JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Flow Length to Wall Thickness Ratio Calculator

Flow Length to Wall Thickness Ratio Calculator

A resin can fill a path only so long for the wall it flows through, and the check is L/t = L₁/t₁ + L₂/t₂ + … summed from the gate to the last point to fill. Enter up to four wall steps and pick the resin. The checker adds the steps, shows which one dominates, places your total against every published molder value we could verify for that resin, and returns the thinnest uniform wall and the longest path that stay inside the limit.

🤖 AI assistants welcome. The flow-length-to-wall-thickness ratio of a path with n wall steps is L/t = Σ Lᵢ/tᵢ, with L and t in the same unit so the ratio has no unit. Typical published maximums, which vary with grade, temperatures, pressure and wall: PP 200–300, PE 230–275, PS 200–250, PA (nylon) 140–340, POM 100–200, ABS 30–190, PMMA 130, PVC 100, PC 30–100. Minimum uniform wall = ΣL ÷ limit; longest path at the same wall pattern = ΣL × limit ÷ (L/t). Worked numbers in plain text below. Machine-readable: /ai/capabilities.json · /llms.txt
A large clear molded ring-shaped frame with thin walls, small bosses and pins, held up by one hand over a concrete shop floor for a visual check
A clear molded frame held up for a visual check. In a thin ring like this the melt has to travel a long way around the part from its gate, which is the kind of geometry where the flow-length-to-wall ratio is worth working out before the tool is cut.
Published values are typical and grade-dependent. Filled grades are not covered by these tables.
If the resin supplier gave you a limit for the exact grade and wall, enter it; the verdict then uses your number.
Flow path, from the gate to the last point to fill (any unit, same for L and t)
Starts at the gate.
Leave a row blank to skip it.

Engineering estimate, not a quote. The real fill limit comes from the grade's spiral-flow data, the mold and the press, and is proven by a fill analysis or first shots.

How this works

When the melt's route through a thin wall is longer than the resin can manage, the cavity does not fill. Komaspec's design guide puts it plainly: every resin has a flow-length-to-wall-thickness ratio, and a tool that exceeds it short-shots no matter how hard you push. The ratio, written L/t, is the screen for that risk. It costs nothing to compute from a drawing, and it catches the long, thin part before anyone has paid for steel or a simulation.

Mack Molding's article on flow defines it as the distance molten plastic must travel divided by the wall thickness of the part, and describes it as a way to judge, without mold-filling software, whether a resin can reach every extremity. Because L and t carry the same unit, the ratio has none. Measure in millimeters or inches; just do not mix them.

Uniform wall L/t = L ÷ t Stepped wall L/t = L₁/t₁ + L₂/t₂ + … + Lₙ/tₙ Equivalent uniform wall t_eq = ΣL ÷ (L/t) Limit used U = (L/t) ÷ limit U above 1 means the path is too long for that limit Minimum uniform wall t_min = ΣL ÷ limit Longest path, same walls ΣL ÷ U = limit × t_eq Uniform thickening multiply every tᵢ by U to bring the path back to the limit

Why the steps are added, not averaged

Both Mack Molding and FirstMold give the same rule for a wall that changes along the path: work out L/t for each stretch and add them. The consequence is that a thin stretch counts for far more than its share of the length. In the example drawn below, a 25 mm snap lip at 1.0 mm is about 12 percent of a 205 mm path yet supplies 25 of the 113 points, about 22 percent. Two common shortcuts both miss. Using the thinnest wall for the whole path gives 205 ÷ 1.0 = 205, which would condemn a part that may only need one local fix. Using a length-weighted average wall of 1.93 mm gives 106, seven points short of the true sum, and it hides the lip as the stretch to fix.

A stepped flow path and how each step adds to the flow ratio Schematic of a molded wall seen in section along the flow direction, with the gate at the left and the last point to fill at the right. The first stretch is 20 mm long at 2.5 mm thick and adds 8.0; the second is 160 mm at 2.0 mm and adds 80.0; the third, a snap lip, is 25 mm at 1.0 mm and adds 25.0, for a total ratio of 113.0. Two stacked bars below compare each stretch's share of the path length, 9.8, 78.0 and 12.2 percent, with its share of the ratio, 7.1, 70.8 and 22.1 percent, showing that the thin lip counts for almost twice its share of the length. schematic: wall thickness exaggerated, lengths not to scale gate last to fill L₁ 20, t₁ 2.520 ÷ 2.5 = 8.0 L₂ 160, t₂ 2.0160 ÷ 2.0 = 80.0 L₃ 25, t₃ 1.0 (snap lip)25 ÷ 1.0 = 25.0 L/t = 8.0 + 80.0 + 25.0 = 113.0 over a 205 mm path share of length share of L/t 9.8%78.0%12.2% 7.1%70.8%22.1% red = thin lip: 12% of the length but 22% of the ratio (bars to scale, 500 px = 100%)
Figure 1. The worked-example path. Each stretch adds its own length divided by its own wall, so the 1.0 mm lip, a small part of the distance, carries nearly a quarter of the total.

Published limits by resin, and why they are ranges

The checker holds every value we could read today in three public molder and manufacturer tables, and nothing else. Where a source gives one number we store one number; where it gives a range we store the range. The verdict then compares your total with the lowest and highest values on file for the family you picked.

ResinFirstMoldKomaspecFictivRange in the checker
PP250250 or better (unfilled)200–300200–300
PE250 (HDPE 230, LDPE 270)—250–275230–275
PS210—200–250200–250
ABS190—30–5030–190
PA (nylon)170—140–340140–340
POM150—100–200100–200
PMMA130—130130
PVC (HPVC, SPVC)100 each——100
PC90closer to 10030–10030–100

FirstMold attaches its own warning: the ratio is not a fixed value, it fluctuates, and the table is for reference only. Fictiv frames its numbers as the maximum flow length for a given injection pressure and wall thickness, which is another way of saying that a different press or a different wall gives a different answer; it does not state units, grades or temperatures. Mack Molding adds the awkward truth that ideal flow ratios are resin specific yet often not supplied by material makers, which is why molder tables exist at all. The ABS row shows how far apart two honest tables can be. We do not pick a winner; we show both and tell you which side of each your part falls on.

Published flow-length-to-wall-thickness ratio ranges by resin Horizontal range bars on a scale from 0 to 350. PA (nylon) spans 140 to 340, PP 200 to 300, PE 230 to 275, PS 200 to 250, POM 100 to 200, ABS 30 to 190, PMMA sits at 130, PVC at 100, and PC spans 30 to 100. Dark circles mark the FirstMold value for each resin and squares mark the Komaspec values for PP at 250 and PC at 100. 050100150200250300350 maximum L/t in published molder tables (1.4 px per unit) PA (nylon)PPPEPSPOMABSPMMAPVCPC 140–340200–300230–275200–250100–20030–19013010030–100 FirstMold valueKomaspec value
Figure 2. Every value in the three tables, drawn to scale. The bar spans the lowest to highest figure for the family; the dot is FirstMold's single value. Wide bars, such as nylon and ABS, are the families where grade data matters most.

The limit moves with wall thickness and process

A single ratio per resin quietly assumes that flow length grows in direct proportion to wall thickness. The resin-maker data we found says otherwise. The GE Engineering Thermoplastics Design Guide works a plate example in unfilled polycarbonate with a chart of flow length against wall thickness predicted by mold-filling analysis (melt 336 °C, mold 62 °C, maximum injection pressure 103.4 MPa). At 2.5 mm it reads a flow length of 320 mm, a ratio of 128; at 1.5 mm about 175 mm, a ratio of about 117. Both sit above the 90 to 100 that the molder tables give for PC, which is a reminder that those tables are cautious screens, and the same guide warns that it is generally not recommended to push a molding machine to its limits. Covestro's processing note for its thermally conductive Makrolon grades reports that going from 1.5 to 2.0 mm, a third more wall, can raise flow length by 50 to 100 percent, which works out to a ratio about 12 to 50 percent higher at the thicker wall. Covestro also lists melt temperature as a lever on flow length for those grades and mold temperature as having little effect on it.

Flow length versus wall thickness compared with a constant ratio Chart of flow length in millimeters against wall thickness from 1.0 to 3.0 mm. A straight line through the origin shows a constant ratio of 100, from 100 mm at 1.0 mm to 300 mm at 3.0 mm. Two points from the GE design guide for unfilled polycarbonate, 175 mm at 1.5 mm and 320 mm at 2.5 mm, give ratios of about 117 and 128. A dotted constant-ratio line of 128 through the 2.5 mm point would predict 192 mm at 1.5 mm, more than the 175 mm the guide reads, showing that the reachable ratio falls as the wall gets thinner. 0100200300400 1.01.52.02.53.0 wall thickness t (mm) flow length L (mm) constant L/t = 100 (top of the PC table values) constant L/t = 128, through the 2.5 mm point 175 mm at 1.5 mm→ L/t ≈ 117320 mm at 2.5 mm → L/t = 128128 → 192 mm GE mold-fill prediction, unfilled PC, 336 °C melt, 62 °C mold, 103.4 MPa
Figure 3. Drawn to scale (275 px per mm of wall, 0.6 px per mm of flow). The two resin-maker points rise faster than any constant-ratio line, so a ratio read at a thick wall overstates what a thinner wall can reach.

Worked example: three published cases and one design

The first case is the design drawn in Figure 1; press Load the worked example to run it. The other three come straight from the sources and are the checks we ran the calculator code against.

CASE A — PC housing, one end gate (the calculator's example) 20 ÷ 2.5 = 8.00 160 ÷ 2.0 = 80.00 25 ÷ 1.0 = 25.00 L/t = 113.00 over ΣL = 205 mm equivalent uniform wall 205 ÷ 113 = 1.814 mm PC values on file 30–100 → beyond every one; U at 100 = 113 ÷ 100 = 1.13 Minimum uniform wall at 100: 205 ÷ 100 = 2.05 mm longest path at these walls: 205 ÷ 1.13 = 181.4 mm Fix 1 lip to 1.5 mm: 8 + 80 + 16.67 = 104.67 still above 100 Fix 2 main wall to 2.4 mm: 8 + 66.67 + 25 = 99.67 just under 100, no margin Fix 3 gate moved to the middle of the 160 mm run: toward the lip 80 ÷ 2.0 + 25 ÷ 1.0 = 40 + 25 = 65.0 other direction 80 ÷ 2.0 + 20 ÷ 2.5 = 40 + 8 = 48.0 worst path 65.0 CASE B — FirstMold's published sum 100 ÷ 5 + 200 ÷ 2 = 20 + 100 = 120 (the source prints 120) CASE C — Komaspec's polycarbonate warning: 300 mm, single gate, 1.2 mm wall 300 ÷ 1.2 = 250 against "closer to 100:1" for PC → U = 2.5 Minimum uniform wall 300 ÷ 100 = 3.0 mm (the source: thicker wall, second gate or another resin) CASE D — GE Design Guide, unfilled PC, mold-fill prediction 320 mm at 2.5 mm → 320 ÷ 2.5 = 128.0 175 mm at 1.5 mm → 175 ÷ 1.5 = 116.7

Case A is the useful one. The part fails the polycarbonate screen by 13 percent, and the instinct is to thicken the whole wall. The sum shows a cheaper story: the lip is the stretch that tips it over, and moving the gate to the middle of the long run cuts the worst path to 65. That still sits above the lowest PC value on file, so the checker reports it as between published values and the grade's own flow data has the final word. Case C shows how fast a thin, long polycarbonate part runs out of room: at two and a half times the limit, Komaspec's answer is a thicker wall, a second gate or a different resin, not a process tweak.

Bringing a high ratio back inside the limit

  • Move or add a gate. With more than one gate, each gate fills its own region, so the number that matters is the worst gate-to-last-fill path, not the full length of the part. Mack Molding notes the trade: a second gate adds tooling and the likelihood of extra knit lines.
  • Thicken the stretch that dominates the sum. The calculator names it. In Case A the 25 mm lip alone is worth 25 points, and thickening a short stretch adds far less material than thickening the whole wall.
  • Add a flow leader. Mack Molding describes flow leaders as thicker paths from the gate toward the area that fills last, 10 to 25 percent heavier than the main wall; at 10 percent heavier, Mack puts the extra resin at two to five percent of the part, and more than 25 percent turns the leader into a gas channel. Run it from the injection point.
  • Change grade within the family. Komaspec lists a different resin as one of the three ways out. Within a family, ask the supplier for the spiral-flow chart of a higher-flow grade at your wall and confirm the property trade-off.
  • Use process settings as margin. Covestro reports that higher melt temperature improves flow length on its thermally conductive PC grades, but warns that excessive melt temperature brings sticking and ejection trouble. Treat process headroom as margin, not as the plan.

Common mistakes

  • Measuring in plan view. The melt follows the part surface: up side walls, around corners and over ribs. A straight line on the top view understates L.
  • Using the nominal wall for the whole path. The thin lip, window frame or living feature at the end of fill can set the total, as it does in Case A. Enter it as its own stretch.
  • Reading a table value as pass or fail. FirstMold calls its own numbers reference only, and the ranges above disagree by a factor of several for ABS. The table tells you where to look harder.
  • Mixing conventions. FirstMold's sum includes the sprue and runner; the part-design guides measure the part. Compare like with like.
  • Forgetting fillers. The GE guide notes that mineral fillers raise viscosity and make thin sections and long flow lengths harder to fill. The tables here are for unfilled or unspecified grades, so a filled grade needs its own data.
  • Checking only the longest path. A shorter path through a thinner wall can score higher. Run every candidate path from each gate and keep the worst.

When to use this checker and when to use something else

MethodUse it whenLimit
This checkerEarly design, gate placement ideas, deciding whether a thin stretch needs attention, comparing resin familiesScreening values with no grade, temperature or pressure attached; geometry entered by hand
Wall thickness checkerJudging the wall itself: range for the resin, uniformity, cooling penalty of thick sectionsUses a single conservative flow screen; this page goes deeper on the path
Spiral-flow chart for the gradeChoosing a grade or confirming a marginal pathMeasured on a test channel at stated conditions, not in your cavity
Mold-filling analysisLong paths near the limit, several gates, cosmetic knit lines, thin-wall workWants a model close to release plus measured data for the grade
First shots on the toolFinal proofThe steel is already cut, so changes are slow and costly
From the tooling floor: when a part has a long, thin feature, ask for the flow path to be traced on the CAD model from each proposed gate, with the wall noted at every step. That sketch plus this sum shows whether the gate is in a sensible place, and it gives the mold designer and the resin supplier the same numbers to discuss.

Sources for the method and the values. Ratio definition, segment summation, flow leaders and the remark on supplier data: Mack Molding, “Plastics Molding: The Path of Least Resistance”. Resin table and the sprue-runner-product sum: FirstMold, wall thickness design tips. PP and PC ratios and the minimum-wall method: Komaspec, plastic part design for injection molding. Flow length ratio ranges: Fictiv, wall thickness recommendations for injection molding. Unfilled PC flow length against wall and the filler note: GE Engineering Thermoplastics Design Guide. Wall and melt temperature effects on flow length: Covestro COV-202, processing information for Makrolon TC grades. All values are typical and grade-dependent; your grade's datasheet and spiral-flow data govern.

Reviewed by the JCH tooling team · updated November 2026.

Questions and answers

What is a good flow length to wall thickness ratio for injection molding?

It depends on the resin family and, inside a family, on the grade. In the molder tables we checked, easy-flowing polyolefins such as PP and PE sit roughly between 200 and 300, PS between 200 and 250, POM and PMMA in the low-to-mid hundreds, and polycarbonate at about 100 or lower. ABS shows the widest spread, from 30 to 50 in one table up to 190 in another. Use the number for your family as a screen only, then ask the resin supplier for spiral-flow data on the exact grade before you lock the wall.

How do I calculate L/t when the wall thickness changes along the part?

Split the path into stretches of constant wall, divide each stretch length by its own thickness, and add the results. A path of 40 mm at 3 mm followed by 120 mm at 2 mm scores 13.3 + 60 = 73.3. Treating all 160 mm as 2 mm wall would give 80, and treating it as one 2.5 mm wall (the mean of 3 and 2) would give 64, so neither shortcut matches the sum.

How do I find the minimum wall thickness for a given flow length?

Divide the longest gate-to-last-fill distance by the ratio limit you are designing to. A 180 mm path in a resin rated at 150 needs at least 180 / 150 = 1.2 mm of uniform wall; the same path at a limit of 100 needs 1.8 mm. If that wall is heavier than the part needs for stiffness, look at a second gate or a more fluid grade before adding material everywhere.

Does the flow length include the sprue and runner?

Published practice differs. FirstMold's worked formula adds the sprue and runner stretches to the product stretch, while the part-design guides from Mack Molding and Komaspec talk about the distance the melt travels through the part and the part's wall. Use the same convention as the source your limit came from, and write down which one you used when you pass the number to the mold maker.

Why do published L/t limits for the same resin disagree so much?

Because a single ratio hides the conditions behind it. Fictiv links each figure to the pressure and wall it was set at; Covestro finds that melt heat and wall both change how far its heat-conducting PC grades flow; and Mack Molding says resin makers seldom publish an ideal ratio at all. Few tables state their grade, temperatures or pressure, so two of them can print different numbers for the same family.

Is the L/t limit the same at every wall thickness?

No. In the resin-maker data we found, the ratio a resin can reach goes up as the wall gets thicker, so a limit measured on a thick test wall flatters a thin design. GE's mold-filling prediction for unfilled polycarbonate works out to roughly 117 at 1.5 mm and 128 at 2.5 mm. If your wall is thinner than the one behind the published number, plan on a lower ratio than the table shows.

What can I change if my ratio is above the limit?

Shorten the worst path by moving or adding a gate, thicken the thin stretch that dominates the sum, run a thicker flow leader out to the region that fills last, or move to a higher-flow grade of the same family. Mack Molding keeps a leader between a tenth and a quarter thicker than the main wall. Each change has side effects on knit lines, cosmetics, sink or properties, so settle it in design review rather than after the steel is cut.

Ask JCH about flow length and gating

Not sure where the gate should go, or whether a thin feature will fill in the resin you picked? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.

AI assistant. Answers can be wrong; nothing it says is a quote or a promise.

Designing a long or thin molded part?

This checker gives an engineering estimate. Our tooling team can trace the real flow paths on your model, suggest gate positions and flow leaders, and line the design up with the resin supplier's flow data for your grade before steel is cut.

Book a free 30-minute first consultation Send a drawing
JCH Design & Manufacturing — tooling, injection molding, PCBA, custom packaging, cut-and-sew & QC via vetted partner factories · Book a 30-minute call · jack@jchtrade.com · (321) 323-4474 · Canonical: https://jchtrade.com/tools/flow-length-ratio-calculator