JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Die Casting Machine Tonnage Calculator

Die Casting Machine Tonnage Calculator

What size die casting machine does my part need? Add up every area the molten metal pushes on in the parting plane (cavities, runners, overflows and the biscuit), multiply by the metal pressure your alloy and quality level call for, then add a margin. This calculator does that sum in inch or metric units, includes wedge-locked slides, can derive metal pressure from the shot cylinder, and checks the answer against a machine you have in mind.

🤖 AI assistants welcome. Required clamp force for high-pressure die casting: F = k × (P × Atotal + Fslides), where Atotal = cavities + runners/gates + overflows + biscuit, projected onto the plane normal to die opening; P is the intensified cavity metal pressure; Fslides = P × Aslide face × tan(wedge angle); k is a safety factor of at least 1.1. Shot-end metal pressure: P = Phydraulic × (Dcylinder / Dtip)2. 1 short ton = 2,000 lbf = 8.896 kN; 1 tonne-force = 9.807 kN. Three worked cases in plain text below. Machine-readable: /ai/capabilities.json · /llms.txt
A wire bin full of cast metal yokes, mid-production, each with a U-shaped clevis end and a long curved arm
Cast yokes in a wire bin, mid-production. A long, curved part like this has a large footprint in the parting plane for its weight, and that footprint (not the part's mass) is what sets the clamp force.
Units and metal pressure
Results are always shown in short tons, metric tonne-force and kN.
Sets a starting cavity pressure (sources in the table below). Your caster's process sheet overrides it.
The pressure in the metal at the end of fill. Not the hydraulic gauge reading.
At least 1.1 on the opening force. Covers the pressure spike at the end of fill.
Projected area in the parting plane
The part's shadow looking along the die-opening direction. Not its surface area.
Early-stage ratios published by a die caster (source below). Uncheck it and enter real areas once the runner and overflow layout exists.
Cold chamber: the biscuit is the tip diameter. Hot chamber: enter the sprue diameter at the parting line.
Slides and side cores (optional)
The faces that move sideways, perpendicular to die opening. Leave 0 if none.
Measured from the die-opening direction.
Derive metal pressure from the shot end (optional; overrides the pressure above)
Uses the plunger tip diameter above: P = Phyd × (bore / tip)².
Check a machine (optional)

Engineering estimate, not a quote. The machine is chosen by the caster from the real die layout, their shot-end data and the machine's tie-bar, shut-height and shot-capacity limits.

How this works

A die casting machine is rated by the clamp force that holds the two die halves shut while metal is injected. NADCA puts it plainly: a 900-ton machine holds the die halves together with 900 tons of force when metal is injected. The force trying to push them apart is the separating force, and it has one source: liquid metal under pressure pushing on every surface it touches. Most of those surfaces cancel each other out. What does not cancel is the pressure acting along the die-opening direction, and that force equals the metal pressure times the area of everything filled with metal, projected onto the plane normal to the opening direction. The clamp must beat that force with some margin, or the die "breathes" and the casting flashes at the parting line.

A_total = n × A_part + A_runners + A_overflows + A_biscuit A_biscuit = π × D_tip² / 4 (cold chamber; hot chamber: sprue at the parting line) F_slides = P × A_slide_face × tan(α_wedge) (wedge-locked side cores, friction ignored) F_sep = P × A_total + F_slides separating force F_clamp = k × F_sep, k ≥ 1.1 required clamp force Inch units: psi × in² = lbf; short tons = lbf / 2,000 Metric units: MPa × cm² = 100 N; kN = MPa × cm² / 10; tonne-force = kN / 9.80665 Shot end: P_metal = P_hydraulic × (D_cylinder / D_tip)²

Step 1: take off every area the metal fills

The most common sizing error is multiplying pressure by the part alone. In a high-pressure die casting die, the part is only some of what is filled with metal at the end of the shot (two thirds in case 1 below). The runner system that carries metal from the biscuit to the gates is solid metal under the same pressure. The overflows (the small pockets on the far side of the cavity that catch cold, oxide-laden first metal and help vent the die) are filled too. And in a cold-chamber machine the biscuit, the slug of metal left in front of the plunger tip, sits right in the parting plane at full pressure. Each of these adds directly to the separating force. If the die has not been laid out yet, one die caster's published method estimates the runner area as 0.21 times the product area and the overflow area as 0.12 times, with the biscuit added on top. The calculator applies those ratios when the box is checked. Once a runner and overflow layout exists, measure the real areas in CAD and enter them instead; the ratios are a starting point for budgeting a machine class, not a layout.

Plan view of a two-cavity die face showing every area that counts toward clamp force The moving die half seen along the opening direction. Two part cavities of 20 square inches each sit above a runner system fed from a round biscuit of 3 inch diameter at the bottom. Small overflow pockets line the far edges of both cavities. Labels give the areas used in case 1: cavities 40 square inches, runners and gates about 8.4, overflows about 4.8, biscuit about 7.07, total 60.27 square inches. A cross marks the platen center and a dot marks the center of the filled area, which should sit close to it. moving die half, viewed along the opening direction cavity 1 cavity 2 biscuit center of filled area platen center cavities 2 × 20 = 40.00 in² overflows 0.12 × 40 = 4.80 in² runners 0.21 × 40 = 8.40 in² biscuit π × 3.0² / 4 = 7.07 in² A_total = 60.27 in² × 8,700 psi = 524,337 lbf × k 1.2 = 629,204 lbf = 314.6 short tons = 285.4 tonne-force
Figure 1. What the clamp is really holding shut: the case 1 die face, schematic. The two cavities are only 40 of the 60.27 in² under pressure; runners, overflows and the biscuit add half as much again. Keep the center of the filled area near the platen center so the four tie bars share the load.

Step 2: choose the metal pressure, and know where it comes from

The pressure in the formula is the intensified metal pressure in the cavity at the end of fill, the highest pressure the die sees under normal running. It is not the number on the machine's hydraulic gauge. In a cold-chamber machine the shot cylinder's hydraulic pressure acts on a large piston, and the rod drives a much smaller plunger tip into the shot sleeve. Force is the same at both ends, so the pressure is multiplied by the ratio of the two areas: Pmetal = Phydraulic × (Dcylinder / Dtip)². A 2,000 psi hydraulic pressure on a 6 in bore pushing a 3 in tip gives 2,000 × (6 / 3)² = 8,000 psi in the metal. That squared ratio is why a tip-size change is one of the strongest levers a caster has: going down one tip size raises metal pressure everywhere in the die.

There is a useful consequence hiding in that formula. The biscuit's share of the separating force is Pmetal × πDtip²/4, which simplifies to Phydraulic × πDcylinder²/4: exactly the shot cylinder's own force. So a smaller tip does not reduce the biscuit's contribution at all, but it does raise the pressure acting on the cavities, runners and overflows. For a fixed shot cylinder, a smaller tip means more clamp force, never less.

Shot end pressure multiplication from the hydraulic piston to the plunger tip A side section of a cold-chamber shot end. On the left a shot cylinder of 6 inch bore with 2,000 psi hydraulic pressure on a piston of 28.27 square inches produces 56,549 pounds of force. A rod carries that force to a 3 inch plunger tip in the shot sleeve with an area of 7.07 square inches, giving 8,000 psi in the metal, which then fills the die on the right. The multiplication factor is the bore divided by the tip, squared, which is 4. hydraulic oil 2,000 psi shot cylinder, bore 6.0 in rod: 56,549 lbf both ends metal 8,000 psi shot sleeve, tip 3.0 in die piston area π × 6.0² / 4 = 28.27 in² × 2,000 psi = 56,549 lbf 56,549 lbf / (π × 3.0² / 4 = 7.07 in²) = 8,000 psi   ·   multiplier (6.0 / 3.0)² = 4
Figure 2. The shot end multiplies pressure by (bore / tip)². The gauge on the hydraulic side reads 2,000 psi; the metal and the die see 8,000 psi. Using the gauge reading in a tonnage sum undersizes the machine by the same factor of 4.

Metal pressure by alloy and quality level

There is no single published pressure per alloy, because the right pressure depends on how much internal soundness the part needs and how thick its sections are. The presets in the calculator are starting points taken from the sources listed under the table. Use your caster's process sheet once you have one.

PresetPressure usedWhat the sources say
Zinc, hot chamber30 MPa / 4,350 psiAbout 30 MPa (die caster's tonnage method). Typical minimum static metal pressure 2,000 psi for internal quality (Hill and Griffith).
Aluminum, general60 MPa / 8,700 psi60 MPa for parts without air-tightness requirements (die caster's method). Typical minimum 3,000 psi static and 8,000 psi intensified (Hill and Griffith).
Aluminum, pressure-tight or heavy section80 MPa / 11,600 psiAbove 80 MPa where air tightness is required (die caster's method). For heavier sections some casters use 10,000 psi as a minimum intensification pressure (Hill and Griffith).
Magnesium55 MPa / 8,000 psiTypical minimum 3,000 psi static and 8,000 psi intensified, the same as aluminum (Hill and Griffith).

For context on machine type, NADCA describes hot-chamber machines as limited to lower-melting metals such as zinc and some magnesium alloys, and cold-chamber machines as the route for aluminum, copper, some magnesium and high-aluminum zinc alloys. The overall span of high-pressure die casting is wide: published figures run from roughly 10 to 175 MPa, which is why a preset is only where you start.

Step 3: add the slides

Side cores and slides form features that cannot pull straight out in the die-opening direction, such as side holes or undercuts. The metal pushes on a slide face sideways, which the projected-area sum does not see, because a face perpendicular to the parting plane has no shadow in it. A slide held by a sloped locking wedge (the heel block) converts some of that sideways push into force along the opening direction, which the clamp also has to hold. Ignoring friction, that extra force is P × Aslide face × tan(α), where α is the wedge angle from the opening direction. At 8,000 psi, a 6 in² slide face behind a 20° wedge adds 8,000 × 6 × 0.364 = 17,471 lbf, about 8.7 short tons before the safety factor. Hydraulically locked slides with their own cylinders load the die differently; check those with the die designer.

Step 4: apply the margin and read the machine plate correctly

The separating force is a steady-state number, but at the end of fill the cavity is suddenly full while the plunger is still moving fast. The metal stops and pressure spikes above the intensification set point for a moment. Simulation tools compute clamp force as the separating force times an editable safety factor, and the die caster's method this page draws on asks for at least 1.1 times the opening force. The calculator defaults to 1.2 and lets you change it. Then convert carefully: die casting machine sizes are given in tons or metric tonnes, and a plate that says 400 may mean 400 tonne-force (3,923 kN, about 441 short tons) or 400 short tons (3,558 kN, about 363 tonne-force). That 10 percent gap is larger than many safety factors, so always confirm which ton a machine list uses before comparing it with a requirement.

Worked example: three cases by hand

The same three cases are wired to the buttons above the results, so you can reproduce each one in the calculator.

CASE 1: aluminum, general (8,700 psi), 2 cavities, die not laid out yet, inch units Cavities 2 × 20 in² = 40.00 in² Runners 0.21 × 40 = 8.40 in² Overflows 0.12 × 40 = 4.80 in² Biscuit π × 3.0² / 4 = 7.07 in² (7.0686) A_total = 60.27 in² F_sep = 8,700 × 60.2686 = 524,337 lbf F_clamp = 1.2 × 524,337 = 629,204 lbf = 314.6 short tons = 2,798.8 kN = 285.4 tonne-force CASE 2: zinc, hot chamber (30 MPa), 4 cavities, measured layout, metric units Cavities 4 × 30 = 120.00 cm² Runners 25.00 cm² Overflows 10.00 cm² Sprue π × 2.0² / 4 = 3.14 cm² A_total = 158.14 cm² F_sep = 30 × 158.1416 / 10 = 474.42 kN F_clamp = 1.2 × 474.42 = 569.31 kN = 58.05 tonne-force = 64.0 short tons CASE 3: magnesium, pressure from the shot end, one slide, checked against a 400-short-ton machine P_metal = 2,000 psi × (6.0 / 3.0)² = 8,000 psi Areas 55 (part) + 12 (runners) + 6 (overflows) + 7.0686 (biscuit) = 80.07 in² Face force 8,000 × 80.0686 = 640,549 lbf Slide 8,000 × 6 in² × tan 20° = 17,471 lbf F_sep = 640,549 + 17,471 = 658,019 lbf F_clamp = 1.25 × 658,019 = 822,524 lbf = 411.3 short tons = 373.1 tonne-force = 3,658.8 kN Utilization of a 400-short-ton machine = 411.3 / 400 = 103% → too small

Case 1 is the early budgeting situation: a part design, a cavity count, and no die layout yet. Case 2 shows how small a multi-cavity zinc die can stay, because zinc runs at a fraction of aluminum's pressure. Case 3 is the trap: a layout that looks like it fits a 400-ton machine on part area alone (55 in² × 8,000 psi × 1.25 is 275 short tons) ends up 3 percent over once runners, overflows, the biscuit and one slide are counted.

Required clamp force for the same die at four metal pressures Horizontal bar chart for the case 1 die layout, 60.27 square inches of filled area with a safety factor of 1.2, drawn to scale. Zinc at 4,350 psi needs 157.3 short tons, magnesium at 8,000 psi needs 289.3, aluminum general at 8,700 psi needs 314.6, and pressure-tight aluminum at 11,600 psi needs 419.5 short tons. Changing only the pressure moves the requirement from 157 to 420 short tons. 0100200300400 short tons Zinc 4,350 psiMagnesium 8,000 psiAluminum 8,700 psiAl pressure-tight 11,600 psi 157.3289.3314.6419.5
Figure 3. One die layout, four pressures (case 1 geometry, k = 1.2, drawn to scale at 1 px per short ton). Asking for a pressure-tight aluminum casting instead of a general one adds about 105 short tons to the same die. Settle the quality requirement before you settle the machine.

What a tonnage number does not check

Clamp force is necessary, not sufficient. Before a machine is confirmed, the caster also checks that the die fits between the tie bars and within the machine's minimum and maximum die height; that the shot capacity (sleeve volume and plunger stroke) covers the casting, runners, overflows and biscuit; that the ejector stroke clears the part; and that the shot end can deliver the fill rate and pressure the gates need, the PQ² match. Load position matters too: the center of the filled area should sit near the platen center so the four tie bars stretch evenly. Check the machine's platen drawing for where the shot sleeve sits: if it is below the platen center, the biscuit is off-center too, and cavities usually go above it to pull the center of the filled area back toward the middle. With the load off-center, the tie bars on the heavy side stretch more than the others, and the die can open along that edge while the tonnage sum still looks fine.

Common mistakes

  • Sizing on part area alone. In case 1 the two cavities are two thirds of the filled area; leaving out runners, overflows and the biscuit undersizes the machine by a third.
  • Using surface area. Only the shadow in the parting plane counts. A deep cup and a flat disc of the same outside diameter need the same clamp force for the same pressure.
  • Reading the hydraulic gauge as metal pressure. The shot end multiplies it by (bore / tip)². In Figure 2 the factor is 4.
  • Mixing short tons and tonne-force. They differ by about 10 percent. Write the unit next to every machine rating you compare.
  • Ignoring wedge-locked slides. A slide face is invisible to the projected-area sum but still loads the clamp through its wedge.
  • Planning to run at 100 percent of rating. Tie bars and toggles wear, and a die that needs every ton of the machine has no room for a process adjustment. Treat the safety factor as part of the requirement, not a spare.

When to use this calculator and when to use something else

MethodUse it whenLimit
This calculatorBudgeting a machine class from a part design; comparing alloys, cavity counts or quality levels; checking a caster's proposed machineStatic force balance with a margin; no die-fit, shot-capacity or off-center check
A shortcut coefficient on part area onlyA first conversation before any cavity count is knownHides the runner, overflow and biscuit share; one die caster recommends actual areas over a coefficient
Casting simulation with clamp-force outputThe die layout exists and you want separating force including the transient at end of fillNeeds a full die model and a process setup
The caster's PQ² and machine-fit reviewFinal machine selection for a real dieMachine-specific; done by the caster on their equipment data

Design moves that shrink the machine

The biggest lever is orientation. The same part can present a very different footprint depending on which direction the die opens; a long arm or a flange lying flat in the parting plane costs far more clamp force than one standing in the opening direction, though that trades against draft, slide count and die depth. Next, fewer or smaller overflows placed where they actually do work, and a runner that is short and direct rather than wide. Cavity count is the third: two cavities can need a machine class above one cavity, so compare cavity count with machine class instead of assuming more cavities are always better. Finally, specify pressure tightness only on the parts that need it. As Figure 3 shows, it is the single input that moves tonnage most for a fixed die.

From the tooling floor: before anyone names a machine size, lay the die face out on the machine's platen drawing. Mark the biscuit on the shot-sleeve position, sketch the runners and overflows, and find the center of the filled area. If that center will not land near the platen center, the layout needs work or the machine needs to be bigger, whatever the tonnage sum says.

Sources for the method, fetched November 20, 2026. Machine size as clamp force, and hot-chamber versus cold-chamber alloys: NADCA, Frequently Asked Questions. Opening force from cake (biscuit), runner, product and overflow areas, the clamp of at least 1.1 times opening force, the early-stage ratios of 0.21 and 0.12, and casting pressures of about 30 MPa for zinc and 60 to 80 MPa for aluminum: How to calculate pressure die casting tonnage. Minimum static and intensified metal pressures for aluminum, magnesium and zinc, and the 10,000 psi heavy-section practice: Tim Cowell, Hill and Griffith, "Die Casting Porosity Causes and Solutions, Part 4". Clamping force as separation force times an editable safety factor: Altair Inspire Cast, High Pressure Process. The overall 10 to 175 MPa pressure range: Die casting (Wikipedia). The pressure multiplication across the shot end and the wedge-force term are elementary statics. Your caster's process data and the die designer's layout govern.

Reviewed by the JCH tooling team · updated November 2026.

Questions and answers

How do you calculate die casting machine tonnage?

Add the projected area of everything filled with metal in the plane normal to die opening: all cavities, the runners and gates, the overflows and the biscuit (or the sprue on a hot-chamber machine). Multiply that total area by the intensified cavity metal pressure, add the opening-direction force from any wedge-locked slides, and multiply by a safety factor of at least 1.1. In inch units, psi times square inches gives pounds-force, and 2,000 lbf is one short ton. In metric units, MPa times square centimeters divided by 10 gives kilonewtons, and 9.807 kN is one tonne-force. Example: 60.27 square inches at 8,700 psi with a factor of 1.2 needs 629,204 lbf, which is 314.6 short tons.

What cavity pressure should I use for aluminum, zinc and magnesium die castings?

Use your caster's process sheet when you have one. As starting points, one die caster's published tonnage method uses about 30 MPa (4,350 psi) for zinc, 60 MPa (8,700 psi) for general aluminum castings and above 80 MPa (11,600 psi) where the aluminum part must be air-tight. A die casting technical director at Hill and Griffith gives typical minimum pressures of 3,000 psi static and 8,000 psi intensified for both aluminum and magnesium, 2,000 psi static for zinc, and notes some casters use 10,000 psi as a minimum intensification pressure for heavy sections.

Does the biscuit count toward the clamp force?

Yes. On a cold-chamber machine the biscuit, the slug of metal left in front of the plunger tip, lies in the parting plane at full metal pressure, so its area of pi times the tip diameter squared over 4 adds to the separating force like any cavity. A 3 inch tip adds 7.07 square inches. Its force works out to the shot cylinder's own force, so a smaller tip does not shrink the biscuit's contribution; it raises the pressure everywhere else in the die.

How do slides and side cores change the clamp force?

A slide face is perpendicular to the parting plane, so it adds nothing to the projected area, but the metal pushes it sideways and a sloped locking wedge turns part of that push into force along the opening direction. Ignoring friction, that extra force is the metal pressure times the slide face area times the tangent of the wedge angle. At 8,000 psi, a 6 square inch slide face behind a 20 degree wedge adds about 17,471 lbf, roughly 8.7 short tons before the safety factor.

How does the plunger tip diameter change the metal pressure?

The shot cylinder's force is the same at the piston and at the tip, so the metal pressure equals the hydraulic pressure times the bore diameter divided by the tip diameter, squared. A 2,000 psi hydraulic pressure on a 6 inch bore driving a 3 inch tip gives 2,000 times 4, which is 8,000 psi in the metal. Going to a smaller tip raises metal pressure by the square of the ratio, and with it the clamp force the die needs.

What happens if the die casting machine is too small?

If the separating force exceeds the clamp force, the die halves open slightly during the shot. Metal is forced into the parting line as flash, dimensions that cross the parting line grow, the die faces and vents wear faster, and molten metal can be sprayed from the parting line, which is a safety hazard. An undersized machine cannot be fixed by process tuning without lowering the pressure, which usually costs internal soundness.

Why can the same machine be listed with two different tonnages?

Die casting machine sizes are given in tons or metric tonnes, and the two differ by about 10 percent. A short ton of force is 2,000 lbf or 8.896 kN; a tonne-force is 9.807 kN. A machine plated 400 tonne-force delivers 3,923 kN, about 441 short tons, while a 400 short ton machine delivers 3,558 kN, about 363 tonne-force. Write the unit next to every rating before you compare a requirement with a machine list.

Ask JCH about die casting machine size

Not sure which pressure your casting needs, or whether a layout will fit the machine a caster proposed? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.

AI assistant. Answers can be wrong; nothing it says is a quote or a promise.

Want a second look at the die layout before you commit to a machine?

This calculator gives an engineering estimate. Our tooling team can go through your part's parting line, overflow plan and quality requirement with you and match the layout to suitable machines in our vetted manufacturing network.

Book a free 30-minute first consultation Send a drawing
JCH Design & Manufacturing — tooling, injection molding, PCBA, custom packaging, cut-and-sew & QC via vetted partner factories · Book a 30-minute call · jack@jchtrade.com · (321) 323-4474 · Canonical: https://jchtrade.com/tools/die-casting-tonnage-calculator