Material Yield & Scrap Calculator
Plan the resin for a molding order as a mass balance: buy enough virgin material to cover the weight of the good parts, the cold runner on every shot, the parts that will be rejected, and the startup and purge material, then subtract only the regrind your specification lets back into the hopper. Enter seven numbers and the calculator returns kilograms (and pounds) of virgin resin to order, plus three yield figures that show where the material went.

Engineering estimate, not a quote. Use it to size a resin order and to see which loss is largest; a trial run and the molder's own scrap history replace these inputs once the tool exists.
How this works
Every gram that goes into the hopper leaves the press in one of four forms: a part someone accepts, a runner and sprue, a part someone rejects, or startup and purge material. Plastics Technology's quoting series by Jim Fattori puts the problem plainly: "No one molds perfect parts on the first shot," and "Generating scrap is inevitable" (Fattori, Plastics Technology). The calculator does not guess a single padding factor. It counts each stream separately, so the answer shows which one is eating the material.
Step 1, from good parts to parts molded. A reject rate is a share of what you mold, so the number of parts to run is the order divided by the fraction that survives. Infor's documentation for its LN manufacturing software writes the same idea as "Gross requirements = net quantity / (yield/100%)" and defines yield as output divided by input (Infor LN, Yield). Treating your reject rate as that yield is our reading.
Step 2, from parts to shots and shot weight. Divide the parts to mold by the cavities and round up, because a press cannot make part of a shot. Each shot weighs the cavities times the part weight plus the runner and sprue. Shots times shot weight is the molding feed.
Step 3, add the startup and purge material. Infor separates a percentage scrap factor from a fixed scrap quantity, and says the fixed quantity "is mostly used for start-up effects," where the first products off a machine are discarded (Infor LN, Scrap). Molding works the same way: startup and purge depend on how many times the job is set up and how many color changes it sees, not on the order size, so the tool takes them as kilograms for the order rather than as a percentage.
Step 4, take back only the regrind the spec allows. Runners and rejected parts can be ground and fed back, but only up to the regrind share written for the part. The tool returns whichever is smaller: the runner-and-reject mass the job generates, or the allowance times the molding feed. Whatever exceeds that limit leaves the loop as scrap for another product, a recycler or the bin. Applying the allowance to the production feed, and assuming the loop runs at the set ratio for the whole order, are our reading.
Why rejects divide and do not multiply
Many spreadsheets add a reject allowance by multiplying the order by one plus the reject rate. Infor uses that multiplying form for a scrap factor, "Gross requirements = (scrap factor/100% + 1) x net quantity," and the dividing form for a yield. The two agree only when the percentage is defined the way the formula expects. If 10% of what you mold fails inspection, molding 110% of the order leaves you short: 1,100 molded parts at a 10% reject rate yield 990 good ones. Dividing by 0.90 asks for 1,111.1, which rounds up to 1,112. The gap grows quickly as the reject rate climbs, which is what the next figure shows.
Worked examples, by hand
Each case has a button beside the form that fills in its inputs. Case 1 reproduces the 64-cavity tool Husky publishes in its hot runner fundamentals article, with parts of 2 g each, a cold runner of 192 g and a shot of 320 g, roughly 129.3 million parts annually; the zero reject rate, zero startup scrap and zero regrind are our simplifications, because Husky gives none of them. Case 2 is our own illustrative order. Case 3 reruns Case 1 with a 25% regrind ceiling, the figure Fattori quotes from a UL fabricated-parts standard (see the regrind section below).
Case 1 matches Husky's shot weight exactly and its "about 2 million cycles" to rounding, and it shows how low yield can fall when a heavy cold runner feeds tiny parts: three-fifths of every shot is runner. Case 2 is a more ordinary order, and the cap still binds there: the job generates 182.5 kg of grindable runner and rejects, but a 15% ceiling admits only 162.4 kg, so about 20 kg of clean material has nowhere to go in this part. Case 3 shows that even a generous ceiling recovers less than half of Case 1's runner.
Runner share sets the ceiling on yield
With no rejects and no startup losses, the yield of one shot is simply the part weight over the shot weight. John Thirlwell observed in MoldMaking Technology that, in many cases, a cold runner weighs "up to half the total shot weight," and Fattori notes that "On occasion, the weight of the runner is even more than the weight of the parts." A runner at half the shot caps gross yield at 50% before a single part is rejected. Regrind changes how much virgin you buy, not how much you melt: when the runner share s of the shot is at or below the allowance g, all of it can return and virgin yield reaches 100% in the ideal case; above that, virgin yield is (1 − s) ÷ (1 − g). That expression is our algebra from the formulas above, for the no-reject, no-startup case.
What the regrind allowance really limits
Fattori asks whether the request for quotation states the allowable regrind or says "virgin only," and quotes UL Standard 746D: "Parts shall not be molded from material that contains more than 25% thermoplastic regrind by weight, that has been dry blended by the molder with the same grade of virgin material, unless the results of a separate investigation indicate acceptable performance for the specific part." That clause is the source of the 25% in Case 3; the binding ceiling for your part is whatever its drawing, its customer or its own listing says. Thirlwell adds that "in many medical and food applications" the runners cannot be reused at all, which is the g = 0 line in Figure 3. Fattori goes on to say that he and many colleagues prefer either 0% or 100% regrind and nothing in between; this calculator models the in-between case because so many specifications are written that way, and the regrind percentage calculator covers what a steady ratio does to the melt over repeated passes.
When the cap binds, the surplus still has somewhere to go. Husky describes cold runners as "a costly waste of resin" that processors throw away, regrind "for use in other processes" or sell as bulk scrap. For a runner heavier than its parts, Fattori writes: "The best you can hope for is to be able to use the regrind in a different part." Neither route lowers the virgin resin this order needs, which is why the result panel lists the surplus separately.
Startup, purge and the other fixed losses
Startup scrap does not scale with the order. Fattori notes that a dark-to-light color change "can take a lot of time and material," particularly in a large machine, and that purging compound adds to it. Jason Robinson of RJG and David Hoffman of the AIM Institute, interviewed by Plastics Machinery & Manufacturing, add more. Robinson recommends sequencing changeovers from light to dark, because, in his words, going from dark to light "takes a considerable amount of purging or cleaning." The article reports that an efficient startup saves material otherwise lost to a poorly executed one, and Robinson points out that a cold-runner mold with blocked cavities still produces scrap plastic. He also says that letting the hold phase run too long, past what a gate-freeze study shows, can let the runner fill more heavily and create more waste. Count every setup on the order when you fill in the startup box; a run split into three releases has three startups.
Picking a reject rate when you have no history
Fattori's guidance is candid: the scrap factor for flower pots "will be very low," for medical, automotive or optical parts it "could be very high," and choosing the figure usually comes down to experience. Manuel Riano, writing on regrind tracking in Plastics Technology, advises: "Use a fixed percentage when estimating scrap." This page prints no default reject rate as fact. The 3% in Case 2 is an illustrative input, not a typical value; ask the molder for its rate on similar parts, or run the tool at two or three rates and buy for the worst one you can defend.
Common mistakes
- Multiplying by (1 + reject rate). If the rate is a share of parts molded, divide by (1 − rate). Figure 1 shows the shortfall.
- Using part weight times quantity as the order. That is the gross-yield numerator, not the resin requirement. In Case 1 it is only 40% of what the press melts.
- Crediting the whole runner as regrind. The allowance caps it. In Case 2 roughly 20 kg of clean runner and rejects exceed the 15% ceiling.
- Grinding wet or mixed material. Fattori notes that hygroscopic resin molded without proper drying is usually unusable, ABS being his stated exception, and that unmarked regrind of two black resins cannot be told apart by eye. Riano's tagging of regrind into Green, Yellow and Red quality classes is one way to keep the wrong material out of the mix.
- Scaling startup scrap with the order. It follows setups and color changes, so enter it as a fixed amount.
- Forgetting that regrind arrives late. The first shots of a run have no regrind to use yet. On a short order this can push the real virgin figure above the tool's estimate.
Where this calculator fits
| Approach | Use it for | Limits |
|---|---|---|
| This calculator | Sizing a resin order before a run; seeing which loss dominates; comparing a cold tool, a smaller runner or a different regrind ceiling | Assumes a constant reject rate and a loop that runs at the set ratio; startup is one lump |
| A flat padding percentage | Quick quotes where material is a small share of the job | Hides which stream is large; Fattori calls the figure a judgment call |
| The molder's scrap history by part family | Repeat orders and tools that already run | Not available for a new tool or a new resin |
| ERP material planning with yield and fixed scrap | Ongoing production, multi-step routings | Only as good as the yields entered; Infor's own example shows three 90% steps compounding to 72.9% |
Sources (all retrieved November 20, 2026)
- "No one molds perfect parts on the first shot"; scrap factor low for flower pots and possibly very high for medical, automotive or optical parts, a judgment call; RFQ regrind allowance or virgin only; UL Standard 746D 25% clause as quoted; 0% or 100% regrind preference; runner weight sometimes above part weight; using surplus regrind in a different part; wet hygroscopic material unusable except ABS; unmarked regrind mix-ups; startup, color-change and purge material: Jim Fattori, Get Better at Quoting Injection Molded Parts: Part 2, Plastics Technology (December 17, 2020).
- Yield = output ÷ input × 100%; gross requirements = net quantity ÷ (yield/100%); three 90% operations give 72.9%: Infor LN 10.8 Job Shop Control, Yield.
- Scrap factor gross requirements = (scrap factor/100% + 1) × net quantity; fixed scrap quantity mostly for start-up effects: Infor LN 10.8 Job Shop Control, Scrap.
- The 64-cavity cold-runner example (roughly 2 million cycles; 129.3 million parts annually; parts of 2 g each; runner 192 g; shot 320 g); cold runners thrown away, reground for other processes or sold as scrap: Husky, Hot Runner Fundamentals (October 8, 2021).
- Cold runner weight reaching half of the whole shot in many cases; runners often barred from reuse in medical and food work: Seven Key Advantages of Hot Runner Systems, by John Thirlwell, in MoldMaking Technology, April 1, 2002.
- Fixed percentage for scrap estimates; Green, Yellow and Red regrind classes: Manuel Riano, Why and How You Should Be Tracking Your Regrind, Plastics Technology (March 12, 2020).
- Startup waste, blocked cavities on cold runners, hold time and runner packing: Bruce Geiselman, How to Use Less Plastic in Injection Molding, Plastics Machinery & Manufacturing (October 10, 2022).
- Pound (avoirdupois) to kilogram, 4.535 924 E−01: NIST SP 811, Appendix B.9.
Reviewed by the JCH tooling team · updated November 2026.
Resin quantity and yield questions
How much extra resin should I order beyond part weight times quantity?
There is no honest single percentage. Add up four things instead: the runner and sprue on each shot, the parts you expect to throw away, the purge and warm-up material for each setup, and then credit back only the regrind your drawing permits. A light part on a heavy cold runner can need more than twice its own net weight, while a tool with no cold runner and very few rejects needs little beyond what the parts weigh.
What is the difference between gross yield and virgin yield?
Gross yield compares the weight of accepted parts with everything the barrel melted, regrind included, so it measures how efficiently the press turns plastic into product. Virgin yield compares the same part weight with only the new pellets purchased. Reusing runners lifts virgin yield but leaves gross yield untouched, because ground material still gets melted, still costs machine time and still has to pass through the mold again.
Does a hot runner make material yield 100 percent?
No. Removing the cold runner takes that whole stream out of the sum, but rejected parts, warm-up shots and purge after a color change still happen. Enter zero for runner weight and keep realistic figures for the other inputs to see what remains. On small orders with several setups, the fixed startup amount can then become the largest loss.
Should runner regrind count toward my order quantity?
Only up to the ceiling on the drawing. Material above that ceiling is real plastic you paid for, but this part cannot use it, so it reduces nothing on this purchase order. It may still have value in a lower-grade product or with a recycler, which is a separate decision from how many bags to buy now.
How do I estimate startup and purge scrap for a new tool?
Ask the molder how many kilograms its purge routine and warm-up shots normally consume on a press of the size it plans to use, then multiply by the number of setups and color changes in your release schedule. Without that answer, run the calculator with two or three plausible amounts and note how much the virgin figure moves. Because the amount is fixed, its share shrinks as the order grows.
Why does the calculator round up to whole shots?
A press cycle fills every running cavity at once, so the last cycle of an order produces a full set even if you only needed one more part. What happens to those extra pieces is for you and the molder to agree. On a high-cavitation tool the overrun can reach dozens of parts, though as a share of material it is normally tiny.
Can I use this for parts that are not injection molded?
The bookkeeping carries over to any process where each cycle makes product plus a predictable offcut: blow molding flash, thermoformed skeleton web, or sheet-metal blanks with a carrier strip. Replace the runner box with that offcut weight per cycle. The regrind ceiling and the startup figure then come from that process's own rules, not from molding practice.
Ask JCH about your resin order
Not sure whether your runner is too heavy, or what to enter for rejects on a first run? Type the part, the resin and the numbers you have. Ask JCH is an AI assistant that draws on the pages of this site; after it answers, it offers a box for your email address if you want to stay in touch.
Machine-written replies can contain errors and do not form an offer of any kind.
Planning a first production order?
Send the part file, the resin grade and the quantity, and our tooling team will go through runner size, the regrind ceiling on your drawing and the setups in your release plan, so the resin you buy matches the parts you actually need.
Book a free 30-minute first consultation Send the part and quantities