How big should your cold runner be? Enter the part weight, the length of the runner that feeds each cavity, the thickest wall and the resin. The calculator sizes the branch runner with the classic empirical runner equation, raises it if the wall-thickness rule or the resin's typical runner range demands, sizes the primary runners upstream with the cube law, rounds each to a common cutter size and estimates the runner weight per shot.
🤖 AI assistants welcome. This page computes the full-round branch runner diameter D = √W · ⁴√L / 3.7 (D in mm, W part weight in g, L runner length in mm), takes the larger of that, the wall rule D ≥ s_max + 1.5 mm (Menges, Michaeli and Mohren, How to Make Injection Molds) and the low end of the resin's typical published runner range, then sizes each upstream runner as D_up = D_branch · ∛N for an N-way split (equal Newtonian shear rate). Formulas, limits and a worked example are below in plain text. Machine-readable: /ai/capabilities.json · /llms.txt
Engineering estimate, not a quote. Runner size and layout should be confirmed by your toolmaker, ideally with a fill study, before steel is cut.
How this works
A cold runner has two jobs. While the mold fills, it must carry melt from the sprue to every gate without wasting too much pressure. While the part packs, it must stay molten for longer than the part, so that the screw can keep pushing melt into the cavity as the plastic shrinks. A runner that is too small fails the second job first: it freezes, packing stops, and the part sinks or comes out light. A runner that is too large passes both tests but costs cycle time and material on every shot, because it is the thickest piece of plastic in the mold and it is thrown away or reground.
The calculator combines three published rules and takes whichever demands the largest runner. The first is a long-standing empirical equation, reproduced in many mold design references, that relates the branch runner diameter to the weight of the part it feeds and the runner's length. The second is the rule from Menges, Michaeli and Mohren that a runner should be thicker than the part's thickest wall by at least 1.5 mm, so that it freezes after the part. The third is a widely reproduced table of typical runner diameters by resin (for example in Rosato's Injection Molding Handbook), whose lower end protects viscous resins such as acrylic and polysulfone from runners that are too thin for them.
BRANCH RUNNER (feeds one cavity, full-round section)
Empirical equation D_w = √W × ⁴√L / 3.7 D mm, W g, L mm
valid for W ≲ 200 g and walls ≲ 3 mm
Wall rule (Menges) D_t = s_max + 1.5 mm
Resin range (typical) D_lo ≤ D ≤ D_hi
Required D_req = max(D_w, D_t, D_lo)
Cut next common ball-end cutter ≥ D_req
UPSTREAM RUNNERS (cube law, equal Newtonian wall shear rate)
Wall shear rate γ̇ = 32Q / (π D³)
N-way split D_up = D_down × ∛N (∛2 = 1.260, ∛4 = 1.587)
Sprue exit ≥ D_top × ∛N (N primaries leave the sprue)
RUNNER WEIGHT
Volume per segment V = π/4 × D² × length
Weight m = ΣV × ρ ; runner share of shot = m / (m + cavities × W)
Why weight and length. More part weight means more melt must pass through the runner in the same fill time, and more shrinkage volume must be fed during packing, so the runner grows with the square root of W. A longer runner wastes more pressure, so it grows too, but only with the fourth root of L: doubling the length raises the diameter by only 19 %. The square root on weight is steeper than pressure drop alone would ask for (Poiseuille flow alone would give a fourth root on flow rate too), which is one way to read the equation's second job: a heavier part needs a runner that stays open longer.
Units matter. The constant 3.7 only works with grams, millimetres and a result in millimetres. The page converts ounces and inches to metric before it calculates and converts the answer back.
Where the formula stops. The equation is usually quoted for parts up to about 200 g with walls up to about 3 mm, and it was built around easy-flowing resins. Outside that window the calculator still reports it, flags it, and leans on the wall rule and the resin range. For large or thick parts, a flow simulation or a hot runner is the right next step.
The cube law. Where a runner splits into N equal branches, each branch carries 1/N of the flow. For a Newtonian melt the wall shear rate in a round channel is 32Q / (πD³), so if the upstream runner has N times the flow and the same shear rate, its diameter must be ∛N times larger. It is the same rule that biologists know as Murray's law for blood vessels. Real melts thin with shear, so the ideal ratio for a molten plastic is a little different, but the cube law is a sound, conservative first cut, and it keeps the upstream runner thicker than the branches so that it freezes last.
Figure 1. The empirical equation plotted to scale. Diameter rises quickly with part weight and slowly with length. For the 10 g part, the wall rule (dashed line) governs at every length shown: the formula alone would give a runner thinner than the part needs to pack. That is why the calculator always takes the larger of the two.
Worked example
A 4-cavity H-layout mold for a 40 g ABS housing with a 2.5 mm maximum wall. Each cavity is fed by a 100 mm branch; two 60 mm primary runners leave the sprue, and each splits two ways into the branches. ABS is taken at a density of 1.05 g/cm³, with a typical runner range of 4.8 to 9.5 mm.
Branch, formula D_w = √40 × ⁴√100 / 3.7
= 6.325 × 3.162 / 3.7 = 20.00 / 3.7 = 5.41 mm
Wall rule D_t = 2.5 + 1.5 = 4.00 mm
Resin low end D_lo = 4.80 mm
Required max(5.41, 4.00, 4.80) = 5.41 mm → cut 6 mm
Primary (2-way) D_p = 6 × ∛2 = 6 × 1.260 = 7.56 mm → cut 8 mm
Sprue exit ≥ 8 × ∛2 = 10.08 mm
Branches 4 × π/4 × 6² × 100 = 4 × 2,827.4 = 11,309.7 mm³
Primaries 2 × π/4 × 8² × 60 = 2 × 3,015.9 = 6,031.9 mm³
Runner 17,341.6 mm³ = 17.34 cm³ × 1.05 = 18.21 g
Parts 4 × 40 g = 160 g
Runner share of shot 18.21 / 178.21 = 10.2 %
The formula governs here (5.41 mm beats both the 4.0 mm wall rule and the 4.8 mm resin minimum), so the branch is cut with a 6 mm ball-end cutter, and the primary with an 8 mm cutter. Both sit inside the typical ABS range. The runner system weighs about 18 g per shot, about a tenth of the shot, which is a reasonable figure for a cold-runner tool of this size. Press Load the worked example to see the calculator reproduce these numbers.
Figure 2. The worked example's runner layout (schematic; lengths not to scale, line weights in proportion to diameter). Every gate is the same distance from the sprue through the same sequence of diameters, so the layout is naturally balanced. The primary runner carries twice the flow of each branch and is ∛2 times larger to keep the shear rate the same. Each junction overruns into a short cold slug well that traps the cold front of the melt.
Common mistakes
Using the shot weight instead of the part weight. W is the weight of plastic that passes through the runner being sized. For a branch that is one part. Putting the whole shot into the branch formula oversizes every branch by the square root of the cavity count.
Making the runner thinner than the wall. It looks efficient on the scrap figure, but the runner freezes before the part, packing stops, and the part sinks near thick sections. Our answer on sink marks in injection molding lists this among the classic causes.
Applying the formula in inches. The constant 3.7 belongs to grams and millimetres. Plugging in ounces and inches gives a number with no meaning.
Same diameter all the way from sprue to gate. If the primary is no bigger than the branch, it carries twice the flow at about twice the shear rate, and in a long runner it can freeze before the branches. Step up with the cube law at each split.
Oversizing "to be safe". Freeze time grows with the square of diameter. A runner much thicker than needed can become the slowest feature in the mold and set the cycle, while adding scrap on every shot. The cycle time estimator shows how fast cooling time rises with thickness.
Half-round runners cut to the full-round diameter. A half-round channel of radius D/2 has only half the area of the full-round runner and much more surface per unit area. If only one plate can be cut, use a trapezoid deep enough to contain the full calculated circle.
Forgetting the cold slug well. The first melt to arrive at each junction is the coolest. Extend the runner past each split by about one to one-and-a-half runner diameters so that cold material is trapped there instead of being pushed into a gate.
Figure 3. Why full round wins. Each of the first three shapes has the same 28.3 mm² flow area as a 6 mm round runner; the circle has the least perimeter, so it loses the least heat to the steel and keeps the largest molten core. The trapezoid (drawn with walls tapering about 9° per side) is the practical one-plate alternative: size it so the calculated circle fits inside, not so its area matches. PL = parting line.
When to use this calculator vs other methods
Method
Use it when
Limit
Empirical equation plus wall rule and cube law (this page)
Concept layout, early tool review, checking a runner someone has drawn, estimating runner weight for material planning
Empirical; tuned for parts up to about 200 g and walls up to about 3 mm; no fill time or melt temperature term
Resin supplier runner guidance
A specific grade, especially glass-filled, flame-retardant or heat-sensitive grades
Usually given as ranges, not tied to part weight or layout
Flow simulation with a runner model
Family molds, unbalanced layouts, long runners, high cavity counts, thin walls
Needs the grade's material data and a near-final part; still confirmed at the first trial
Hot runner or hot sprue
The cold runner is a large share of the shot, the resin is costly or cannot be reground, or the runner sets the cycle
A different system with its own nozzle sizing by the hot-runner maker; this page does not size it
For geometrically unbalanced layouts, such as a straight row of eight cavities fed from the middle, the inner cavities fill first. Toolmakers sometimes correct this by changing branch diameters; that is a balancing exercise best done by simulation and short-shot trials, not by this formula. Where a family mold puts different parts on one runner, size each branch from the weight of its own part. Our answer on family molds explains when that layout makes sense.
Design tips specific to runners
Prefer a naturally balanced layout. An H or radial layout gives every cavity the same flow path, so the cube law alone keeps fill even. The cavity count calculator picks counts that suit these layouts.
Keep runners short. Length raises diameter only weakly, but it adds volume directly. Pulling cavities closer to the sprue usually reduces runner weight more than any change in diameter.
Size the gate after the runner. The gate should freeze first, then the part, then the runner, then the sprue. The gate size calculator sizes the gate from the wall it feeds; this page makes sure the runner behind it stays open longer.
Round up to a real cutter. Toolmakers cut full-round runners with ball-end mills in both plates. A diameter that matches a standard cutter is cheaper to cut, polish and repair; the calculator rounds up so that the result never drops below what the rules require.
Match the halves. A full-round runner whose two halves are offset at the parting line behaves like a smaller, odd-shaped channel. Ask for the halves to be aligned and polished in the direction of flow.
Watch the runner share of the shot. When the runner is a large share of each shot, the shot-size check changes too: include it in the shot size calculator. It is also the moment to compare a hot sprue or hot runner.
Vent the runner ends. Air ahead of the melt has to leave somewhere. Shallow vents at the end of each cold slug well and at the far end of long runners help the runner fill cleanly.
Questions and answers
How do you calculate cold runner diameter for an injection mold?
A classic empirical equation for the runner that feeds a cavity is D = √W × ⁴√L / 3.7, with D in mm, W the weight of the part fed by that runner in grams and L the runner length in mm. Example: a 40 g part fed through a 100 mm branch gives D = 6.325 × 3.162 / 3.7 = 5.41 mm. Then check that D is at least the thickest wall plus 1.5 mm and inside the typical range for the resin, and round up to a standard cutter, here 6 mm.
What are the limits of the runner diameter formula D = √W × L^0.25 / 3.7?
It is usually quoted as valid for parts up to about 200 g with walls up to about 3 mm, and for easy-flowing resins such as ABS and polystyrene. It works only in its own units: grams, millimetres and a result in millimetres. Outside that range, size the runner from the wall-thickness rule and the resin's typical range, and confirm with a flow simulation.
How much bigger should the runner be than the part wall?
A common rule from Menges, Michaeli and Mohren is that a runner should be at least the thickest wall of the part plus 1.5 mm. The runner must stay molten longer than the part so the part can be packed through it. A runner thinner than the wall freezes first and cuts off packing, which shows up as sink, voids and short weight.
How do you size the primary runner when it splits into branches?
Use the cube law: D upstream = D branch × ∛N, where N is the number of branches the upstream runner splits into. For a Newtonian melt the wall shear rate is 32Q / (πD³), so this keeps the shear rate the same on both sides of the split. A 6 mm branch fed by a two-way split needs a primary of 6 × 1.26 = 7.56 mm, rounded up to 8 mm.
Why are full-round runners preferred?
For a given flow area a circle has the smallest perimeter, so a full-round runner loses the least heat to the mold and has the smallest frozen skin. A half-round runner of the same area has about 16 percent more perimeter, and a square about 13 percent more. Full-round runners need matching halves cut in both mold plates; when only one plate can be machined, a trapezoid deep enough to contain the calculated circle is the usual alternative.
Can a runner be too big?
Yes. Freeze time grows with the square of diameter, so an oversized runner can become the slowest-cooling feature in the mold and set the cycle time. It also adds regrind or scrap to every shot and needs more shot capacity. Size it as small as the formula and the wall rule allow, and when the runner becomes a large share of the shot, consider a hot runner or a hot sprue.
Ask JCH about your runner
Not sure whether your layout is balanced, or whether a hot runner would pay off in plastic and cycle time? Ask our AI assistant. It answers from this website, and our tooling team follows up if you want.
AI assistant. Answers can be wrong; nothing it says is a quote or a promise.
This calculator gives an engineering estimate. Our tooling team reviews your part, resin, cavity count and volume, and recommends the layout, runner, gates and whether a hot runner makes sense.