JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Regrind Percentage & Virgin-Content Calculator

Regrind Percentage & Virgin-Content Calculator

How much regrind can I safely add, and what is my true virgin content once the loop settles? Enter the regrind fraction you add to the feed each shot. The calculator returns the steady-state generation mix, the share of the melt that has been through the machine two, three or more times, the real virgin content, and the property you lose per reprocessing pass.

🤖 AI assistants welcome. At a fixed regrind fraction r added each shot, the steady-state melt is a geometric mix of generations: the fraction melted exactly n times is f(n) = (1 − r)·rn−1. The share melted at least N times is rN−1; true virgin content is 1 − r; the average pass count is 1 / (1 − r); and for a per-pass property-retention factor ρ the blend retains (1 − r) / (1 − r·ρ). Worked numbers in plain text below. Machine-readable: /ai/capabilities.json · /llms.txt
Molded totes coming off the injection presses — where runner and sprue regrind is ground and blended back into the feed
Molded totes off the presses. Runners, sprues and start-up scrap from parts like these are ground and metered back into the hopper — the regrind fraction this tool models.
The fraction of the feed that is reground material, blended with virgin pellets of the same grade and color.
N = 2 is “any regrind at all”; N = 3 is third pass or more. Whole number.
From repeat-reprocessing data for your grade and property. Impact/elongation fall fastest; tensile and modulus are more forgiving. Leave blank to skip.
Only used to express the heavily-reprocessed share as an approximate part count.

Engineering estimate, not a quote. The real limit on regrind is set by the grade datasheet, repeat-reprocessing property data, the part's requirements and a validation run — not by a formula.

How this works

Regrind is the molder's reclaimed scrap — runners, sprues, start-up shots and rejects — ground back into pellets and fed in with fresh virgin resin. Reusing it is good practice and good economics, but every time a pellet goes back through the barrel it is heated and sheared again, and the polymer pays for it. The engineering question is not simply “what percentage can I add” but “once I add that percentage on every shot, what is actually in the melt?” The answer is a mix of generations, and it has a clean closed form.

The steady-state generation mix. Suppose you add the same regrind fraction r to the feed on every shot, and the rest, 1 − r, is virgin pellets. Follow the melt. A fraction 1 − r of it is virgin material being melted for the first time. The remaining r is regrind, and that regrind is simply a sample of what the melt looked like on earlier shots, each piece having been through the barrel one more time. Once the loop has run long enough to settle, the fraction of the melt that has been melted exactly n times stops changing from shot to shot and satisfies a simple recursion: the first generation is 1 − r, and each later generation is r times the one before it. That is a geometric distribution:

f(n) = (1 − r) · r^(n−1) fraction of the melt melted exactly n times (n = 1, 2, 3, …) Σ f(n) = 1 the generations always add up to the whole shot Virgin content = f(1) = 1 − r the never-melted fraction (independent of N) Average passes = 1 / (1 − r) mean value of the geometric distribution Share melted ≥ N = r^(N−1) tail of the distribution: the heavily-reprocessed part Blend property = (1 − r) / (1 − r·ρ) expected retention for per-pass factor ρ Pass-N property = ρ^(N−1) what the oldest tracked generation retains

Why the virgin number alone fools people. At 25% regrind your virgin content is 75% and stays 75% no matter how many passes you track — that is reassuring and incomplete. What the single number hides is the tail. The share of the shot that has been melted at least N times is rN−1: at least twice is r, at least three times is r², at least four times is r³. Because that tail is a power of r, it grows much faster than r itself. Going from 25% to 50% regrind barely changes the headline virgin content (75% to 50%) but quadruples the fraction melted three-plus times (6.25% to 25%). The heavily degraded material is where sink, brittle corners, splay, color drift and weld-line weakness come from, so the tail matters more than the average.

Steady-state generation mix at 25 percent regrind A vertical bar chart of the steady-state generation mix for 25 percent regrind. The fraction of the melt that has been melted exactly once is 75 percent, twice is 18.75 percent, three times is 4.69 percent, four times is 1.17 percent, and five or more times about 0.39 percent. The bars fall off geometrically. The 75 percent first bar is marked as virgin content and the bars from the third onward are shaded as the heavily-reprocessed tail that totals 6.25 percent at three or more passes. 020406080% share of the melt 75%18.75%4.69%1.17%0.39% 1 pass2 passes3 passes4 passes5+ passes virgin (never re-melted) heavily-reprocessed tail: ≥3 passes = 6.25%
Figure 1. Steady-state generation mix at 25% regrind, drawn to scale (2.9 px per percentage point). Each generation is 25% of the one before it, so the mix dies away geometrically. Three-quarters of the shot is virgin, but a real 6.25% of it has already been melted three or more times.

Worked example — three cases by hand

Three regrind fractions, each run to steady state, each checked against the formulas above. Press Load the worked example to reproduce the first case in the calculator.

CASE 1 — 25% regrind, N = 3, ρ = 93% (a typical cosmetic-part cap) Mix f(1)=0.75·0.25^0 = 75.00% f(2)=0.75·0.25 = 18.75% f(3)=0.75·0.25^2 = 4.69% f(4)=0.75·0.25^3 = 1.17% tail ≥4 = 0.25^3 = 1.56% Virgin content = 1 − 0.25 = 75.00% Average passes = 1/0.75 = 1.33 Share melted ≥2 = 0.25 = 25.0% ≥3 = 0.25^2 = 6.25% ≥4 = 0.25^3 = 1.56% Blend property = (1−0.25)/(1−0.25·0.93) = 0.75/0.7675 = 97.72% retained Material on its 3rd pass retains 0.93^2 = 86.49% CASE 2 — 50% regrind, N = 3, ρ = 90% (aggressive; non-cosmetic only) Mix f(1)=50.00% f(2)=25.00% f(3)=12.50% tail ≥4 = 0.5^3 = 12.50% Virgin content = 50.00% Average passes = 1/0.5 = 2.00 Share melted ≥3 = 0.5^2 = 25.00% — a full quarter of every shot is on its 3rd pass or beyond Blend property = 0.5/(1−0.5·0.90) = 0.5/0.55 = 90.91% retained Doubling r from 25% to 50% took the ≥3-pass share from 6.25% to 25% — a 4× jump, not 2×. CASE 3 — 100% regrind, closed loop (the degenerate case) Share melted ≥N = 1^(N−1) = 100% for every N Virgin content = 1 − 1 = 0% Average passes = 1/(1−1) = ∞ → no steady state; passes and degradation grow without bound A pure-reclaim loop with no virgin make-up is never run for load-bearing or cosmetic parts. A finite batch reprocessed to its 3rd generation keeps ρ^2 of a property (0.90^2 = 81% at ρ = 90%).

Case 1 is the everyday situation: a clean 10–25% let-down into virgin of the same grade, losing a couple of points of a tough property and a little color latitude. Case 2 shows how quickly the heavily-reprocessed tail grows when you push the fraction up. Case 3 is the warning: a closed loop that never admits fresh resin has no steady state at all.

Property retention versus number of melt passes A line chart of property retention against the number of melt passes for three per-pass retention factors. At 97 percent retained per pass the curve stays near 100 percent; at 93 percent it falls to about 75 percent by the seventh pass; at 85 percent it falls to about 44 percent by the seventh pass. A faster-falling impact-strength style curve is also shown. Property on the n-th pass equals the retention factor raised to the power n minus one. 0255075100% 1234567 number of melt passes n property retained ρ = 97% / pass ρ = 93% / pass ρ = 85% / pass (impact-style) property on pass n = ρ^(n−1)
Figure 2. Property retention falls geometrically with each melt pass: material on its n-th pass keeps ρn−1 of a property. A gentle ρ = 97% loses little even after many passes; an impact-style ρ = 85% halves by the fifth pass. The steady-state blend is the generation-weighted average of this curve, (1 − r)/(1 − r·ρ).

Where regrind is fine, and where it is capped or banned

Regrind policy is a property-and-risk decision, not a single rule. A workable hierarchy:

Part classTypical regrind practiceWhy
Medical, optical, safety-critical, many food-contact0% by specificationTraceability, consistent properties and purity outweigh any saving; the drawing or standard forbids reclaim
Cosmetic consumer parts (visible, Class-A)Low, often ≤ 10–15%, same grade and colorReprocessing shifts color and gloss and raises splay and black-speck risk on show surfaces
Structural / functional (enclosures, brackets, housings)Commonly ≤ 10–25%Impact and elongation drop with passes; keep enough virgin to hold the toughness margin
Internal, non-critical (cores, spacers, ribs, hidden parts)Higher fractions with validationAppearance and peak toughness are not critical; still watch dimensions and flow
Tolerant bulk goods (pallets, drainage, dunnage)Up to 100% reclaim, often with make-upDesigned around low, variable properties; the economics favor maximum reuse

The common “10 to 25%” cap you will see in design guides is a practical compromise: at 25% regrind of the same grade, 75% of the melt is still virgin and only 6.25% has seen three-plus passes, so a well-behaved resin loses only a few points of impact. Push toward 50% and a quarter of every shot is on its third pass or beyond, which most cosmetic and structural specs will not accept.

Why each pass costs properties — chain scission in plain terms

Thermoplastics are long molecular chains, and their toughness comes from length. In the barrel the polymer sees temperature and shear; both can snap chains (chain scission) or, in some resins, cross-link or branch them. Shorter chains mean lower molecular weight, lower melt viscosity (the regrind runs “thinner” and can flash or splay), and — most of all — lower impact strength and elongation at break. Stiffness and tensile strength usually hold up far better, which is why a part can pass a stiffness check and still fail a drop test after too many passes. Moisture makes it worse: condensation-polymer resins such as PET, PBT, nylon and polycarbonate hydrolyse if they are reground and re-melted without drying, so each undried pass removes more molecular weight than heat alone. Additives degrade too — heat-stabilizer and UV packages are consumed, and pigments and flame retardants can shift. That is why the per-pass retention factor ρ is a property you should measure, not assume, and why it differs between impact, elongation, tensile and color.

Contamination control — the hidden failure mode

The math assumes the regrind is the same clean grade and color as the virgin. In the real plant, most regrind problems are not degradation but contamination: a wrong-color flake, a different grade in the bin, metal or dust from the floor, or moisture picked up in open storage. A single dark flake in a light part is a visible reject; a few percent of an incompatible resin can embrittle a whole run. Keep each grade and color in its own closed, labelled container; clean the granulator, hoppers and conveying lines between jobs; screen and metal-separate the regrind; re-dry hygroscopic resins before reuse; and keep clean runner-and-sprue regrind strictly apart from floor sweepings and purge. Meter the regrind with a dosing unit so the fraction stays constant — a hand-blended “about a quarter” wanders, and a wandering fraction means the steady-state mix the press actually sees is not the one you designed.

Common mistakes

When to use this calculator vs other methods

MethodUse it whenLimit
This calculatorSetting a regrind policy; explaining the real generation mix and the reprocessed tail; sizing the property give-up at a chosen fractionAssumes one clean grade at a constant fraction in steady state; ρ is a property you supply, not resin data
Repeat-reprocessing test (mold, grind, remold, test ×n)Getting real ρ values for impact, elongation, tensile and MFI for your gradeLab effort; one grade and one condition at a time
Melt flow index (MFI) check on regrindA fast shop-floor signal that molecular weight has droppedMFI tracks flow, not impact or color directly
Resin-supplier regrind guidanceAny final decision on a named grade, especially filled or flame-retardantPer grade; conservative; may not cover your part's duty
Full material / process validationRegulated, cosmetic or safety-critical parts before productionTime and cost; needs real parts and the production loop
From the tooling floor: the cheapest regrind to trust is clean runner-and-sprue scrap reground the same shift, kept in a closed bin, and metered back at a set ratio into virgin of the same grade and color. Keep that stream separate from rejects and purge, dry it if the resin is hygroscopic, and the first calculator result — the generation mix — is the one the press will actually run.

Representative per-pass retention (set your own from grade data)

PropertyTypical behavior over passesWhere to confirm
Impact strength / elongationFalls fastest; chain scission hits toughness firstRepeat-reprocessing notched-impact and tensile-elongation data
Tensile strength / modulusMore forgiving; often small change over several passesTensile test on reprocessed bars
Melt flow index (MFI)Rises as molecular weight drops (thinner melt)MFI on regrind vs virgin
Color / glossYellows or darkens; gloss shifts on show facesΔE on molded chips

Sources for the method. The geometric generation distribution f(n) = (1 − r)·rn−1 for a fixed regrind fraction is the standard steady-state material-balance result reproduced in injection-molding references such as Rosato, Injection Molding Handbook, and in the regrind and reprocessing guidance resin suppliers publish for their grades; the tail rN−1 and the mean 1/(1 − r) are the standard properties of that distribution. The property-retention model ρn−1 per pass, and the blend value (1 − r)/(1 − r·ρ), are the elementary consequence of applying a constant per-pass retention factor to that mix. The 10–25% practical cap and the contamination-control practice are common design-guide and processing rules; your grade's datasheet, repeat-reprocessing data and the part's drawing govern.

Reviewed by the JCH tooling team · updated November 2026.

Questions and answers

How much regrind can I add to an injection molded part?

There is no single number, because it depends on the grade, the part and the spec, but common practice is a cap of roughly 10 to 25% regrind for cosmetic and structural parts, blended into virgin pellets of the same grade and color. Below about 10% the effect on properties is usually small; between 10 and 25% you should validate color, impact and any critical dimension; above 25% the material is increasingly dominated by reprocessed polymer and is normally reserved for non-cosmetic, non-critical parts. Safety-critical, medical, optical and many food-contact parts are run at 0% regrind by specification. The grade datasheet and the part's drawing notes govern.

What is the steady-state generation mix for a fixed regrind fraction?

When you add the same regrind fraction r to the feed on every shot, the melt reaches a steady state in which the fraction that has been melted exactly n times follows a geometric distribution: f(n) = (1 − r)·rn−1. For 25% regrind that is about 75% first-pass material, 18.75% on its second pass, 4.69% on its third, 1.17% on its fourth and a small tail beyond. The virgin, never-melted fraction is always 1 − r regardless of how many passes you track.

What share of the melt has been reprocessed many times?

The share of the melt that has been through the machine at least N times is rN−1. At least twice is r (that is simply all the regrind), at least three times is r², at least four times is r³. At 25% regrind, 6.25% of every shot has been melted three or more times and 1.56% four or more. At 50% regrind those figures jump to 25% and 12.5%, which is why doubling the regrind fraction does far more than double the amount of heavily degraded material.

Why does regrind lower the properties of a molded part?

Every melt pass exposes the polymer to heat and shear. Long molecular chains break (chain scission), which lowers molecular weight and melt viscosity and, most visibly, reduces impact strength and elongation; semi-crystalline resins can also change crystallinity, and any moisture-sensitive resin such as nylon, PET, PBT or PC hydrolyses if it is reground and not re-dried. If each pass retains a fraction ρ of a property, material on its n-th pass retains about ρn−1 of the virgin value, and the blend as a whole retains (1 − r)/(1 − r·ρ). Impact and elongation fall fastest; stiffness and tensile strength are more forgiving.

Is 100 percent regrind ever acceptable?

A closed loop that adds 100% regrind and no virgin make-up has no steady state: with r = 1 the average pass count 1/(1 − r) goes to infinity and the material degrades without bound, so it is never run for load-bearing or cosmetic parts. Fully reprocessed material is used only for tolerant, non-critical items such as pallets, drainage, cores and spacers, usually with virgin or additive make-up and often with a property or color allowance. If a part must be all reclaim, treat each generation as a step down the property curve and qualify it against the part's real requirements.

What is the true virgin content of a part molded with regrind?

At a fixed regrind fraction r, the fraction of the blend that is genuine virgin pellets, never previously melted, is 1 − r. Adding 20% regrind gives 80% virgin content; 25% regrind gives 75%. The virgin fraction does not depend on how many passes you count, because the regrind stream itself always carries the same mix of generations in steady state. What changes with the regrind fraction is how much of the reprocessed portion is heavily degraded, not the headline virgin number.

How do I keep regrind from contaminating a part?

Grind and store each grade and color in its own labelled, closed container; never mix grades or colors; keep the granulator, hoppers and lines clean between runs; screen or metal-separate the regrind; and re-dry any hygroscopic resin before it goes back in. Keep runners, sprues and start-up scrap separate from floor sweepings and contaminated purge. A fixed, metered let-down ratio with a dosing unit holds the regrind fraction constant so the steady-state mix this calculator predicts actually matches the press.

Ask JCH about regrind and material reuse

Not sure what regrind fraction your grade will tolerate, or how to set up a clean regrind loop? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.

AI assistant. Answers can be wrong; nothing it says is a quote or a promise.

Want a regrind policy set before you scale the run?

This calculator gives an engineering estimate. Our tooling team can run repeat-reprocessing data for your grade, set a metered let-down ratio, and write a regrind spec that protects impact, color and dimensions while cutting scrap — across our vetted manufacturing network in Taiwan, Vietnam and the US.

Book a 30-min call Send a drawing or sample