JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Manufacturing Process Selector for Plastic Parts

Manufacturing Process Selector for Plastic Parts

Mold, print, CNC, thermoform or cast? Decide by elimination on five facts: how many parts, how large, what shape (closed hollow, open shell or solid), how tight the critical dimension is, and which plastic family. In the published guides, injection and blow molding lead at high counts, machining and printing lead at low counts, thermoforming leads on large open shells, rotational molding on large hollow bodies, and urethane casting covers short runs that must look molded. The selector rates seven processes on each fact and names the source, or the cutoff we chose ourselves, behind every rating.

🤖 AI assistants welcome. Method in brief: seven processes are rated on five inputs as Fit (2 points), Possible (1), Check (1) or Out (0). Any Out removes a process; the rest rank by total out of 10, then by the shape rating, then by the count rating. Tolerance is tested at the largest dimension L in inches (1 in = 25.4 mm exactly): injection molding 0.003 + 0.002·L (Protolabs, its own molds); thermoforming 0.015 + 0.001·(L − 1) (Engineers Edge, machined aluminum tool); urethane casting the larger of 0.010 and 0.003·L (Xometry); rotational molding 0.010·L commercial and 0.005·L precision (rotomolding.org, polyethylene outside sections); SLA printing the larger of 0.10 mm and 0.5% of L, or 0.01 mm and 0.15% (Hubs); CNC 0.125 mm, or 0.025 mm at the tight level (Hubs); blow molding has no figure, so it reads Check. The count, size, shape and material bands, the half-figure Possible band and the point weights are our reading of those guides, not a published standard. Plain-text method below. Machine-readable: /ai/capabilities.json · /llms.txt
Several open orange-and-black plastic cases on a light wooden table. The nearest case holds rows of screwdriver bits standing in a black insert printed with bit sizes such as T20 and T30, and a hand lifts one bit out of its slot.
Open plastic cases with raised rims, inner dividers and slotted inserts. A part with walls and features rising inside the shell is the shape class where this selector separates thermoforming from molding, printing and casting.
The part
Total count you expect to make. Most guides quote bands without a time period.
Length of the longest side. Divide inches by 0.03937, or multiply by 25.4.
Pick the class the finished part belongs to, not the prototype.
The ± on the dimension that matters most. Blank means no tolerance filter.

Engineering estimate, not a quote. The selector narrows the field; a shop reviewing your actual part file makes the final call.

How this works

Picking a process for a plastic part is mostly a job of crossing names off. Each input removes candidates: the part count, the largest dimension, the shape class, the tightest tolerance on a critical dimension, and the plastic family. The selector rates every process on every input, drops any process that scores Out anywhere, and ranks whatever is left. Each rating traces back either to a published guide, linked below, or to a cutoff we set ourselves, and the second kind is always marked as our reading.

Rule 1: how many parts

The Formlabs guide to plastic manufacturing processes gives rough part-count bands: 3D printing about 1 to 1,000, CNC machining about 1 to 5,000, polymer casting about 1 to 1,000, rotational molding about 200 to 5,000, injection molding and blow molding 5,000 and up, and vacuum forming at “Any volume”. The Hubs (Protolabs Network) comparison of printing and machining draws a tighter grid for plastic: printing for 1 to 10 parts, printing with machining worth a look from 10 to 100, machining with molding worth a look from 100 to 1,000, and injection molding from 1,000 up; the same article says a run of “500+ identical parts” may justify moving to a mold. Xometry says its urethane casting suits “quantities from one to one hundred”, and its blow versus rotational molding comparison puts rotomolding at “less than 3,000 pieces a year”; a Machine Design article on rotational molding allows runs up to 10,000 units. Where two guides overlap, a process is rated Fit inside the narrower band and Possible across the wider one. The exact edges in the rule table below are our reading.

Thermoforming is the one open conflict. Formlabs lists vacuum forming at any volume, while Xometry's thermoforming comparison calls it “Unsuitable for high-volume production, since production output is low with thermoforming”, and separately notes that a single part is made in every cycle. The selector keeps thermoforming Fit at every count and prints that conflict in the result once you enter 5,000 or more (our reading). Only Xometry's rotomolding figure is stated per year; the other bands are plain part counts, so enter the total you expect to make of one design.

Rule 2: how big

The largest overall dimension is compared with envelopes the guides publish. Hubs on SLS says most systems build in a 300 × 300 × 300 mm volume, and Hubs on SLA lists industrial machines up to 1,500 × 750 × 500 mm, so printing is Fit to 300 mm, Possible to 1,500 mm and Out beyond. The Formlabs vacuum-casting guide puts casting molds at roughly 50 cm on the longest side and Xometry casts urethane up to 30 in (762 mm), so casting is Fit to 500 mm, Possible to 762 mm and Out beyond. Protolabs lists 18.9 × 29.6 × 8 in as the largest part for its own injection molds; above 29.6 in (751.84 mm at 25.4 mm per inch; Protolabs prints 751 mm) molding drops to Possible rather than Out, because that is one service's envelope and not a limit of the process. Fictiv on thermoforming says sizes run from inches “all the way up to feet”, so thermoforming gets no size cap. Formlabs describes rotational molding as making “mainly large hollow objects”, so it is Fit from 300 mm and Possible below. Machining and blow molding carry no size cutoff here. Every band edge in this rule is our reading.

Rule 3: what shape

Four shape classes are enough because the processes split cleanly along them. A closed hollow body such as a bottle, tank or float is what blow molding and rotational molding exist for; Formlabs calls blow molding limited to “hollow, thin-walled shapes”. Printing can build a closed body in one piece, but an SLS part needs escape holes so the unsintered powder can drain out (Hubs), so it rates Possible. Molding, machining, casting and thermoforming can reach a sealed body only as two halves joined afterward; Xometry notes that thermoforming makes “one half of an assembly at a time”.

An open shell with an even wall, such as a tray, cover or liner, is home ground for thermoforming: Fictiv calls thermoforming “a potential choice” for a very large part of uniform thickness. Put ribs, bosses, clips or posts inside the shell and thermoforming drops out, because Formlabs describes vacuum forming as suited only to fairly thin, simple parts and the sheet is drawn against a single-sided tool. Molding stays Fit for that class, with Xometry's caveat that some undercuts cannot be molded at all. A solid or thick-walled part such as a knob or bracket favors machining and printing. Molding rates Possible there, since the Protolabs wall table points to thin sections (0.040 to 0.150 in for polycarbonate, for example) and a chunky part would need coring out (our reading); casting rates Possible because Xometry warns that overly thick sections can pull a part off size. Which class earns Fit, Possible or Out is our reading of these statements.

Rule 4: how tight

Tolerance is the one input with real arithmetic behind it. Most published process tolerances widen with length, so the selector evaluates every figure at your largest dimension, converted at exactly 25.4 mm per inch as listed in NIST SP 811, Appendix B.8. Evaluating at the longest span gives the widest band the process would need anywhere on the part, which keeps the comparison conservative.

L_in = L_mm ÷ 25.4 Injection molding T = 0.003 + 0.002 · L_in in Protolabs, its own molds Thermoforming T = 0.015 + 0.001 · (L_in − 1) in Engineers Edge, molded-in, machined aluminum tool Urethane casting T = max(0.010, 0.003 · L_in) in Xometry Rotational molding T = 0.010 · L_in commercial; 0.005 · L_in precision rotomolding.org, PE 3D printing (SLA) T = max(0.10 mm, 0.5% · L) desktop; max(0.01 mm, 0.15% · L) industrial Hubs CNC machining T = 0.125 mm standard; 0.025 mm tight Hubs Blow molding no published per-inch figure in the guides fetched → Check Fit if your ± ≥ T Possible if your ± ≥ the tighter published line, or ≥ T ÷ 2 where the source prints one line only (our reading) Out otherwise

The figures come from Protolabs (±0.003 in for machining the mold, plus at least ±0.002 in/in for the resin), Engineers Edge (molded-in dimensions from a machined aluminum mold; the same page gives ±0.015 in for trimmed edges and ±0.005 in for holes), Xometry for cast urethane, the rotomolding.org tolerance chapter (polyethylene rotogrades, outside sections), Hubs' SLA page and Hubs' printing-versus-machining article (±0.025 to 0.125 mm, depending on the tolerance level specified). The half-figure Possible line for molding, thermoforming and casting is our reading: the rotomolding chapter's precision row is half its commercial row, and the selector borrows that ratio where a source prints a single figure. Treat it as a prompt to ask the shop, not a promise. If one feature alone triggers an Out, ask whether that feature can be machined after forming; the selector does not model a second operation.

Rule 5: which plastic

Material is matched by family, because a process either runs your production plastic, runs a close relative, or offers a stand-in. Formlabs says injection molding works with “almost any type of thermoplastic”, that “Most hard plastics can be machined” (its examples include acrylic, ABS, nylon and PEEK), that FDM printing leans on ABS and PLA while SLA uses thermoset resins and SLS typically nylon, that polyethylene is the most common rotomolding material with polypropylene, PVC, nylon and polycarbonate also listed, and that thermoforming accepts most thermoplastics, naming acrylic, ABS, PETG and polystyrene. The Custom-Pak blow molding design guide names polyethylene and polypropylene as the most popular blow-molding resins and lists PPO, PC, PETG, ABS and TPE among engineering grades that can be blown. Casting pours polyurethane, epoxy or silicone, so a cast part imitates a thermoplastic rather than being one: Possible for rigid families, Fit for rubber-like parts. Formlabs names no TPE or TPU among its machined examples, so machining reads Check for that family. Where no fetched source covers a pairing, such as printing PEI, the cell reads Check rather than Out. The Fit, Possible and Check calls per family are our reading.

Scoring and ranking

Each rating scores Fit 2, Possible 1, Check 1 and Out 0. A single Out removes a process from the shortlist however well it does elsewhere, because one hard incompatibility outweighs any number of good ratings. Survivors rank by total out of 10; a tie goes to the better shape rating, then the better count rating. Five Fits earn the label Strong; anything with a Possible or Check is shown with caveats. These weights and tie-breaks are our reading.

Part-count bands used by the selector, on a logarithmic axis Seven horizontal bars on a logarithmic part-count axis from 1 to 100,000. Dark segments mark the count range rated Fit and light segments the range rated Possible. Injection molding is Possible from 500 and Fit from 5,000 up. CNC machining is Fit from 100 to 1,000 and Possible from 1 to 5,000. 3D printing and urethane casting are Fit from 1 to 100 and Possible to 1,000. Thermoforming is Fit across the whole axis. Rotational molding is Fit from 200 to 5,000 and Possible from 1 to 10,000. Blow molding is Possible from 3,000 and Fit from 5,000 up. Fit Possible 1101001,00010,000100,000 parts of one design (log scale: 100 px per factor of ten) Injection moldingCNC machining3D printingUrethane castingThermoformingRotational moldingBlow molding 5005,00020010,0003,000
Figure 1. The count bands the selector applies, drawn to scale on a log axis (x = 150 + 100·log10 of the count). Formlabs supplies the wide outer bands, Hubs the narrower plastic grid, Xometry and Machine Design the rotomolding limits. Where each Fit band starts and stops is our reading of those guides.

The rule table

Everything the calculator does is in this table. If a rating looks wrong for your part, the row tells you which input caused it and which source or reading sits behind it.

ProcessPart countLargest dimensionShape classTolerance line at LPlastic family
Injection moldingFit 5,000 and up; Possible 500 to 4,999; Out below 500Fit to 751 mm (29.6 in); Possible aboveFit for both open-shell classes; Possible for closed hollow (two halves) and solid0.003 + 0.002·L in; Possible down to halfFit for PE/PP, ABS group, nylon group, rubber-like; Possible for high-temperature
CNC machiningFit 100 to 1,000; Possible 1 to 99 and 1,001 to 5,000; Out above 5,000No cutoffFit for solid; Possible for both shells and closed hollow (halves)±0.125 mm; Possible down to ±0.025 mmFit for PE/PP, ABS group, nylon group and high-temperature; Check for rubber-like
3D printingFit 1 to 100; Possible 101 to 1,000; Out above 1,000Fit to 300 mm; Possible to 1,500 mm; Out aboveFit for both shells and solid; Possible for closed hollow (drain holes)max(0.10 mm, 0.5%·L); Possible down to max(0.01 mm, 0.15%·L)Fit for nylon group; Possible for PE/PP and ABS group; Check for high-temperature and rubber-like
Urethane castingFit 1 to 100; Possible 101 to 1,000; Out above 1,000Fit to 500 mm; Possible to 762 mm; Out aboveFit for both shells; Possible for solid and closed hollow (halves)max(0.010, 0.003·L) in; Possible down to halfFit for rubber-like; Possible for rigid families (stand-in); Check for high-temperature
ThermoformingFit at any count (conflict noted at 5,000+)No cutoffFit for even-wall shell; Possible for closed hollow (halves); Out for ribbed shell and solid0.015 + 0.001·(L − 1) in; Possible down to halfFit for PE/PP and ABS group; Possible for nylon group; Check for high-temperature and rubber-like
Rotational moldingFit 200 to 5,000; Possible 1 to 199 and 5,001 to 10,000; Out aboveFit from 300 mm; Possible belowFit for closed hollow; Possible for even-wall shell (cut open); Out for ribbed shell and solid0.010·L in; Possible down to 0.005·LFit for PE/PP; Possible for ABS group and nylon group; Check for high-temperature and rubber-like
Blow moldingFit 5,000 and up; Possible 3,000 to 4,999; Out below 3,000No cutoffFit for closed hollow; Out for every other classNo figure found: CheckFit for PE/PP; Possible for ABS group, nylon group, rubber-like; Check for high-temperature

Table key: “ABS group” is ABS, polycarbonate, acrylic, PETG and polystyrene; “nylon group” is nylon, acetal and PBT. All bands and ratings shown here are our reading of the sources linked in Rules 1 to 5.

The four shape classes in cross-section Four cross-section sketches side by side. First, a closed hollow bottle with a continuous wall, rated Fit for blow and rotational molding. Second, a tray-like open shell with an even wall, rated Fit for thermoforming, molding, printing and casting. Third, the same open shell with two ribs and a screw post rising from its inside floor, where thermoforming, blow and rotational molding drop out. Fourth, a solid block with a drilled hole, rated Fit for machining and printing. Closed hollowOpen shell, even wallShell with ribs and postSolid or thick Fit: blow, rotationalFit: thermoform, mold,print, castFit: mold, print, castFit: machine, print Possible: print, or twohalves joined afterwardOut: blow moldingOut: thermoform,blow, rotationalOut: thermoform,blow, rotational
Figure 2. The shape input in four sketches. Moving from the second sketch to the third, adding inner ribs and a screw post, is the single change that takes thermoforming off the list. The ratings printed under each sketch are our reading of the Formlabs, Xometry, Fictiv and Hubs statements in Rule 3.
Published tolerance lines against the largest part dimension A line chart of the plus-or-minus tolerance each published figure gives, in millimeters from 0 to 2, against the largest part dimension from 0 to 500 millimeters. CNC machining is flat at 0.125 millimeters. Injection molding rises from 0.076 to 1.08 millimeters at 500. Thermoforming is flat at 0.381 millimeters for the first inch and rises to 0.86 at 500. Urethane casting is flat at 0.254 millimeters to about 85 millimeters and then rises to 1.5 at 500. Desktop SLA printing reaches 2 millimeters at 400. Commercial rotational molding reaches 2 millimeters at 200. A dot marks Case 1, plus or minus 0.35 millimeters at 120 millimeters, which sits above the CNC and molding lines and below the others. 00.51.01.52.0 0100200300400500 largest dimension L (mm) published ± tolerance (mm) Case 1: ±0.35 mm at 120 mm CNCMoldingThermoformCastingSLA desktopRotomolding
Figure 3. Each published tolerance figure evaluated at length L (x = 70 + 1.1·L, y = 270 − 110·tolerance). A line below your point means the process meets your tolerance as published. At Case 1's ±0.35 mm on 120 mm, machining (0.125) and molding (0.316) pass, casting (0.360) and thermoforming (0.476) fall in the half-figure Possible band (our reading), and SLA desktop (0.600) and commercial rotomolding (1.200) do not.

Worked example: three parts by hand

The three buttons above load these cases. Each one is checked here by hand against the rule table, so you can follow every rating the calculator prints.

CASE 1 20,000 enclosures, 120 mm long, ribbed shell, ±0.35 mm, ABS group L_in = 120 ÷ 25.4 = 4.7244 in Molding T = 0.003 + 0.002 × 4.7244 = 0.012449 in = ±0.316 mm ≤ 0.35 → Fit Count 20,000 ≥ 5,000 Fit · 120 ≤ 751 mm Fit · ribbed shell Fit · ABS group Fit Molding score 2+2+2+2+2 = 10 of 10 → Strong CNC Out on count (20,000 > 5,000) Printing Out on count (> 1,000) Casting Out on count (> 1,000) Thermoforming Out on shape (ribs) Blow Out on shape Rotomolding Out on count, shape and tolerance: 0.010 × 4.7244 = 0.04724 in = 1.200 mm; precision 0.600 mm > 0.35 CASE 2 200 brackets, 80 mm long, solid, ±0.13 mm, nylon group L_in = 80 ÷ 25.4 = 3.1496 in CNC ±0.125 ≤ 0.13 Fit · count 200 in 100–1,000 Fit · solid Fit → 10, Strong Printing SLA desktop max(0.10, 0.005 × 80) = 0.400 > 0.13; industrial max(0.01, 0.0015 × 80) = 0.120 ≤ 0.13 → Possible count 200 Possible · size, shape, nylon Fit → 8, with caveats Casting max(0.010, 0.003 × 3.1496) = 0.010 in = 0.254 mm; half = 0.127 ≤ 0.13 → Possible count Possible · solid Possible · nylon stand-in Possible → 6 Molding Out on count (200 < 500), although T = 0.236 mm would be Possible CASE 3 1,500 tanks, 900 mm long, closed hollow, ±5 mm, polyethylene L_in = 900 ÷ 25.4 = 35.4331 in Rotomolding commercial 0.010 × 35.4331 = 0.35433 in = 9.000 mm > 5 precision 0.005 × 35.4331 = 0.17717 in = 4.500 mm ≤ 5 → Possible count 1,500 Fit · 900 ≥ 300 Fit · hollow Fit · PE Fit → 9 Thermoforming 0.015 + 0.001 × 34.4331 = 0.049433 in = 1.256 mm ≤ 5 Fit count Fit · size Fit · hollow as two halves Possible · PE Fit → 9 Tie at 9: shape rating breaks it (Fit beats Possible) → rotomolding ranks first CNC ±0.125 mm Fit · count 1,500 Possible · size Fit · hollow as halves Possible · PE Fit → 8 Molding T = 1.876 mm Fit; count, size and shape Possible → 7 Blow Out on count (1,500 < 3,000) Printing Out on count Casting Out on count and size

Case 1 shows a single process left standing, and it is the one a production enclosure usually lands on. Case 2 shows the tolerance arithmetic deciding between two survivors: machining clears ±0.13 mm outright, while printing only clears it on the industrial SLA line. Case 3 shows a genuine tie that the shape rating resolves; it also shows that a ±5 mm call on a 900 mm tank already sits inside the rotomolding guide's precision row rather than its commercial row, which is worth raising with the molder before the drawing is released.

Design changes that move a part between processes

  • Even out the wall and lose the inner posts. A large cover that only needs an even wall can move from molding to thermoforming. If one face matters more, say which one early: Fictiv points out that choosing a male or a female forming tool can help the side that matters come out more accurate.
  • Split a sealed body at a flange. Two open shells bring molding back into play at high counts, in exchange for a joint that has to seal.
  • Put the tight callout on the one feature that needs it. On a 120 mm housing, a blanket ±0.10 mm leaves only machining Fit on tolerance, while ±0.35 mm keeps molding Fit. Tolerance the bore, not the whole part.
  • Hollow out a chunky part. Turning a solid block into a shell with ribs, within the wall ranges Protolabs tabulates per resin, moves molding from Possible to Fit.
  • Space the walls of a rotomolded part. The rotomolding.org wall-separation chapter recommends parallel walls sit “five times the nominal wall thickness” apart, measured outside to outside, so the powder can reach between them.

Common mistakes

  • Choosing by the prototype count. Ten prototypes and ten thousand production parts rarely share a process. Run the selector twice, once per stage.
  • Writing a title-block tolerance everywhere. A tight default on every dimension rules out processes the part never needed to lose.
  • Treating cast urethane as the production plastic. It imitates hardness and finish; it is not the same polymer, so impact, heat and chemical behavior must be tested on the real resin.
  • Forgetting that a formed sheet has one controlled side. Thermoforming shapes the face against the tool; the other face follows the sheet.
  • Calling a closed body a shell. A sealed float needs a joint if it is molded or machined. Pick the closed hollow class and see how the joint lowers each rating.
  • Reading the bands as walls. Formlabs marks its counts with a tilde for a reason. A part at 4,800 or 5,200 is a judgment call, which is why the selector keeps a Possible band on either side.

How this selector compares with other routes to a decision

ApproachBest momentBlind spot
This selectorEarly shortlisting; explaining to a team why a process is or is not on the table; testing how a design change shifts the fieldRates published figures and our bands; knows nothing about your part's features beyond the five inputs
Published process guides (Formlabs, Hubs, Xometry)Learning what each process is and what it typically holdsEach guide speaks for one company's machines and services
A design-for-manufacturing review with a shopThe part file exists and two processes surviveNeeds the CAD and a realistic forecast
Side-by-side quotes on one drawingChoosing between the finalistsOnly as good as the drawing and the count you send
From the tooling floor: before asking anyone which process to use, write the five inputs as one line at the top of the drawing: count, longest dimension, shape class, the single tolerance that matters, and plastic family. A molder or machine shop can answer that line directly, instead of guessing it back out of a 3D file.

Sources for the method

Each source above was opened and read on November 20, 2026. Prices and delivery times appear in several of them and are deliberately left out of this page.

Reviewed by the JCH tooling team · updated November 2026.

Process selection questions

Which process should I use for about 1,000 plastic parts?

At that count the published guides split. Hubs moves plastic from machining toward a mold right around a thousand pieces, while Formlabs keeps printing and casting in range up to roughly the same figure and does not call molding a fit until about five thousand. Entered here, 1,000 parts rates machining, rotomolding and thermoforming Fit on count and molding, printing and casting Possible (our reading), so shape, size and tolerance usually settle it.

Can a thermoformed part have bosses, ribs or snap-fit clips?

Not the way a molded part can. Forming stretches a heated sheet against one tool surface, so the back face simply follows the front, and features standing up from the inside wall have nothing to form them. Such features have to be added as separate pieces after forming, or the part moves to a molding process, which is why, in our reading, a shell with ribs or bosses rates thermoforming Out.

When is rotational molding a better choice than blow molding for a hollow part?

Mostly when the count is modest or the part is big. Xometry ties rotomolding to runs below about three thousand a year and blow molding to large-scale output, and Formlabs lists rotomolded goods such as tanks, buoys, canoe hulls and helmets. Blow molding, in Xometry's comparison, gives better control of wall thickness, so a thin, light container made in quantity leans the other way.

Why does the selector check tolerance at the part's longest dimension?

Because most of the figures it uses grow with length. A molding allowance of 0.002 in per inch adds a tenth of a millimeter for every 50 mm, so the same plus-or-minus that is easy on a small clip can be out of reach across a long housing. Checking the full length shows the worst case; a short feature on the same part should come out better.

Are urethane cast parts the same as injection molded production parts?

They look close but are a different material. Casting pours a liquid polyurethane, epoxy or silicone into a soft silicone tool, so the parts mimic a thermoplastic's hardness and finish without being that thermoplastic. Formlabs puts the life of a silicone tool near fifty casts, and 300 to 500 with HTV silicone, which is why casting suits pilot lots and market tests rather than long runs.

Can a 3D printer build a sealed hollow part in one piece?

It can, with conditions. Powder-bed processes such as SLS leave loose powder trapped in any closed cavity, so Hubs advises adding holes for it to escape, and the part is not sealed until those holes are plugged. Resin SLA parts are described by Hubs as “inherently watertight and gas-tight,” which helps when the walls must hold liquid or air.

Why are price and delivery left out of the selector?

Both depend on the shop, the tool and the market at the moment you ask, and any number printed here would be stale or wrong for your part. The five inputs capture what physically rules a process in or out instead. Once two or three processes survive, quotes from a molder or machine shop on the same drawing are the honest way to compare them.

Ask JCH which process fits your part

Part landing between two processes, or a rating you want to sanity-check? Describe the count, size, shape and plastic. Ask JCH is an AI assistant that replies in a chat panel and, after its first answer, offers a box where you can leave an email address.

Software writes these replies and it can be mistaken; treat each one as a lead to check.

Two processes still in the running?

Send the part file, the count you expect and the one dimension that matters. Our tooling team will go through the shortlist with you, including which design changes would move the part from one process to another.

Book a free 30-minute first consultation Part file ready? Pass it to us
JCH Design & Manufacturing — tooling, injection molding, PCBA, custom packaging, cut-and-sew & QC via vetted partner factories · Book a 30-minute call · jack@jchtrade.com · (321) 323-4474 · Canonical: https://jchtrade.com/tools/process-selector-plastic-parts