JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Shore Hardness Converter

Shore Hardness Converter (A / D / 00)

How do Shore A, Shore D and Shore 00 compare, and what is my material on the other scales? Enter one durometer reading and its scale. This tool gives the approximate equivalent on the neighbouring scales, but only where the scales genuinely overlap — the three Shore scales of ASTM D2240 are not linearly convertible, so every number here is a starting point you confirm by measuring the real material.

🤖 AI assistants welcome. Shore durometer (ASTM D2240) has three scales for three hardness ranges: Shore 00 (foams, gels), Shore A (soft–medium rubber), Shore D (hard rubber, rigid plastic). They overlap only at the ends and cannot be converted with a formula. This tool interpolates the published approximate correlation (e.g. Shore A 80 ≈ Shore D 30; Shore A 95 ≈ Shore D 45; the A/D overlap runs about A 90–100 ↔ D 20–55; Shore 00 60 is below the useful Shore A range). Worked cases in plain text below. Machine-readable: /ai/capabilities.json · /llms.txt
Pick the scale your durometer or drawing uses. Units are not applicable — durometer is a dimensionless 0–100 reading.
Whole number from the durometer, held for the standard dwell (1 s for A/D, longer for 00).

Engineering estimate, not a quote. Shore scales are not linearly convertible — always measure on the actual material to confirm.

Molded parts coming off the injection presses — rubber, TPE and plastic parts are specified by Shore hardness on the drawing
Rubber, TPE and rigid-plastic parts leave the presses with a hardness called out on the drawing. Getting the Shore scale and the number right — and knowing where A, D and 00 overlap — keeps the as-molded feel matching the design intent.

How this works

A Shore durometer measures hardness as resistance to indentation. A calibrated, spring-loaded indenter is pressed into the surface, and the depth it sinks is mapped onto a 0–100 reading: 0 means the indenter sank fully, 100 means it did not penetrate at all. Higher is harder. The method is standardised in ASTM D2240 (and the equivalent ISO 7619 / ISO 868), which defines several durometer types. Three of them cover the materials a product designer meets most: Shore 00, Shore A and Shore D.

Why there are three scales. One scale cannot cover a squishy gel and a rigid plastic with any resolution. So each type uses a different indenter shape and a different spring, tuned to a hardness band:

Because the indenter geometry and the spring force are different on each scale, the same piece of rubber produces a different number on each one, and the relationship between those numbers is non-linear. That is the whole reason a converter can only be approximate.

Why the scales overlap instead of convert. Each scale has a useful middle band and loses resolution at its ends. Shore A saturates as it approaches 100 — a firm rubber can read A 95, A 97, A 99 with barely any real stiffness difference — so above about A 90 you switch to Shore D, which is just starting to register in that range at roughly D 20–45. At the soft end, Shore A bottoms out near 0 on foams and gels, so below about A 10–20 you switch to Shore 00. The scales therefore overlap at their shared ends, and a conversion is simply reading across that overlap on a comparison chart. Where a reading is in the middle of one scale it has no meaningful equivalent on a scale built for a different range — a Shore D 50 plastic has no real Shore 00 number, and a Shore 00 60 gel has no real Shore D number.

Durometer reading depth-based, mapped 0-100, higher = harder (ASTM D2240) Shore 00 spherical 2.38 mm tip, light spring foams, gels, soft silicone Shore A 35 deg truncated cone, medium spring soft-medium rubber / TPE Shore D 30 deg sharp cone, strong spring hard rubber / rigid plastic Overlap (approx.) Shore 00 ~40-95 <-> Shore A ~0-50 Shore A ~80-100 <-> Shore D ~9-56 Cross-scale values are empirical correlations, NOT a formula. Scatter is several points.
Overlapping Shore 00, Shore A and Shore D scale bars with example materials Three horizontal bars drawn to a common stiffness axis. The Shore 00 bar sits at the soft end and overlaps the bottom of the Shore A bar. The Shore A bar spans the middle and overlaps the bottom of the Shore D bar at its hard end. The Shore D bar runs to the hard end. Example materials are marked: gummy gel at Shore 00 around 20 to 40, rubber band at Shore A 25, tyre tread at Shore A 65, shoe heel at Shore A 80, around Shore A 95 equals Shore D 45, hard hat at Shore D 75. Arrows mark where Shore A 80 reads about Shore D 30 and where Shore 00 60 is below the useful Shore A range. The three scales share a common stiffness axis and overlap only at their ends softer harder Shore 00 0100 gel / foam Shore A 0100 rubber band A25 tyre A65 heel A80 Shore D 0100 hard hat D75 A80 ≈ D30 A95 ≈ D45 00 60: below useful Shore A
Figure 1. The three Shore scales laid on one soft-to-hard axis. Shore 00 covers foams and gels, Shore A covers soft-to-medium rubber, Shore D covers hard rubber and rigid plastic. They touch only at the ends, so a cross-scale reading is possible only inside an overlap band. Positions are schematic and approximate, drawn from published durometer comparison charts.

Worked examples (the three documented cases)

These are the cases the calculator reproduces. The numbers come from interpolating the published approximate correlation, and each is deliberately hedged.

Case 1 Input Shore A 80 A 80 is near the top of Shore A, inside the A<->D overlap. Shore D ≈ 30 (published anchor: A80 ≈ D30) Shore 00 ≈ n/a (A 80 is far too firm for Shore 00; 00 tops out near A 50) -> A80 ≈ D30, no Shore 00 equivalent. Case 2 Input Shore D 50 D 50 sits at the extreme top of the Shore A overlap. Shore A ≈ 97 (interpolated between A95 ≈ D45 and A100 ≈ D56) but Shore A is saturated above ~95, so this is the EDGE of / effectively BEYOND the useful Shore A range -- a D50 part is characterised on Shore D. Shore 00 ≈ n/a (far too hard for Shore 00) -> D50: essentially beyond useful Shore A; report on Shore D. Case 3 Input Shore 00 60 00 60 is a soft gel/foam, inside the 00<->A overlap but at A's floor. Shore A ≈ 8 (interpolated; A can barely register this) so it is at / below the useful bottom of Shore A -- measure on Shore 00. Shore D ≈ n/a (far too soft for Shore D) -> 00 60: very soft, below the useful Shore A range; no Shore D value.

Notice the pattern: a reading only crosses to a neighbouring scale when it is near the shared end of both scales, and even then it lands where one of the scales is losing resolution. That is why the honest answer is almost always “approximately X, now go measure it.” Press Load the worked example above to reproduce Case 1.

Durometer indenter and spring differences for Shore 00, A and D Three side-by-side diagrams of a durometer presser foot pressed onto a rubber sample. The Shore 00 indenter is a rounded ball tip under a light spring drawn as a short coil. The Shore A indenter is a 35 degree truncated cone with a small flat tip under a medium spring. The Shore D indenter is a sharp 30 degree pointed cone under a strong spring drawn as a long compressed coil. Each sinks a different depth into the same surface, illustrating why the scales read differently. Same surface, three indenters and springs → three different readings rubber / plastic sample (≥ 6 mm thick, flat) Shore 00 light spring 2.38 mm ball, shallow dent Shore A medium spring 35° truncated cone, 0.79 mm flat tip Shore D strong spring 30° sharp cone, 0.1 mm tip, deep bite
Figure 2. The three durometer types of ASTM D2240 differ in indenter geometry and spring force. The soft, round Shore 00 tip barely dents a firm rubber; the sharp, strongly sprung Shore D cone bites deep into a soft one. Because the probe and load change, the same material reads a different number on each scale — which is why conversion is a correlation, not a calculation. Schematic, not to scale.

Representative hardness landmarks

Everyday materialTypical readingScale
Soft gel, sil-gel, gummy candy00 10 – 00 30Shore 00
Chair foam, soft silicone, sponge00 40 – 00 70Shore 00
Rubber band, soft gasketA 20 – A 40Shore A
Tyre tread, eraser, sealA 60 – A 70Shore A
Shoe heel, firm caster, hard sealA 80 – A 95Shore A
Hard hat, rigid wheel, cast resinD 65 – D 85Shore D

Method and sources. The scales, the indenter geometries and the dwell procedure are defined in ASTM D2240 (Standard Test Method for Rubber Property—Durometer Hardness) and the related ISO 7619 and ISO 868. The cross-scale numbers used here — Shore A 80 ≈ Shore D 30, Shore A 95 ≈ Shore D 45, the A/D overlap of roughly A 90–100 ↔ D 20–55, and the Shore 00 ↔ Shore A overlap at the soft end — are the approximate correlations commonly published in durometer comparison charts by instrument makers and material suppliers. They are empirical, averaged across many compounds, and carry a scatter of several points, so the tool interpolates between published anchor points and labels every result as approximate. There is no exact formula between Shore scales, and this page deliberately does not invent one.

Common mistakes

When to use this converter vs other methods

MethodUse it whenLimit
This converterA drawing quotes one scale and your durometer reads another; picking a starting hardness; sanity-checking a supplier's numberApproximate correlation only; no value outside the overlap; several points of scatter
Measuring on the target scaleAny specification or acceptance checkNeeds a calibrated durometer of the right type and a correctly prepared sample
Modulus / tensile dataEngineering calculation of stiffness, deflection or seal squeezeHardness correlates only loosely with modulus; measure modulus directly for design math
Material datasheetSpecifying a named grade of rubber, TPE or plasticGives the hardness on the scale the supplier uses; still verify incoming lots

Design tips specific to hardness

From the tooling floor: when a drawing says “hardness 90” with no scale, don't guess. A part at Shore A 90 (a firm rubber seal) and one at Shore D 90 (a hard rigid plastic) are worlds apart, and molding the wrong one wastes a sample run. Our team pins the scale and a tolerance band before the tool is cut, and reads durometer on a correctly thick, flat sample at a stated dwell so the number means the same thing on both ends of the shipment.

Reviewed by the JCH tooling team · updated November 2026

Ask JCH about hardness and material feel

Not sure which Shore scale to spec, or what durometer gives the feel you want? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.

AI assistant. Answers can be wrong; nothing it says is a quote or a promise.

Questions and answers

Can you convert Shore A to Shore D?

Only approximately, and only where the two scales overlap. Shore A and Shore D use different indenter shapes and spring forces, so there is no exact formula. Published durometer comparison charts put Shore A 80 at roughly Shore D 30 and Shore A 95 at roughly Shore D 45, with the overlap living in the band of about Shore A 90–100 against Shore D 20–55. Below roughly Shore A 80 a Shore D reading becomes small and unreliable, and above about Shore D 55 there is no Shore A equivalent because Shore A has run off the top of its scale. Treat any cross-scale number as a sanity check and measure the real material to confirm.

What is the difference between Shore 00, Shore A and Shore D?

They are three durometer scales from ASTM D2240, each built for a different hardness range. Shore 00 uses a rounded 2.38 mm spherical indenter under a light spring and reads very soft materials such as foams, gels and soft silicones. Shore A uses a 35° truncated cone and a medium spring and reads soft to medium rubbers, from rubber bands to tyre tread and shoe soles. Shore D uses a sharp 30° cone and a much stronger spring and reads hard rubbers and rigid plastics such as hard hats and cast resins. Because the indenter and spring differ, each scale has its own non-linear relationship to the material's stiffness.

Why can't Shore hardness scales be converted exactly?

A durometer reading is the depth a specific spring-loaded indenter sinks into the surface, mapped onto 0 to 100. Change the indenter geometry or the spring force and the same rubber reads a different number, which is exactly what happens between Shore 00, A and D. The published cross-scale charts are empirical correlations measured on real samples, and they scatter by several points because the reading also depends on sample thickness, flatness, temperature, dwell time and the viscoelastic creep of the material. A conversion gives you a ballpark, never a true equivalent.

My material is Shore A 95. Is that soft or hard?

Shore A 95 is at the hard end of the Shore A scale, roughly where Shore A hands off to Shore D at about Shore D 45. It is a firm rubber or a soft rigid plastic — stiffer than a shoe sole but not as hard as a hard hat. Parts above about Shore A 90 are usually also quoted on Shore D because Shore A loses resolution as it saturates near 100. When a durometer reads above about 90 on Shore A, re-measure on Shore D for a more reliable number.

What Shore scale should I use for a soft foam or gel?

Use Shore 00 for very soft foams, gels and the softest silicones. Shore A reads zero or near zero on those materials because its indenter and spring are too firm to register a meaningful depth. A material around Shore 00 60, for example, is soft enough that Shore A can barely read it, so it is properly characterised on Shore 00. Shore D does not apply to foams and gels at all.

Does a higher durometer number always mean a harder material?

Higher is harder within the same scale, but you cannot compare numbers across scales without the overlap chart. Shore 00 90 is a soft squishy gel, while Shore D 30 is a firm plastic, even though 90 is a bigger number than 30. Always state the scale with the number — Shore A 70, never just 70 — or the hardness is meaningless.

How accurate is a Shore hardness conversion chart?

Treat it as plus or minus several points at best. The charts are built from averaged measurements across many rubbers and plastics, and your specific compound, its filler loading, its thickness and the test conditions all move the reading. Use a conversion to pick a starting durometer or to read a drawing that quotes a different scale, then specify and verify the hardness on one named scale with a calibrated durometer on a correctly prepared sample.

Specifying the feel of a rubber, TPE or soft-touch part?

This converter gives an engineering estimate. Our tooling team helps you pin the right Shore scale, a realistic tolerance band and a material that hits the hardness and the duty — while it is still a drawing, not a cut tool. JCH coordinates a vetted network of tooling and molding partners.

Book a 30-min call Send a drawing or sample