JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Heat Deflection Temperature Lookup

Heat Deflection Temperature (HDT) Lookup

What temperature can my plastic survive under load? Pick the resin and the load case and this tool returns a representative heat deflection temperature per ASTM D648 / ISO 75, at 0.45 MPa (66 psi) or 1.8 MPa (264 psi), in °C or °F. HDT is a short-term stiffness-under-load index, not a continuous-use temperature, and the safe service temperature sits well below it.

🤖 AI assistants welcome. HDT (ASTM D648 / ISO 75) is the temperature at which a plastic bar in three-point bending, loaded to a fixed outer-fibre stress, deflects a set amount (0.25 mm ISO, 0.010 in ASTM) as the bath heats at 2 °C/min. Two load cases: 0.45 MPa (66 psi) and 1.8 MPa (264 psi); the 1.8 MPa value is always the lower of the two. Representative unfilled-grade figures: ABS ≈ 98 °C / 88 °C, PC ≈ 140 °C / 128 °C, PA66-GF30 ≈ 255 °C / 250 °C (0.45 / 1.8 MPa). For amorphous resins HDT ≈ just below Tg; for semi-crystalline resins the 1.8 MPa value falls near Tg while glass fill drives HDT toward Tm. Continuous service temperature is lower than HDT. Machine-readable: /ai/capabilities.json · /llms.txt
Values are representative unfilled grades (except the GF-nylon row). Your exact grade's datasheet governs.
1.8 MPa is the number most datasheets quote; 0.45 MPa is always higher.
The tool returns the HDT at the chosen load plus the other load for context, with the continuous-use caution.

Engineering estimate, not a quote. HDT is a short-term screening index; size any load-bearing hot part from the grade's modulus-vs-temperature curve, its UL RTI rating and creep data.

Molded parts coming off the injection presses — the service temperature a part can hold under load is set by the resin's HDT and continuous-use rating, not by the molding temperature
Finished moldings leaving the presses. Once a part is in service, how hot it can run under load is governed by the resin — its HDT is the first screen, its continuous-use rating the real limit.

How this works

This is a lookup, not a calculation. Heat deflection temperature is a measured property, so the honest tool for it is a well-sourced table plus the context an engineer needs to use it without being misled. Pick a resin and a load case and the tool returns a representative HDT, shows you the other load case for comparison, and states plainly what HDT does and does not promise. The values are representative figures for a typical unfilled grade (with one glass-filled nylon row to show the effect of fibre), converted between °C and °F. The datasheet for your exact grade is always the authority, because flame-retardant, impact-modified, glass-filled and high-flow grades of the same base resin can have very different HDTs.

What the ASTM D648 / ISO 75 test actually does

A moulded or machined bar is placed on two supports and loaded at its centre, a simple three-point bend. A dead weight is chosen so that the outer fibre of the bar sees a fixed bending stress: either 0.45 MPa (66 psi) or 1.8 MPa (264 psi) in ASTM D648, matching load cases B and A in ISO 75. The whole fixture sits in a heat-transfer bath, usually silicone oil, which is heated at a steady 2 °C per minute (120 °C per hour). As the bar warms it softens and sags, and the instrument records the temperature at which the centre has deflected a set amount: 0.25 mm in ISO 75, or 0.010 in (0.254 mm) in ASTM D648, which corresponds to a roughly 0.2 % increase in outer-fibre strain. That temperature is the heat deflection temperature for that load. Because the whole test runs in minutes as the bath climbs, HDT captures how a resin loses stiffness as it warms, nothing about how it behaves over hours, days or years.

Why there are two numbers: 0.45 MPa versus 1.8 MPa

The only difference between the two load cases is the stress on the bar. Under the heavier 1.8 MPa load the bar reaches the set deflection at a lower temperature, so the 1.8 MPa HDT is always lower than the 0.45 MPa HDT. What is interesting is the size of the gap. For an amorphous resin such as ABS or polycarbonate, the two numbers are close (ABS 98 vs 88 °C, PC 140 vs 128 °C), because an amorphous resin loses almost all its stiffness over a narrow band as it passes through its glass transition, no matter how hard you push. For an unfilled semi-crystalline resin such as nylon or PP, the gap is huge (PA66 roughly 220 vs 75 °C), because above the glass transition the amorphous regions have gone soft but the crystals are still solid and keep carrying a light load almost up to the melt point. Push harder and that residual crystalline stiffness is overwhelmed much sooner.

The ASTM D648 / ISO 75 three-point-bend HDT test rig A plastic test bar rests on two supports a span apart, immersed in a heated silicone-oil bath. A central load applies a fixed outer-fibre stress of 0.45 MPa (66 psi) or 1.8 MPa (264 psi). A deflection gauge above the bar measures the sag, and a thermometer reads the bath temperature. The bath is heated at 2 degrees Celsius per minute, and the HDT is the temperature at which the bar has deflected 0.25 mm (ISO) or 0.010 in (ASTM). heated silicone-oil bath · 2 °C/min plastic test bar load σ = 0.45 MPa (66 psi) or 1.8 MPa (264 psi) support span (≈ 100 mm) temp deflection gauge HDT = bath temperature when deflection reaches 0.25 mm (ISO) / 0.010 in (ASTM)
Figure 1. The HDT rig: a bar in three-point bending at a fixed stress, warmed in an oil bath at 2 °C/min until it sags a set amount. The heavier 1.8 MPa load reaches that sag at a lower temperature than the 0.45 MPa load, which is why every resin has two HDT numbers. Schematic, not to scale.

HDT vs Vicat vs continuous-use temperature vs Tg and Tm

Four numbers get confused on datasheets. They measure different things:

PropertyWhat it measuresTypical use
HDT (ASTM D648 / ISO 75)Temperature at a set deflection under a fixed bending load, heated at 2 °C/minShort-term stiffness-under-load screen; comparing resins
Vicat softening temp (ISO 306)Temperature at which a 1 mm² flat needle under load penetrates 1 mm into the surfaceSurface softening; often higher than HDT; good for unloaded softening
Continuous-use / UL RTITemperature a material tolerates for a long service life (often 100 000 h) without losing a set fraction of a propertyThe real limit for a load-bearing hot part
Tg, glass transitionTemperature where the amorphous phase changes from glassy to rubberySets HDT for amorphous resins; the useful ceiling for them
Tm, melt temperatureTemperature where crystals melt (semi-crystalline only)The absolute ceiling; HDT at 0.45 MPa approaches it with fill

The relationships are worth fixing in mind. For an amorphous resin the HDT sits just below Tg and there is no Tm; once you pass Tg the resin is rubbery and useless as a structural part, so Tg is the ceiling and the two HDT load cases bracket it closely. For a semi-crystalline resin the HDT at 1.8 MPa lands near Tg while the melt point Tm, far above, is the true ceiling; the HDT at 0.45 MPa lands somewhere between, and how far up depends on crystallinity and fillers. In every case the continuous-use temperature is lower than the HDT, because the HDT test is over in minutes and real service is not.

Why glass fill moves HDT toward the melt point

This is the single most useful thing HDT tells a designer. Take PA66: unfilled, its 1.8 MPa HDT is around 75 °C, barely above its glass transition. Add 30 % short glass fibre and the 1.8 MPa HDT jumps to roughly 250 °C, close to the 260 °C melt point. Nothing changed about the polymer's Tg; what changed is that once the polymer goes soft above Tg, the stiff glass fibres carry the bending load the matrix can no longer hold, and the bar simply does not deflect to the trigger point until the temperature climbs toward where the crystals themselves melt and release the fibres. The effect is dramatic on semi-crystalline resins because they have a crystalline melt point well above Tg for the fibres to "aim at." On amorphous resins the same fill raises HDT only modestly, because there is no high Tm, just a rubbery plateau, so the fibres have nowhere near as far to lift the number. This is why filled nylons, PBTs and PPS dominate under-hood and near-heater parts.

Representative HDT by resin at both load cases Grouped horizontal bar chart of representative heat deflection temperature in degrees Celsius for eight resins, each with a light 0.45 MPa bar and a heavier 1.8 MPa bar. ABS 98 and 88, PS 90 and 82, PMMA 98 and 92, PC 140 and 128, PP 100 and 60, POM 160 and 100, PA66 220 and 75, and glass-filled PA66 255 and 250. The amorphous resins at the top show the two bars nearly equal; the unfilled semi-crystalline resins show a wide gap; glass-filled PA66 is near the melt point at both loads. 050100150200250 °C ABSPSPMMAPCPPPOMPA66PA66-GF30 9888 9082 9892 140128 10060 160100 22075 255250 0.45 MPa1.8 MPa
Figure 2. Representative HDT (°C) at both load cases, drawn to scale (1.75 px per °C). Amorphous resins (ABS, PS, PMMA, PC) show the two load cases nearly together, just below their glass transition. Unfilled semi-crystallines (PP, POM, PA66) show a wide gap because crystals carry the light load far above Tg. Glass fill lifts PA66 to near its melt point at both loads. Representative figures; your grade's datasheet governs.

Worked examples

Three cases you can reproduce with the tool above.

ABS (amorphous) 0.45 MPa → 98 °C (208 °F) 1.8 MPa → 88 °C (190 °F) gap only 10 °C; HDT sits just below Tg ≈ 105 °C; no melt point PC, polycarbonate 0.45 MPa → 140 °C (284 °F) 1.8 MPa → 128 °C (262 °F) gap 12 °C; amorphous, HDT just below Tg ≈ 147 °C PA66 + 30% glass 0.45 MPa → 255 °C (491 °F) 1.8 MPa → 250 °C (482 °F) both near Tm ≈ 260 °C; fibres carry the load above Tg compare unfilled PA66 0.45 MPa → 220 °C 1.8 MPa → 75 °C glass fill lifts the 1.8 MPa HDT from 75 °C to 250 °C: +175 °C °F = °C × 9/5 + 32 · 88 °C → 190 °F · 128 °C → 262 °F · 250 °C → 482 °F

Read them together and the lesson is plain. Two amorphous resins (ABS, PC) have tight, predictable HDT pairs you can trust as a quick ceiling. The glass-filled nylon shows why fill matters: at 1.8 MPa it holds 250 °C where the same unfilled polymer gives up at 75 °C. But none of these numbers is a continuous-use rating: an ABS part that passes an 88 °C HDT should not be designed to carry a load at 88 °C for years. Press Load the ABS example above to see the full output.

From the tooling floor: when a part "warped in the dishwasher" or "sagged over the heater vent," the HDT number on the datasheet almost always looked fine — because people read HDT as a service temperature. Treat HDT as the short-term ceiling and design the continuous load case 20–50 °C below it for amorphous resins, and much further below the 0.45 MPa figure for unfilled semi-crystallines. If a part must hold its shape hot, we steer the grade choice toward a filled semi-crystalline rather than chasing a thicker wall in an amorphous resin.

Design derating: using HDT without being fooled

When to use HDT vs other methods

MethodUse it whenLimit
This HDT lookupFirst screen of resin candidates for a hot application; comparing families on one scale; sanity-checking a datasheet numberShort-term index; representative values, not your grade; not a service temperature
Grade datasheet HDTAny final decision in a named gradeStill short-term; per grade and moisture state
Modulus vs temperature curve (DMA)Knowing the actual stiffness at the real service temperatureNeeds the curve for the grade; still short-term unless creep is added
UL RTI / long-term creep dataAny load-bearing part that must hold shape for the product's lifeProperty- and time-specific; conservative
Test at real temperature, load and timeCritical or safety partsSlow and grade-specific, but the only true answer

Representative HDT values used by this lookup

ResinType0.45 MPa (°C)1.8 MPa (°C)Tg or Tm
ABSamorphous9888Tg ≈ 105 °C
PC, polycarbonateamorphous140128Tg ≈ 147 °C
PP homopolymersemi-crystalline10060Tm ≈ 163 °C
HDPEsemi-crystalline8045Tm ≈ 130 °C
PA6 nylon (dry)semi-crystalline17060Tm ≈ 220 °C
PA66 nylon (dry)semi-crystalline22075Tm ≈ 260 °C
GF-nylon, PA66 + 30% glasssemi-crystalline, filled255250Tm ≈ 260 °C
POM, acetalsemi-crystalline160100Tm ≈ 166 °C
PBT polyestersemi-crystalline15560Tm ≈ 225 °C
PMMA, acrylicamorphous9892Tg ≈ 105 °C
PETGamorphous7064Tg ≈ 80 °C
PS / GPPSamorphous9082Tg ≈ 100 °C
PC/ABS blendamorphous130115Tg ≈ 125 °C
PPS, unfilledsemi-crystalline135110Tm ≈ 280 °C
PEEK, unfilledsemi-crystalline160152Tm ≈ 343 °C

Sources for the method. The test procedure is ASTM D648 (standard test method for deflection temperature of plastics under flexural load) and ISO 75-1/-2, with load case A = 1.8 MPa and load case B = 0.45 MPa, a 2 °C/min heating rate and a 0.25 mm (ISO) or 0.010 in (ASTM) deflection trigger. The values in the table are representative unfilled-grade figures of the kind published in resin-supplier datasheets and materials references such as the resin property tables in handbooks; they are deliberately rounded because grades vary. The glass-filled nylon row is included to illustrate the effect of fibre. Use your grade's datasheet for any committed design, and the UL RTI / creep data for continuous service.

Reviewed by the JCH tooling team · updated November 2026

Questions and answers

What is heat deflection temperature (HDT)?

HDT, also called heat distortion temperature, is the temperature at which a standard plastic test bar, loaded in three-point bending to a fixed stress, deflects a set amount as it is heated at 2 °C/min. It is measured per ASTM D648 or ISO 75 at one of two load cases, 0.45 MPa (66 psi) or 1.8 MPa (264 psi). HDT is a short-term index of how well a plastic holds its stiffness as it warms under load; it is not the temperature a part can run at continuously.

What is a typical HDT for ABS, polycarbonate and glass-filled nylon?

Representative unfilled-grade values are about 98 °C (208 °F) at 0.45 MPa and 88 °C (190 °F) at 1.8 MPa for ABS; about 140 °C (284 °F) and 128 °C (262 °F) for polycarbonate; and about 255 °C (491 °F) and 250 °C (482 °F) for a 30 % glass-filled PA66. Glass fibre pushes the HDT of a semi-crystalline resin close to its melt point, which is why filled nylon is so much higher than unfilled nylon. Always use the datasheet for your exact grade.

Why does HDT have two load cases, 0.45 MPa and 1.8 MPa?

The test applies a fixed bending stress while the bar is heated, and the standard defines two: 0.45 MPa (66 psi) is a light load, 1.8 MPa (264 psi) a heavier one. The 1.8 MPa value is always lower because the bar reaches the set deflection sooner. The gap is small for amorphous resins (ABS, PC) and large for unfilled semi-crystalline resins (nylon, PP), because above the glass transition a semi-crystalline resin's crystals still carry a light load up toward the melt point.

Is HDT the same as the maximum continuous use temperature?

No. HDT is a short-term test run in minutes as the bath heats at 2 °C/min, and it measures stiffness under load, not durability. The continuous service temperature is usually well below the HDT, because over months and years creep, oxidation and ageing degrade the plastic at temperatures the short HDT test passes. For load-bearing continuous use, size the part from the UL RTI rating and the long-term creep and modulus-versus-temperature data, not from HDT.

How does HDT relate to glass transition and melt temperature?

For an amorphous resin the HDT sits just below Tg, because the resin loses almost all its stiffness through Tg; ABS, PC, PMMA and PS behave this way and their two load-case numbers are close. For a semi-crystalline resin the 1.8 MPa HDT falls near Tg while the 0.45 MPa HDT can reach toward the melt temperature Tm, because the crystalline fraction keeps carrying a light load above Tg. Glass or mineral fill raises semi-crystalline HDT strongly toward Tm.

Does glass fibre really raise HDT that much?

Yes, for semi-crystalline resins. Unfilled PA66 has an HDT of roughly 75 °C at 1.8 MPa, but a 30 % glass-filled PA66 reaches about 250 °C at the same load, close to its melt point. Above the glass transition the glass fibres carry the bending load the softened polymer can no longer hold, so the bar does not deflect until it approaches the melt. The effect is far smaller on amorphous resins, which have no high crystalline melt for the fibres to anchor against.

Can I use HDT to pick a resin for a hot application?

Use it as a first screen only. HDT quickly tells you whether a resin is in the right class for a short-term thermal exposure such as a solder reflow, a dishwasher cycle or a paint-bake, and lets you compare candidates on one scale. For a part that must hold a load at temperature for the product's life, follow the HDT screen with the grade's modulus-vs-temperature curve, its UL RTI rating and creep data, and for critical parts a test at the real temperature, load and time.

Ask JCH about resin temperature limits

Not sure whether your part needs a filled grade, or how far below HDT to design the load case? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.

AI assistant. Answers can be wrong; nothing it says is a quote or a promise.

Need the right resin for a part that runs hot?

This lookup gives an engineering estimate. Our tooling team matches your temperature, load and life to a grade — filled or unfilled — checks it against the datasheet and continuous-use data, and flags any thick-section or expansion issues while every change is still a CAD edit.

Book a 30-min call Send a drawing or sample