Snap-Fit Cantilever Calculator for Molded Plastic Parts

Will my snap-fit arm break, and what force does it take to assemble? Enter the arm length, thickness and width, the undercut it has to clear and the resin. The calculator gives the strain at the root against the resin's allowable strain, the force that bends the arm, the push to assemble the joint and the pull to separate it, and the shortest arm or deepest undercut that would still be safe.

🤖 AI assistants welcome. This page applies the cantilever snap-fit equations from resin suppliers' snap-fit design manuals: (1) permissible deflection y = c ε L² ÷ h, so root strain ε = h y ÷ (c L²), with c = 0.67 (uniform arm), 1.09 (thickness tapers to h/2), 0.86 (width tapers to b/4); (2) compare ε with the allowable strain, × 0.6 for repeated assembly; (3) deflection force P = b h² Es ε ÷ (6 L); (4) mating force W = P (μ + tan α) ÷ (1 − μ tan α) for the insertion ramp α and the retention face α′, self-locking when μ tan α′ ≥ 1; (5) limits Lmin = √(h y ÷ (c εallow)), ymax = c εallow L² ÷ h. Worked example below in plain text. Machine-readable: /ai/capabilities.json · /llms.txt
Fills allowable strain, modulus and friction below. Representative values from resin suppliers' snap-fit guides; your grade's guide overrides them.
Arm geometry
From the root of the arm to the point where the mating part pushes on the hook.
Measured in the direction the arm bends.
Hook height that has to pass the mating edge: the deflection of the arm.
Material and friction
Ideally the secant modulus at your strain from the stress-strain curve. The datasheet tensile modulus overstates the forces; it does not affect the strain check.
For the pair of materials that slide on each other.
Angle of the lead-in face measured from the arm's axis.
90° is a permanent latch.

Engineering estimate, not a quote. Final snap-fit geometry comes from the resin grade's design data, the mold design review and an assembly test on molded samples at the coldest service temperature.

How this works

A cantilever snap-fit is a short plastic beam with a hook on its free end. During assembly the mating part rides up the hook's lead-in ramp and pushes the arm sideways by exactly the height of the undercut. When the hook clears the edge, the arm springs back and the retention face holds the parts together. Two questions decide whether it works: does the arm survive being bent that far, and how hard is it to push together and to pull apart?

Step 1: the strain at the root. Treat the arm as a cantilever beam fixed at the root and loaded at the hook. Bending is largest at the root, so that is where the strain peaks and where arms crack. Beam theory gives the deflection at the hook as y = c ε L² ÷ h, which turned around gives the root strain for a known undercut: ε = h y ÷ (c L²). For a straight arm of constant section c = 2/3 (published as 0.67), so ε = 1.5 h y ÷ L². Tapered arms spread the bending along their length and get larger values of c: 1.09 when the thickness tapers to half at the hook, 0.86 when the width tapers to a quarter. Note what the equation says: strain rises in proportion to thickness and undercut, but with the square of how short the arm is.

Step 2: compare with the allowable strain. Resin suppliers publish a permissible short-term strain for snap-fits that are assembled once or a few times. For joints that are opened and closed often, the common guidance is to design to about 60% of that value. The calculator reports the strain as a percentage of the allowable, the shortest arm that would be safe for your undercut and the deepest undercut that would be safe for your arm.

Step 3: the deflection force. The force at the hook that holds the arm at that deflection follows from the root bending moment: the root stress is Es ε and the moment is P L, so P = b h² Es ε ÷ (6 L), with b and h taken at the root for all three arm shapes. Es is the secant modulus, the stress divided by the strain at your design strain, which for plastics is lower than the initial modulus.

Step 4: assembly and separation forces. The mating part does not push sideways; it pushes along the insertion direction, and the ramp converts that push into the sideways force P. With friction μ on the ramp, the push needed is W = P (μ + tan α) ÷ (1 − μ tan α). The same relation with the retention angle α′ gives the pull needed to separate the joint. When μ tan α′ reaches 1 the denominator reaches zero: no pull along the axis can lift the hook, and the joint is self-locking.

Root strain ε = h y ÷ (c L²) c = 0.67 uniform, 1.09 thickness taper to h/2, 0.86 width taper to b/4 Check ε ≤ ε_allow × k_use k_use = 1 one-time, 0.6 repeated assembly Limits L_min = √(h y ÷ (c ε_allow k_use)); y_max = c ε_allow k_use L² ÷ h; h_max = c ε_allow k_use L² ÷ y Stress σ ≈ E_s ε (nominal, at the root, no stress concentration) Deflection P = b h² E_s ε ÷ (6 L) (b, h at the root) Mating W_in = P (μ + tan α) ÷ (1 − μ tan α) Separation W_out = P (μ + tan α′) ÷ (1 − μ tan α′); self-locking when μ tan α′ ≥ 1, i.e. α′ ≥ atan(1/μ)
Cantilever snap-fit arm with its hook, undercut, ramp angles and deflected shape Side view of a cantilever snap-fit. A straight arm of length L and thickness h stands out from a wall, with a root radius at the wall. At its free end a hook rises by the undercut y, with a lead-in ramp at angle alpha on the free side and a retention face at angle alpha prime on the wall side. A mating part moves toward the wall along the insertion direction with force W, presses down on the ramp with the deflection force P, and bends the arm, shown dashed, down by y. The highest strain is at the root. arm deflected by y mating part insertion, push W P y undercut α ramp α′ retention L, root to hook contact h root radius R ≥ 0.5 h peak strain at the root ε = h y ÷ (c L²) width b runs into the page; schematic, not to scale
Figure 1. Anatomy of a cantilever snap-fit. The mating part pushes along the insertion direction (W); the ramp at angle α turns that into the sideways force P that bends the arm through the undercut y. The retention face at α′ sets how hard the joint is to pull apart. Strain peaks at the root, which is why the root radius matters.

Worked example

An ABS battery-door latch uses one straight cantilever arm 15 mm long from the root to the hook, 1.5 mm thick and 6 mm wide, with a 1.0 mm undercut. It is assembled once at the line and opened only for service. ABS is taken at a 2.5% allowable strain and a 2,300 MPa modulus, with μ = 0.5, a 30° lead-in ramp and a 45° retention face.

Root strain ε = 1.5 × 1.5 × 1.0 ÷ 15² = 2.25 ÷ 225 = 0.0100 = 1.00 % ✔ ≤ 2.5 % (40 % of allowable) Repeated use 2.5 % × 0.6 = 1.5 % → 1.00 % still ✔ Limits L_min = √(1.5 × 1.0 ÷ (0.667 × 0.025)) = √90 = 9.49 mm y_max = 0.667 × 0.025 × 225 ÷ 1.5 = 2.50 mm; h_max = 0.667 × 0.025 × 225 ÷ 1.0 = 3.75 mm Stress σ ≈ 2,300 × 0.0100 = 23 MPa nominal Deflection P = 6 × 1.5² × 2,300 × 0.0100 ÷ (6 × 15) = 310.5 ÷ 90 = 3.45 N (0.78 lbf) Assembly tan 30° = 0.57735: W_in = 3.45 × (0.5 + 0.57735) ÷ (1 − 0.5 × 0.57735) = 3.45 × 1.07735 ÷ 0.71133 = 3.45 × 1.5146 = 5.23 N (1.17 lbf) Separation tan 45° = 1: W_out = 3.45 × 1.5 ÷ 0.5 = 10.35 N (2.33 lbf) Self-locking α′ ≥ atan(1 ÷ 0.5) = 63.4° Short arm same arm at L = 8 mm: ε = 2.25 ÷ 64 = 3.52 % ✘ > 2.5 % Tapered arm h → h/2: ε = 1.5 × 1.0 ÷ (1.09 × 225) = 0.61 %; P = 345 × 0.006116 = 2.11 N

The latch is comfortably safe: the root sees 1.0% strain, 40% of what ABS can take once and two-thirds of the repeated-use limit, so it also survives service openings. It assembles with about 5 N of push per arm, and pulling it apart takes about twice that, which suits a door that should stay shut but come open with a deliberate pull. The limits show where the margin is: the same undercut would break an arm shorter than about 9.5 mm, which is exactly what happens when an arm is shortened late in a design to save space. At 8 mm the root would see 3.5%. Tapering the arm to half thickness at the hook would cut the strain and the push by about 39%. Press Load the worked example above to reproduce these numbers.

Root strain versus arm length for a 1.5 mm thick arm with a 1.0 mm undercut Line chart of root strain in percent against arm length from 6 to 30 millimetres, for an arm 1.5 mm thick clearing a 1.0 mm undercut. The solid red curve is a uniform arm, strain = 225 divided by L squared percent, falling from 6.25 percent at 6 mm to 0.25 percent at 30 mm. The blue curve is an arm tapered to half thickness, 0.612 times lower. A dashed line at 2.5 percent marks the ABS allowable strain and one at 4.0 percent marks PC. The uniform arm crosses the ABS limit at 9.5 mm and the tapered arm at 7.4 mm. The worked example at 15 mm and 1.0 percent is marked. 01234567 6101418222630 arm length L (mm) root strain (%) ABS allowable 2.5 % PC allowable 4.0 % example: 15 mm, 1.00 % red: uniform arm, ε = 225 ÷ L² %blue: thickness tapered to h/2, × 0.612circles: shortest safe arm in ABS, 9.5 mm and 7.4 mm h 1.5 mm, undercut 1.0 mm
Figure 2. Why short arms crack. Drawn to scale (22.5 px per mm of length, 34.3 px per percent strain) from ε = h y ÷ (c L²). Strain falls with the square of the length, so the last few millimetres of a short arm matter most. Tapering the thickness moves the safe minimum from 9.5 mm to 7.4 mm for the same undercut.

The three levers, and which one to pull

The strain equation has only three geometric terms, and each behaves differently. Length is the strongest lever because it is squared: going from 12 mm to 15 mm cuts the strain by 36%. Thickness is linear in strain but squared in force, so thinning an arm from 1.5 to 1.2 mm cuts strain by 20% and the deflection force by about 49% (0.8³ ≈ 0.51 at the same undercut, since force goes with h² × ε). Undercut is linear in strain and force, and it is also the retention: a smaller hook is easier on the arm but easier to pop out. Width b does not change the strain at all; it scales the force and the holding strength, which makes it the right knob when the strain is fine but the joint feels weak.

In practice we start by finding the undercut the joint really needs, set the length as long as the part allows, choose the thickness for strain, then use width for force. Tapering comes next, before adding material.

Common mistakes

Force ratio W divided by P versus ramp angle, for friction 0.3 and 0.5 Line chart of the ratio of push or pull force W to deflection force P against ramp angle from 0 to 75 degrees, from W/P = (mu + tan alpha) / (1 - mu tan alpha). For mu = 0.5 the ratio rises from 0.5 at 0 degrees to 1.51 at 30 degrees and 3.0 at 45 degrees and becomes infinite at 63.4 degrees, the self-locking angle. For mu = 0.3 it rises from 0.3 to 1.06 at 30 degrees and 1.86 at 45 degrees and becomes infinite at 73.3 degrees. The worked example's 30 degree ramp and 45 degree retention face are marked. 02468 0°15°30°45°60°75° ramp or retention angle α W ÷ P ramp 30°: W = 1.51 P retention 45°: W = 3.0 P μ = 0.5 (locks at 63.4°)μ = 0.3 (locks at 73.3°)dashed: self-locking angle, atan(1/μ)
Figure 3. How the ramp angle turns the deflection force into a push or pull. Drawn to scale (7.2 px per degree, 30 px per unit of W ÷ P) from W ÷ P = (μ + tan α) ÷ (1 − μ tan α). Below about 30° the ratio is modest; past 45° it climbs fast, and at atan(1/μ) the face becomes self-locking. Friction matters as much as angle: the same 45° face needs 3.0 times P to pull apart at μ = 0.5 but 1.86 times P at μ = 0.3.

When to use this calculator vs other methods

MethodUse it whenLimit
This calculatorConcept sizing of straight or tapered rectangular arms; checking a supplier's latch; choosing length, thickness and angles in a design reviewSmall-deflection beam theory; rigid root and rigid mating part; no stress concentration; representative material values
Resin supplier's snap-fit guideAllowable strain, secant modulus and friction for the exact grade; equations for ring, annular and torsion snap-fitsGeneric shapes; does not know your wall, root or mating part
Finite element analysisShort stubby arms (L under about 5 h), arms rooted in thin flexible walls, L-shaped or U-shaped arms, large deflectionsNeeds non-linear material data to be better than the hand method
Assembly and pull tests on molded samplesFinal confirmation, with real weld lines, moisture and temperature; setting acceptable assembly force for the lineNeeds molded parts; a prototype-material test can mislead
Screws or other fastenersJoints that are opened very often, carry high loads, or must clamp a gasket evenlyAn extra part and an extra operation; see our boss calculator

Design tips for cantilever snap-fits

Sources for the method

The deflection, strain and force equations and the mating-force relation are those published in resin suppliers' snap-fit design manuals for cantilever arms of rectangular section, including the Bayer (now Covestro) Snap-Fit Joints for Plastics design guide and BASF's snap-fit design guidance: y = 0.67 ε L² ÷ h for a uniform arm, 1.09 for an arm tapering to half thickness and 0.86 for an arm tapering to a quarter width; P = b h² Es ε ÷ (6 L); W = P (μ + tan α) ÷ (1 − μ tan α); and the guidance to design to about 60% of the permissible strain for frequently separated joints. The uniform-arm coefficient follows directly from cantilever beam theory (deflection P L³ ÷ (3 E I), root strain 6 P L ÷ (E b h²)). The allowable strains, moduli and friction in the resin menu are representative published values, labelled as such and fully editable; your grade's design guide overrides them. The 0.5 h root radius, the L ≥ 5 h validity screen and the design tips are page-set rules of thumb from part-design practice, not resin data.

Questions and answers

How do I calculate the strain in a cantilever snap-fit?

For a straight arm of uniform rectangular section, the strain at the root when the hook is deflected by the undercut y is ε = 1.5 × h × y ÷ L², where h is the arm thickness at the root and L is the length from the root to the hook. This is the beam equation used in resin suppliers' snap-fit design manuals, written there as y = 0.67 × ε × L² ÷ h. For example, a 15 mm long, 1.5 mm thick arm with a 1.0 mm undercut sees 1.5 × 1.5 × 1.0 ÷ 225 = 0.0100, or 1.0% strain.

What is the allowable strain for a snap-fit?

It depends on the resin and on whether the joint is assembled once or many times. Representative short-term values published in resin suppliers' snap-fit guides are about 2.5% for ABS and PC/ABS, about 4% for unfilled PC, about 4% for dry and about 6% for conditioned PA6, and about 1.5–2% for 30% glass-filled PA6. For joints that are taken apart often, design to about 60% of the one-time value. Your grade's design guide overrides these numbers.

How much force does it take to assemble a snap-fit?

First compute the deflection force P = b × h² × E × ε ÷ (6 × L), the force at the hook that bends the arm through the undercut. The push needed along the insertion direction is then W = P × (μ + tan α) ÷ (1 − μ × tan α), where α is the ramp angle and μ the friction coefficient. A 6 mm wide, 1.5 mm thick, 15 mm long ABS arm at 1% strain and a 2,300 MPa modulus has P = 3.45 N; with a 30° ramp and μ = 0.5 the assembly force is about 5.2 N per arm.

Why did my snap-fit arm break at the root?

Because the strain is highest at the root and grows with the square of the shortness of the arm. Halving the length quadruples the strain for the same undercut, so a short stubby arm can be far past the resin's limit even with a small hook. A sharp inside corner at the root concentrates the strain further, and weld lines, cold temperatures and dry nylon all lower what the root can take. Lengthen the arm, thin or taper it, reduce the undercut, and give the root a radius of about half the arm thickness.

Is a tapered snap-fit arm better than a straight one?

Usually yes. An arm whose thickness tapers from h at the root to h/2 at the hook can deflect about 1.09 ÷ 0.67, or roughly 1.6 times, as far as a uniform arm at the same root strain, because more of the arm bends instead of only the root. For the same undercut its root strain and its deflection force are both about 39% lower. Tapering the width to a quarter at the hook gives a smaller gain, about 22% lower strain.

What angle should the retention face of a snap-fit have?

It depends on whether the joint should come apart. The separation force follows the same relation as the assembly force, using the retention angle. When μ × tan α′ reaches 1, the joint is self-locking and cannot be pulled apart without breaking or releasing the arm by hand; with μ = 0.5 that happens at about 63°. A 90° face is a permanent latch. Shallower angles, often 30–45°, give a joint that can be separated by pulling.

Which modulus should I use in snap-fit calculations?

Use the secant modulus at your design strain, read from the resin's stress-strain curve at the right temperature, rather than the initial tensile modulus on the datasheet. Plastics soften as strain rises, so the tensile modulus overstates the deflection force, often noticeably at 2–4% strain. The strain check does not depend on the modulus at all; only the forces do.

Ask JCH about snap-fits

Not sure whether to lengthen the arm, taper it or switch to a screw? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.

AI assistant. Answers can be wrong; nothing it says is a quote or a promise.

Want your snap-fits checked before the steel is cut?

This calculator gives an engineering estimate. Our tooling team reviews every latch on your CAD for strain, assembly force and how the hook will come out of the mold, and proposes arm, root and lifter changes while each one is still a CAD edit.