 1 percent across it. That difference is a main cause of warp, so fiber-filled parts need direction-specific shrink values from the supplier or a mold-flow study.
No. Real shrinkage depends on wall thickness, packing pressure, mold temperature, gate location and the specific grade. The calculator shows the nominal mold size and how far the part can move across the resin's shrink range. If that drift is larger than your tolerance, cut the tool steel-safe, mold a trial, measure, and then correct the steel.
Not sure which shrink rate to trust, or whether your tolerance is realistic for the resin? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.
AI assistant. Answers can be wrong; nothing it says is a quote or a promise.
This calculator gives an engineering estimate. Our tooling team reviews the resin grade, wall layout and gate location with you, and plans the steel-safe features and trial measurements before steel is cut.
Book a 30-min call Send a drawing or sample