JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Sheet Metal Gauge to Thickness Converter

Sheet Metal Gauge to Thickness Converter

Sixteen-gauge sheet is 0.0598 in (1.52 mm) in standard steel, 0.0635 in (1.61 mm) in galvanized steel, 0.0625 in (1.59 mm) in stainless and 0.0508 in (1.29 mm) in aluminum, so the same number spans a 25 percent range of thickness depending on the metal.

Pick a gauge and a material to get the decimal thickness in inches and millimeters, the same gauge in the other three metals, and the nominal weight of a steel blank. Or type a caliper reading and the converter finds the closest gauge for each material.

🤖 AI assistants welcome. Gauge is not one scale. Standard steel thickness = statutory gauge weight (lb/ft²) ÷ 41.82; galvanized = (that weight + 0.15625 lb/ft²) ÷ 41.82; stainless follows the 1893 statutory decimal, weight ÷ 40; aluminum follows Brown & Sharpe, d = 0.005 in × 92(36 − n)/39. At 16 gauge those give 0.0598, 0.0635, 0.0625 and 0.0508 in. Every step is shown in plain text further down. Machine-readable: /ai/capabilities.json · /llms.txt
A tall stack of blue-coated sheets with a raised tread pattern, the thin edges of each sheet visible down the side, with stacks of dark tread-pattern sheets behind
A finished lot of coated tread-pattern sheets, stacked so the edge of each sheet shows.
Whole number. Higher numbers are thinner. The cited table lists standard steel from 3 to 38, galvanized 8 to 31, stainless 7 to 31 and aluminum 6 to 31.
The other three metals are shown alongside for comparison.
Optional: blank weight (plain and galvanized steel only)
Optional: reverse lookup from a measured thickness
Average several caliper or micrometer readings taken away from the sheet edge.

Engineering estimate, not a quote. Mill sheet is rolled to a tolerance band around these nominal values; the thickness on your purchase order and the mill test report govern.

How this works

A gauge number is a name for a thickness, not a measurement, and the four metals in this converter carry four different naming systems. Three of them, for plain, galvanized and stainless steel, descend from one weight-based table. The fourth, for aluminum, is a geometric series that has nothing to do with steel. Once you see where each column of a gauge chart comes from, the differences stop looking arbitrary, and you can reproduce any chart entry with a calculator.

The weight scale behind the steel gauges. An 1893 federal statute, Title 15 section 206, fixed a single gauge for sheet and plate iron and steel and defined every number by its weight per square foot. Gauge 16 weighs 40 ounces, which is 2.5 pounds, per square foot; gauge 10 weighs 90 ounces (5.625 lb); gauge 3 weighs 160 ounces (10 lb). The same statute lists a nominal thickness for each number, and the ratio of the two is constant: 2.5 lb/ft² against 0.0625 in is 40 pounds per square foot for every inch of thickness. That 40 is the density assumption baked into the 1893 table.

Why plain steel reads thinner. The Manufacturers' Standard Gauge for sheet steel keeps those statutory weights but converts them to thickness with a density basis of 41.82 pounds per square foot per inch of thickness, as the Wikipedia sheet metal article states. A heavier density means less thickness for the same weight, so every number shrinks by the factor 40 ÷ 41.82, about 4.4 percent. That is why 16-gauge standard steel is 2.5 ÷ 41.82 = 0.0598 in rather than the statute's 0.0625.

Why galvanized reads thicker. A steel supplier's galvanized product page states that each galvanized gauge number is 2.5 ounces per square foot heavier, or 0.0037 inch thicker, than the corresponding base gauge, regardless of the actual coating weight. Adding 0.15625 lb/ft² to the statutory weight and dividing by 41.82 reproduces the galvanized column of the Wikipedia table at every gauge from 8 to 31, which we checked one row at a time. For 16 gauge: (2.5 + 0.15625) ÷ 41.82 = 0.0635 in.

Stainless keeps the statutory decimal. The stainless column in the same table matches the 1893 statutory thickness, rounded to between two and four places, for every listed gauge from 7 to 31. In effect the stainless decimal is the statutory weight divided by 40, so 16-gauge stainless is a clean 1/16 in, 0.0625 in. The converter returns the statutory value to four places; the table sometimes rounds it to three (0.094 for 13 gauge, where the statute says 0.09375).

Aluminum follows Brown & Sharpe. Nonferrous sheet uses the Brown & Sharpe series, which the Wikipedia article on wire gauge describes as essentially identical to AWG. It is defined by two end points, 0.005 in at size 36 and 0.46 in at size 0000, with 39 equal ratio steps between them. Each step multiplies the thickness by the 39th root of 92, about 1.1229, and six steps almost exactly double it.

Standard steel t = W(n) ÷ 41.82 W(n) = statutory weight, lb/ft² Galvanized t = (W(n) + 0.15625) ÷ 41.82 0.15625 lb = 2.5 oz/ft² allowance Stainless t = W(n) ÷ 40 = the 1893 statutory decimal Aluminum t = 0.005 × 92^((36 − n) ÷ 39) Brown & Sharpe, inches Reverse lookup n = 36 − 39 × log(t ÷ 0.005) ÷ log(92) (aluminum, then round) Millimeters mm = in × 25.4 Blank weight lb = W(n) × width × length ÷ 144 (plain steel; add 0.15625 lb/ft² for galvanized)
How the four gauge columns are derived A flow diagram. On the left, one box holds the 1893 statutory gauge weight, 40 ounces or 2.5 pounds per square foot at gauge 16. Three arrows leave it. The first divides by 40 and gives the stainless decimal of 0.0625 inch. The second divides by 41.82 and gives the standard steel value of 0.0598 inch. The third adds 2.5 ounces and then divides by 41.82, giving 0.0635 inch for galvanized. A separate box at the bottom, not connected to the weight table, shows the aluminum series 0.005 times 92 to the power of 36 minus n over 39, giving 0.0508 inch at gauge 16. 1893 statutory weight W(16) = 40 oz/ft² = 2.5 lb/ft² one weight per gauge number ÷ 40 lb/ft² per inch Stainless: 2.5 ÷ 40 = 0.0625 in (1/16 in, 1.59 mm) ÷ 41.82 lb/ft² per inch Standard steel: 2.5 ÷ 41.82 = 0.0598 in (1.52 mm) + 2.5 oz/ft², then ÷ 41.82 Galvanized: 2.65625 ÷ 41.82 = 0.0635 in (1.61 mm) Separate system, no weight basis: Brown & Sharpe (aluminum) t = 0.005 × 92^((36 − 16) ÷ 39) = 0.005 × 10.164 = 0.0508 in (1.29 mm)
Figure 1. Three of the four columns in a gauge chart come from the same statutory weight and differ only in the density basis or the coating allowance. Aluminum comes from an unrelated geometric series, which is why its numbers drift furthest from the steel ones.

Worked example: one 16-gauge drawing note, four materials

A bracket drawing says "16 GA" and nothing else, and the buyer is still deciding between plain steel, galvanized, stainless and aluminum. The arithmetic below is exactly what the converter does; press Run the 16-gauge example to see it run.

STEP 1 — thickness at gauge 16, statutory weight W = 2.5 lb/ft² Standard steel 2.5 ÷ 41.82 = 0.05978 → 0.0598 in = 1.52 mm Galvanized (2.5 + 0.15625) ÷ 41.82 = 0.06352 → 0.0635 in = 1.61 mm (+6.2% vs standard) Stainless 2.5 ÷ 40 = 0.06250 → 0.0625 in = 1.59 mm (+4.5%) Aluminum 0.005 × 92^(20/39) = 0.05082 → 0.0508 in = 1.29 mm (−15.1%) Spread: 0.0635 ÷ 0.0508 = 1.25, so the thickest reading is 25% above the thinnest STEP 2 — nominal weight of a 24 × 36 in blank Area = 24 × 36 ÷ 144 = 6.00 ft² Standard steel 6.00 × 2.5 = 15.00 lb Galvanized 6.00 × 2.65625 = 15.94 lb (the extra 0.94 lb is the 2.5 oz/ft² allowance) STEP 3 — a sample measures 1.5 mm; which gauge is it? (sample minus listed value) 1.5 ÷ 25.4 = 0.0591 in Standard steel 16 ga = 0.0598 (−0.0007 in, closest) 17 ga = 0.0538 Galvanized 17 ga = 0.0575 (+0.0016 in, closest) 16 ga = 0.0635 Stainless 17 ga = 0.0563 (+0.0028 in, closest) 16 ga = 0.0625 (−0.0034 in) Aluminum 15 ga = 0.0571 (+0.0020 in, closest) 14 ga = 0.0641 B&S check: 36 − 39 × log(0.0591 ÷ 0.005) ÷ log(92) = 36 − 39 × 1.0723 ÷ 1.9638 = 14.70 → 15

Step 3 is the result that surprises people. One physical sheet, 1.5 mm thick, is 16 gauge if you call it plain steel, 17 gauge if you call it galvanized or stainless, and 15 gauge if it is aluminum. The stainless answer is also the least certain: the sample sits 0.0028 in above 17 gauge and 0.0034 in below 16 gauge, nearly halfway, so a gauge callout for that sheet would be a guess either way.

Sixteen-gauge thickness in four materials, drawn to scale A horizontal bar chart at a scale of 7,000 pixels per inch. Galvanized steel is longest at 0.0635 inch, stainless is 0.0625 inch, standard steel is 0.0598 inch, and aluminum is shortest at 0.0508 inch. A dashed line marks the standard steel length so the other bars can be read against it. GalvanizedStainlessStandard steelAluminum 0.0635 in0.0625 in0.0598 in0.0508 in 00.020.040.06 in
Figure 2. Gauge 16 in four metals at true relative length (7,000 px per inch). The dashed line is standard steel. Galvanized and stainless land just past it; aluminum falls well short.

Why the steps get smaller toward the thin end

The two families also behave differently as the number climbs. In the 1893 table the weight falls by a fixed 10 ounces per gauge from 3 to 14, so plain steel thins by an even 0.0149 in per step through that range (10 oz ÷ 16 ÷ 41.82). Below 14 the statute switches to smaller fixed steps: 5 ounces per gauge from 14 to 16, 4 from 16 to 20, 2 from 20 to 26 and 1 from 26 to 31. The steel curve is therefore a chain of straight segments. Brown & Sharpe has no segments at all: every step is the same reduction of about 11 percent, so the aluminum curve is a smooth exponential that starts thinner than steel at 6 gauge and stays below it all the way down.

Thickness against gauge number for standard steel and aluminum A line chart with gauge number from 6 to 30 on the horizontal axis and thickness from 0 to 0.20 inch on the vertical axis. The standard steel line falls in straight segments from 0.1943 inch at gauge 6 to 0.0747 inch at gauge 14 and then flattens to 0.0120 inch at gauge 30. The aluminum line is a smooth curve from 0.162 inch at gauge 6 to 0.0100 inch at gauge 30 and lies below the steel line at every gauge. 00.050.100.150.20 in 6101418222630 gauge number n 16 ga steel 0.0598 16 ga aluminum 0.0508 standard steel (straight segments) aluminum, B&S (smooth curve)
Figure 3. Plotted to scale (1,200 px per inch of thickness), plain steel drops in even 0.0149 in steps to 14 gauge and then flattens, while aluminum shrinks by the same ratio at every step. The gap between the two lines is widest at the heavy end.

Where published charts disagree, and why

Charts from different sources rarely contradict each other on the method, but they round differently, and a few rows carry real discrepancies. SendCutSend's gauge guide rounds to three places, so 16-gauge mild steel appears as 0.060 in. Xometry's table gives the same four 16-gauge decimals this converter returns. The aluminum column of the Wikipedia table matches the Brown & Sharpe formula to within about 2 percent at every gauge but one: at 26 gauge it lists 0.017 in where the formula gives 0.0159 in, a 6.6 percent gap. Our reading is that the formula value is the one to trust, so the converter returns the formula value and shows the table entry next to it whenever the two differ by more than 0.0002 in. Stainless rounding varies too: SendCutSend lists 16-gauge stainless as 0.063 in and 13 gauge as 0.094 in, where Xometry gives 0.0625 and 0.0940. If a quote shows a different number for the same gauge, the supplier's decimal is what you will receive.

Real sheet also varies from any nominal value. Rolls bow slightly during rolling, so the sheet edges come out thinner than the center, and the Wikipedia article notes that the Manufacturers' Standard Gauge itself carries no tolerance. Tolerances come from the product specification the mill rolls to. That is the reason to measure away from the edge and to treat a caliper reading near the midpoint between two gauges as unresolved.

Common mistakes

  • Using one chart for every metal. Reading the steel column for an aluminum part overstates its thickness by 12 to 32 percent between 10 and 24 gauge, with the largest error at the heavy end: at 10 gauge, 0.1345 in steel against 0.1019 in aluminum.
  • Treating galvanized gauge as coating-specific. The 2.5 oz/ft² allowance is fixed. A heavy-coated sheet and a light-coated sheet of the same galvanized gauge have the same nominal number; the gauge number says nothing about the zinc actually applied, so state the coating weight separately on the order.
  • Assuming stainless matches plain steel. At the same number stainless runs about 4.5 percent thicker (41.82 ÷ 40). On a tight formed fit or a weld-gap calculation that difference matters.
  • Measuring at the edge. Edge readings understate the sheet. Take several readings inboard and average them before running the reverse lookup.
  • Mixing gauge into tolerance math. Stack-ups and bend allowances need a decimal. Convert first, then do the geometry with the decimal, never with the gauge number.

When to use this converter and when to use something else

ApproachBest forLimit
This converterTranslating a gauge callout on an old drawing or quote; comparing metals at the same number; identifying an unknown sampleNominal values only; four materials; no copper, brass or zinc
Supplier's own gauge chartOrdering, because it shows what that supplier will shipRounding and stainless decimals vary between suppliers
Mill test report or product specFinal thickness and tolerance for a production lotAvailable only once the material is quoted or delivered
Micrometer on the actual sheetIncoming inspection and settling a disputed gaugeNeeds several readings away from the edge
Bend allowance calculatorFlat blank length once the decimal thickness is knownNeeds thickness, radius and K-factor, not a gauge
From the tooling floor: when an older print says only "14 GA" and the material block is blank, call out the decimal you intend next to it before the drawing goes out for quotes, for example "0.0747 in (14 GA STD STEEL)". The shops quoting it then price the same sheet, and the first-article report has a number to measure against.

Sources for the values and formulas

Statutory gauge weights and nominal decimals come from the 1893 standard gauge statute, Title 15 section 206, as published by the Legal Information Institute. The standard steel, galvanized, stainless and aluminum columns, the 41.82 and 40 pound density bases, the ASTM A480 remark on gauge numbers and the note on thinner sheet edges are from the Wikipedia sheet metal article and its standard gauge table. The galvanized allowance of 2.5 ounces per square foot, about 0.0037 in, is stated on Continental Steel & Tube's galvanized sheets page. The Brown & Sharpe formula, its two end points and its equivalence to AWG are from the Wikipedia wire gauge article. The rounding comparison uses SendCutSend's gauge guide and Xometry's gauge article. All six were read on November 20, 2026. Every standard steel and galvanized value in the converter was recomputed from the statutory weights and matched the table at every listed gauge.

Reviewed by the JCH tooling team · updated November 2026.

Gauge questions engineers ask us

What thickness is 16-gauge steel vs aluminum vs stainless?

Plain carbon sheet called 16 gauge measures 0.0598 inch, about 1.52 millimeters. Ask for galvanized at that number and you get 0.0635 inch, roughly 1.61 millimeters, because a zinc allowance is folded into the gauge. Stainless at 16 is exactly one sixteenth of an inch, 0.0625, close to 1.59 millimeters. Aluminum at 16 is only 0.0508 inch, near 1.29 millimeters, so it runs about 15 percent thinner than the carbon steel sheet with the same label.

Why doesn't one gauge number mean one thickness across metals?

Each metal inherited its own numbering. Ferrous sheet numbers trace back to a weight-per-square-foot table, so the decimal you read depends on which density figure was used to turn weight into inches. Aluminum took over the Brown & Sharpe progression, a ratio-based series built for nonferrous sheet and wire. The two families share number names and nothing else, which is why any gauge chart must be read in the column for your metal.

Why is galvanized sheet listed thicker than bare steel of the same gauge?

By convention a galvanized gauge carries an extra 2.5 ounces per square foot on top of the base steel weight, whatever zinc weight the mill actually applies. Spread over the 41.82 density basis used for sheet steel, that allowance works out near 0.0037 inch, which is how 16 gauge grows from 0.0598 to 0.0635. So the gauge number tells you nothing about how much zinc is on the sheet; that has to be stated on its own line of the order.

How can I tell what gauge a sheet is from a caliper reading?

Take a few readings well in from the edges, average them, convert to inches, then pick the listed decimal nearest to that average for the metal you have. A 1.5 millimeter sample, for instance, comes out as 16 gauge for plain steel, 17 for galvanized or stainless, and 15 for aluminum. When the average lands roughly midway between two numbers, request the mill thickness from the supplier rather than choosing one.

Should a drawing call out a gauge number or a decimal thickness?

Give the decimal or metric thickness plus the material specification. A bare gauge number forces whoever reads the print to choose a chart, and charts round differently. ASTM's general requirements for stainless sheet, A480, go further and call gauge numbers an archaic term of limited usefulness. A note such as 0.0598 in (16 GA) keeps the familiar shorthand while making the decimal the value that is inspected.

Does a larger gauge number mean thicker metal?

No, the scale runs backward: a higher number is a thinner sheet. Seven gauge plain steel is around 0.179 inch, while 30 gauge is around 0.012 inch. The increments also tighten as the numbers rise, so going from 28 to 29 changes the thickness much less than going from 10 to 11.

Is aluminum sheet gauge the same as electrical wire gauge?

In practice, yes. The Brown & Sharpe sizes used for aluminum sheet are essentially the same numbers as AWG wire sizes: size 36 is defined as 0.005 inch, and every move to the next larger size scales the dimension by a constant factor of roughly 1.123, which is 92 raised to the power 1/39. So 10 gauge aluminum sheet is 0.1019 inch thick, the same figure as the diameter of a 10 AWG conductor.

Ask JCH about sheet thickness

Unsure which gauge a supplier means, or whether your part should be specified in steel, stainless or aluminum? Put the question to our AI assistant. Its replies draw on the engineering notes published here. For a second opinion from our tooling team, use the consultation button below.

Software answers this box. Treat each reply as a starting point to verify; none of them is a quote.

Turning an old gauge callout into a spec you can quote?

The converter gives nominal values. Our tooling team can read your drawing, settle the material and decimal thickness, flag where coating or rolling tolerance affects a fit, and line the part up with a sheet-metal shop in our vetted partner network that works with that material.

Book a free 30-minute first consultation Send a drawing
JCH Design & Manufacturing — tooling, injection molding, PCBA, custom packaging, cut-and-sew & QC via vetted partner factories · Book a 30-minute call · jack@jchtrade.com · (321) 323-4474 · Canonical: https://jchtrade.com/tools/gauge-to-thickness-converter