Is my shot a sensible percentage of the press barrel? Enter the part volume, the number of cavities, the runner, the resin and the barrel's polystyrene shot rating or its screw diameter and stroke. The calculator gives the shot weight, the share of the barrel the shot uses in your resin, the shot stroke in screw diameters, whether a cushion still fits, how long the melt sits in the barrel and which barrel sizes would put the shot in the right range.
Engineering estimate, not a quote. Final press and barrel selection comes from the press maker's specification for the exact screw, the resin processing guide and a molding trial.
An injection press does not melt plastic on demand. The screw rotates, conveys pellets forward, melts them and pushes the melt to the front of the barrel, retracting as the melt builds up. On injection the screw is pushed forward like a plunger and that melt pool becomes the shot. How far the screw can travel, and how much of that travel each shot uses, decides two things a part designer rarely sees but always pays for: whether the melt is uniform and whether it has been cooking in the barrel for too long.
Step 1: the shot. The shot is everything that leaves the nozzle in one cycle: every cavity plus the cold runner and sprue. Its solid volume is Vs = n × Vpart + Vrunner, and its weight is W = Vs × SG, the solid density of the molded resin.
Step 2: the barrel, in volume. Press makers rate injection units by the weight of general-purpose polystyrene they can inject, in ounces or grams. What the screw really sweeps is a volume: π/4 × D² × stroke. The calculator turns a PS rating into that swept volume by dividing by the melt density of polystyrene, about 0.95 g/cm³, or computes it directly from the screw diameter and maximum stroke.
Step 3: utilisation in your resin. The shot occupies the barrel as melt, not as solid, so its volume in the barrel is W ÷ ρmelt. Utilisation is that melt volume divided by the swept volume. The commonly published guideline is to keep it between 20% and 80%. The quick handbook rule, capacity in your resin = PS rating × SG ÷ 1.05, is shown for comparison; it uses solid densities and so understates how much barrel a semi-crystalline resin needs.
Step 4: stroke, cushion and residence. With the screw diameter known, the shot stroke is the melt volume divided by the screw's cross-section, and dividing by D gives the stroke in diameters, a number processors use directly. The cushion is added to check the shot still fits. Finally, the melt in front of the screw is used up over Vsw ÷ Vmelt shots, so a minimum estimate of how long it sits at temperature is that many cycles.
A two-cavity ABS housing: each part is 38.0 cm³ and the cold runner and sprue add 9.0 cm³. The candidate press has an 8 oz PS-rated injection unit with a 40 mm screw. The cycle is 30 s and the processor leaves a 5 mm cushion. ABS is taken at a solid density of 1.05 g/cm³ and a melt density of 0.94 g/cm³.
The two-cavity tool is a good fit for this barrel: the shot uses about 40% of it, the screw travels just under two diameters, a 5 mm cushion leaves plenty of stroke and the melt is used up in about two and a half cycles. Any injection unit rated from about 4 oz to about 16 oz PS would keep this shot inside the guideline, so the choice of press can be made on clamp force and platen size. The two extra lines show why the conversion matters. Molding the same tool in PP uses 44% of the barrel, not the 39% the specific-gravity rule suggests, because PP expands more when it melts. And a single small part on the same press would use about 4% of the barrel and sit at temperature for about 12 minutes, which is a real risk for heat-sensitive resins. Press Load the worked example above to reproduce these numbers.
The PS rating is a convenience: one number that lets buyers compare injection units. But polystyrene is an amorphous resin whose melt is only about 10% less dense than its solid, while semi-crystalline resins lose much more density when their crystals melt. PP drops from about 0.905 to about 0.73 g/cm³, so the same gram of PP takes about 24% more room in the barrel than it does in the mold. The handbook rule of multiplying the PS rating by the ratio of solid specific gravities treats every resin as if it expanded like polystyrene. For ABS, PC and other amorphous resins that is close enough; for PP, PE, POM and nylon it overstates the capacity, which is exactly the direction that hides an oversized shot. The calculator works in melt volume for the verdict and prints the specific-gravity figure beside it so you can see the gap.
| Method | Use it when | Limit |
|---|---|---|
| This calculator | Choosing a press size for a new tool; checking a molder's proposed press; deciding cavitation; spotting residence-time risk early | Representative densities; front-of-screw residence only; assumes the screw is in good condition with a sealing check ring |
| Specific-gravity rule alone | A quick look for amorphous resins such as ABS, PC, PS and PMMA | Understates the barrel needed for PP, PE, POM and nylon |
| Press maker's injection unit data | Final selection: swept volume, screw L/D, injection pressure and rate for the exact screw | Does not know your part or resin |
| Molding simulation | Fill, pack and the shot needed to fill a new or difficult tool, including runner balance | Needs a 3D model and a material card; does not pick the press for you |
| Short-shot study on the press | Confirming the real shot and cushion during the first molding trial | Needs the tool and the press |
The shot volume, shot weight and specific-gravity conversion of a PS-rated shot capacity follow the treatment in Rosato and Rosato, Injection Molding Handbook, and the injection-unit data that press makers publish (rated PS shot weight, screw diameter, stroke and swept volume). The melt-volume form of the check and the 20–80% barrel utilisation guideline are the approach set out in resin suppliers' processing guides and processing references, which also give the maximum residence times for their grades. The residence estimate (swept volume ÷ shot volume × cycle time) is the common front-of-screw approximation; it ignores melt held in the screw flights, which is why the true residence is longer. The solid and melt densities in the resin menu are representative published values, labelled as such and fully editable. The 1–4 D stroke range, the 0.95 g/cm³ PS melt basis and the design tips are page-set rules of thumb from processing practice, not press-maker data; where a press maker states a different basis for its PS rating, use theirs.
The commonly published processing guideline is 20–80% of the barrel's shot capacity, measured in the resin being molded. Below about 20% the melt sits in the barrel for many cycles and heat-sensitive resins can degrade, and the short screw stroke is hard to control. Above about 80% there is little room left for a cushion and the screw may not deliver a fully and evenly melted shot. Many processors prefer the middle of the band, and heat-sensitive resins sit better toward its upper half.
Presses are rated in ounces or grams of general-purpose polystyrene. The screw meters a volume of melt, so the accurate conversion uses melt densities: capacity in your resin = PS capacity × (melt density of your resin ÷ melt density of PS). The quick handbook rule uses solid specific gravities instead: PS capacity × (SG of your resin ÷ 1.05). The two agree within a few percent for amorphous resins, but the specific-gravity rule overstates the capacity for semi-crystalline resins such as PP, PE and POM, which expand more on melting. For an 8 oz PS barrel, PP at 0.73 g/cm³ melt density holds about 8 × 0.73 ÷ 0.95 = 6.1 oz, not the 6.9 oz the specific-gravity rule gives.
The melt stays in the barrel for many cycles, so its residence time grows, and resins such as PVC, POM, flame-retardant grades and some nylons can discolour, lose properties or gas. The screw also moves only a short distance per shot, so small differences in check-ring closing and screw position become a large fraction of the shot and part weight varies. A 9 cm³ ABS shot on an 8 oz barrel uses about 4% of it, and at a 30 s cycle the melt spends roughly 12 minutes in the barrel.
Above about 80% of capacity the screw has to retract close to its full stroke. The rear of the shot has had little time in the metering zone, so melt temperature can be uneven, and there may not be room for a cushion at the end of injection, which means the screw bottoms out and cannot hold pressure. Screw recovery time can also become longer than the cooling time and set the cycle. The fix is a larger barrel or press, or fewer cavities.
A common estimate is residence time = (barrel swept volume ÷ shot melt volume) × cycle time, the number of shots the stroke can hold times the cycle. For a shot using 39.8% of the barrel at a 30 s cycle that is 2.51 × 30 = 75 s. Melt also sits in the transition and feed flights of the screw, so the true residence is longer than this front-of-screw figure; some processors double it as a conservative check against the resin supplier's maximum residence time.
A common rule of thumb is a shot stroke of about 1–3 screw diameters, with up to about 4 diameters acceptable on many machines. Shorter than about 1 D the shot is hard to control; longer than about 4 D the screw's effective length for melting shrinks as it retracts and the melt quality can suffer. A 95 cm³ melt shot on a 40 mm screw needs a 75.6 mm stroke, or 1.89 D.
A cold runner and sprue do: they fill every shot and are ejected with the parts, so their volume is part of the shot weight and the barrel utilisation. With a hot runner the manifold stays full of melt between shots, so only the parts and any cold sub-runner count toward the shot, but the manifold's own melt volume adds to the residence time of a heat-sensitive resin.
Not sure whether to add a cavity, shrink the runner or move to a different press? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.
AI assistant. Answers can be wrong; nothing it says is a quote or a promise.
This calculator gives an engineering estimate. Our tooling team checks shot size, clamp force and cavitation together on your CAD, and proposes runner, coring or cavity changes while each one is still a design edit.
Book a 30-min call Send a drawing or sample