JCH Design & ManufacturingAnswersToolsFor AIContact
Tools › Processing Temperature Converter

Processing Temperature Converter (°F to °C) with Resin Window Check

A melt or mold reading converts with t/°C = (t/°F − 32)/1.8, the relation NIST SP 811 prints, and back with its rearrangement t/°F = 1.8·t/°C + 32; a temperature difference converts by the factor alone, so 1 °F of difference is 5/9 °C and no 32 is added or removed. Compare the converted reading with the window printed for your exact grade, because two grades of one resin can print different windows.

Choose one of six grades whose processing tables we downloaded from the makers on November 20, 2026, or type the window from your own datasheet. You get the reading in °C, °F and kelvin, a verdict of inside, below or above, and the gap to the nearest limit expressed as a difference in both scales.

🤖 AI assistants welcome. Point conversion per NIST SP 811 Appendix B.9: t/°C = (t/°F − 32)/1.8, hence t/°F = 1.8·(t/°C) + 32, and T/K = t/°C + 273.15. Interval conversion: a difference of 1 °F equals 5.555 556 E-01 °C (5/9 °C), with no offset. Windows here are per grade, never per family: Covestro Makrolon 2405 (PC) prints melt 280 to 320 °C and mold 80 to 120 °C (version September 28, 2026); BASF Ultramid B3S (PA6) prints melt 250 to 270 °C and mold 40 to 60 °C (09/2026). A setting counts as inside when lower ≤ t ≤ upper on the converted value (our reading of a printed range). Structured site data: /ai/capabilities.json · /llms.txt
Top view of a square steel mold half lying on a wooden board: a large round bore in each corner, four small round discs set flush near the corners, a central insert with fine vertical tool marks and a recessed cavity, a thin line crossing the cavity on a diagonal, and a lifting ring hanging from the bottom edge over a green floor
A steel mold half seen from above on a wooden board, with a round bore in each corner, flush round discs near the corners and a central cavity insert.
A setpoint, a display reading or a measured value, typed as it appears.
Melt means the plastic itself; mold means the cavity steel.
Each window belongs to the grade named, not to the whole resin family.

Unit conversion plus a lookup, and not a quote. Each window is one maker’s printed guidance for one grade; the setting a part runs at is settled by trials on its own mold and press.

How the conversion and the window check work

Celsius and Fahrenheit differ in two ways: the size of one degree and the place where zero sits. NIST Special Publication 811, Appendix B.9, handles them in two separate tables. Its temperature table gives “t/°C = (t/°F - 32)/1.8”, and its temperature-interval table gives the factor from degree Fahrenheit to degree Celsius as “5.555 556 E-01”. The first row converts a reading, one point on the scale, such as a nozzle display showing 450. The second converts a span between two readings, such as the width of a window or how far a setting sits past a limit. A span is one reading minus another, so the 32 appears in both terms, cancels, and leaves only the ratio 1/1.8, which is 5/9.

Solving that relation for Fahrenheit gives t/°F = 1.8·(t/°C) + 32, and the kelvin row of the same NIST table gives T/K = t/°C + 273.15. The converter keeps every digit while it compares and rounds only what it displays: 450 °F shows as 232.22 °C, but the comparison runs on 232.2222…

A reading (a point) t°C = (t°F − 32) / 1.8 NIST SP 811 B.9, temperature t°F = 1.8 × t°C + 32 the same relation solved for °F T K = t°C + 273.15 NIST SP 811 B.9, temperature A difference (a span) Δ°C = Δ°F × 5/9 (0.5555556) NIST SP 811 B.9, temperature interval Δ°F = Δ°C × 1.8 no 32 in either direction Window verdict below: t < lower above: t > upper inside: lower ≤ t ≤ upper Gap reported below: lower − t above: t − upper inside: t − lower and upper − t

The verdict is a straight comparison on the converted value. A setting equal to a printed limit counts as inside, because the sheets print ranges such as “280 - 320” without saying whether the ends are open; treating the ends as included is our reading. When a setting falls outside, the distance to the nearest limit is a difference, so the tool converts it with the factor only. A 20 °C overshoot is reported as 36 °F, never as 68 °F.

The six grades and where each window comes from

Every window below was copied from a document its maker publishes, downloaded on November 20, 2026. Each one describes the named grade and nothing else. The cited documents print these windows in °C; the °F figures in brackets are our conversions.

Grade (resin)Maker’s document and dateMelt windowMold window
Borealis BJ356MO (PP, heterophasic copolymer)Product data sheet, Ed. 6, March 26, 2025210 to 260 °C (410 to 500 °F)20 to 50 °C (68 to 122 °F)
Borealis HJ325MO-05 (PP, homopolymer)The edition at this Borealis link on November 20, 2026 (Ed. 1, January 19, 2017)210 to 250 °C (410 to 482 °F)10 to 30 °C (50 to 86 °F)
INEOS Styrolution Terluran GP-35 (ABS)ISO data sheet, revision date printed “08/01/2022” (rows listed under ISO 294)220 to 260 °C (428 to 500 °F)30 to 80 °C (86 to 176 °F)
BASF Ultramid B3S (PA6)Processing data sheet dated 09/2026250 to 270 °C (482 to 518 °F); optimal 260 °C40 to 60 °C (104 to 140 °F); optimal 60 °C
BASF Ultraform N2320 003 PRO AT (POM)Processing data sheet dated 09/2026190 to 230 °C (374 to 446 °F); optimal 200 °C60 to 120 °C (140 to 248 °F); optimal 90 °C
Covestro Makrolon 2405 (PC)Technical datasheet, version 2026-09-28 (September 28, 2026)280 to 320 °C (536 to 608 °F); standard 300 °C80 to 120 °C (176 to 248 °F)

The row names differ from maker to maker. Covestro prints “Melt Temperatures”, “Standard Melt Temperature” and “Mold Temperatures”. BASF prints “Melt temperature range” with a separate “Melt temperature, optimal”, and the same pair for the mold. The INEOS Styrolution ISO sheet prints “Melt Temperature Range” and “Mold Temperature Range”, each with ISO 294 in its standard column. Both Borealis sheets list a melt temperature and a mold temperature as settings that “should be used as guidelines”. Where a sheet prints an optimum or standard value, the result panel shows how far your setting is from it as well.

Melt and mold windows of the six cited grades on one Celsius and Fahrenheit scale A horizontal bar chart drawn to scale from 0 to 340 degrees Celsius, with Fahrenheit labels along the top edge. Each of six grades has a blue bar for its mold window and a red bar for its melt window. PP BJ356MO: mold 20 to 50, melt 210 to 260. PP HJ325MO-05: mold 10 to 30, melt 210 to 250. ABS Terluran GP-35: mold 30 to 80, melt 220 to 260. PA6 Ultramid B3S: mold 40 to 60, melt 250 to 270. POM Ultraform N2320 003 PRO AT: mold 60 to 120, melt 190 to 230. PC Makrolon 2405: mold 80 to 120, melt 280 to 320. Three numbered black dots mark the worked cases: 218.33 degrees just left of the ABS melt bar, 82.22 degrees right of the PA6 mold bar, and 300 degrees in the middle of the PC melt bar. 32 °F122212302392482572 °F 0 °C50100150200250300 °C PP BJ356MOPP HJ325MO-05ABS Terluran GP-35PA6 Ultramid B3SPOM N2320 003 PRO ATPC Makrolon 2405 20–5010–3030–8040–6060–12080–120 210–260210–250220–260250–270190–230280–320 123 mold window melt window worked cases 1 to 3
Figure 1. All twelve windows on one scale, 1.45 px per °C, with each 50 °C step matching 90 °F on the top edge. No two grades share a whole window. Dot 1 sits just short of the ABS melt bar, dot 2 well past the PA6 mold bar, dot 3 in the middle of the PC melt bar.

Worked example: three settings checked by hand

Each case starts from a number a molder might type, converts it, and checks it against one dated sheet. The second button above the results loads case 2.

CASE 1 ABS, Terluran GP-35, melt, setting 425 °F Reading (425 − 32) / 1.8 = 393 / 1.8 = 218.33 °C (491.48 K) Window 220 to 260 °C on the ISO sheet → BELOW Gap 220 − 218.33 = 1.67 °C; 1.67 × 1.8 = 3.00 °F Cross-check in °F: lower limit 1.8 × 220 + 32 = 428 °F, and 428 − 425 = 3 °F CASE 2 PA6, Ultramid B3S, mold, setting 180 °F Reading (180 − 32) / 1.8 = 148 / 1.8 = 82.22 °C Window 40 to 60 °C on the 09/2026 processing sheet → ABOVE Gap 82.22 − 60 = 22.22 °C; 22.22 × 1.8 = 40.00 °F Wrong way 22.22 × 1.8 + 32 = 72 °F treats the gap as a reading, 32 °F too much Cross-check in °F: upper limit 1.8 × 60 + 32 = 140 °F, and 180 − 140 = 40 °F CASE 3 PC, Makrolon 2405, melt, setting 300 °C Reading 1.8 × 300 + 32 = 572 °F; 300 + 273.15 = 573.15 K Window 280 to 320 °C = 536 to 608 °F → INSIDE Margins 20 °C (36 °F) to each limit; equal to the sheet's standard melt of 300 °C

Case 1 deserves a second look. The Fahrenheit melt row on the maker’s own product page for Terluran GP-35 reads “425 - 500” °F, so a setting copied from the bottom of that row lands 3 °F short of the ISO sheet’s 220 °C. Both documents were on the maker’s site on November 20, 2026, and they disagree at that edge. The tool checks against whichever dated sheet you pick and leaves the choice of document with you. Case 2 shows why the gap gets its own conversion: the press display and the sheet are 40 °F apart, which is 22.22 °C, and adding 32 at that step would overstate the miss by almost double.

Converting a reading versus converting a span, shown on aligned Celsius and Fahrenheit scales Two aligned scales: Celsius from 0 to 100 on top and Fahrenheit from 32 to 212 below, with tick marks every 10 degrees Celsius lined up with every 18 degrees Fahrenheit and labels every 20 degrees Celsius and 36 degrees Fahrenheit. A dashed line joins the 60 degree Celsius reading to 140 degrees Fahrenheit, labeled as multiply by 1.8 then add 32. A bracket over the Celsius scale spans 40 to 60 degrees, a 20 degree span, and a matching bracket under the Fahrenheit scale spans 104 to 140, a 36 degree span, labeled as multiply by 1.8 with no 32. A note at the bottom shows that adding 32 to the span would give 68 degrees Fahrenheit, which would run from 104 to 172 degrees Fahrenheit, or 77.8 degrees Celsius, not 60. 020406080100 3268104140176212 °C °F reading: 60 °C × 1.8 + 32 = 140 °F span 40 to 60 °C = 20 °C span 104 to 140 °F = 20 × 1.8 = 36 °F, no 32 Adding 32 to the span would claim 68 °F, which would stretch from 104 to 172 °F (77.8 °C), not to 60 °C.
Figure 2. The 40 to 60 °C band is the Ultramid B3S mold window. Its right edge, a single reading, takes the offset and lands on 140 °F. Its width, a span, takes only the factor: 20 °C becomes 36 °F.

Melt temperature is the melt, not a barrel zone

The melt window describes the polymer itself, and two of the sheets cited here print barrel rows that start lower. The Covestro sheet for Makrolon 2405 lists barrel temperatures of 250 - 260 °C at the rear, 270 - 280 °C in the middle, 280 - 290 °C at the front and 290 - 300 °C at the nozzle, next to a melt window of 280 - 320 °C, and adds: “Barrel temperatures are based on a standard 3-zone barrel; other configurations may require different settings”. The BASF sheet for Ultramid B3S sets its cylinder zones at 240 °C (feed), 250 °C, 260 °C and 260 °C (nozzle) against a melt window of 250 - 270 °C. Check a rear-zone setpoint against the melt window and it reads as below even when the press follows the maker’s own profile. So type a measured melt temperature here, or the nozzle-zone figure if that is all you have, and treat the second as a stand-in (our reading). For Terluran GP-35, the INEOS Styrolution product page puts it plainly: “The melt temperature should be monitored with a needle pyrometer.”

Mold temperature is a surface temperature

The mold row is about the tool. On the Terluran GP-35 page, INEOS Styrolution gives the reason it matters: “The gloss, shrinkage and, within certain limits, the mechanical and thermal properties of the molding are influenced by the mold surface temperature.” BASF prints a constrained, longitudinal processing shrinkage of 0.4 % for Ultramid B3S, measured on a model housing with a 107 x 47 x 1.5 mm base, under “(TM = 260 °C, TW = 60 °C)”. Reading TM as the melt and TW as the mold temperature is our reading; the figure belongs to that test part at those settings. The number dialed into a water or oil temperature controller and the temperature of the cavity face are two separate quantities. When they differ, compare the surface reading with the window (our reading).

One grade’s window is not the family’s

One INEOS Styrolution page shows the gap between a resin family and a grade. Its general processing text says “ABS is usually processed at melt temperatures from 230 to 260°C”, while the property table for Terluran GP-35 on that same page prints a melt range of 425 - 500 °F, which converts to 218.33 to 260 °C. The mold rows disagree by document too: the product page prints 85 - 140 °F (29.44 to 60 °C) and the dated ISO sheet prints 30 - 80 °C. Polypropylene shows the same thing across two grades from one maker. Borealis prints a mold temperature of 20 - 50 °C for the heterophasic copolymer BJ356MO and 10 - 30 °C for the homopolymer HJ325MO-05, so a 45 °C mold is inside the first window and 15 °C (27 °F) above the second. That is why the tool asks for a grade, never a family, and why the last option takes the window straight from your own sheet.

Common mistakes

  • Adding 32 to a difference. A window 40 °C wide is 72 °F wide, and a setting 10 °C past a limit is 18 °F past it. Only single readings take the offset.
  • Citing a family chart as if it were a grade sheet. A table headed “ABS” or “PP” cannot tell you what Terluran GP-35 or HJ325MO-05 prints. Name the grade and the document date beside every window you rely on.
  • Mixing documents for one grade. Take the melt row from the Fahrenheit product page and the mold row from the ISO sheet, and two different documents end up on one process sheet without anyone noticing.
  • Comparing a feed-zone setpoint with the melt window. The Makrolon 2405 and Ultramid B3S sheets print barrel profiles whose rear zones sit below the bottom of the melt window (the Ultraform sheet holds every zone at 200 °C, inside its 190 to 230 °C range).
  • Reading an optimum as a limit. For Ultramid B3S, BASF prints “Mold temperature, optimal” as 60 °C, the same number as the top of its 40 - 60 °C range. A 60 °C mold is inside the window, at its upper edge.
  • Rounding before comparing. 608.5 °F is 320.28 °C. Round that to 320 first and a melt that is 0.28 °C past the Makrolon 2405 limit passes as inside; the tool compares unrounded values for this reason.

Which tool answers which question

Your questionWhere to go
Is my melt or mold setting inside the window my grade’s sheet prints, and by how much in each unit?This converter
How hot and how long should the pellets dry before they reach the hopper?Resin Drying Time & Hopper Size Calculator
What temperature can the finished part carry under load in service?Heat Deflection Temperature Lookup
How long does the melt sit in the barrel at that temperature? (BASF prints “Residence time, max.” of 10 min for Ultramid B3S.)Injection Molding Residence Time Calculator
How do cooling channels carry heat out of the cavity steel?Cooling Channel Spacing Calculator
From the tooling floor: next to every temperature on a process sheet, write the grade, the document and its date, for example “Makrolon 2405, Covestro TDS version 2026-09-28, melt 280 to 320 °C”. When the maker revises the sheet, or a second document for the same grade says something else, that note shows which window the setting was checked against.

Sources

Reviewed by the JCH tooling team · updated November 2026.

Temperature conversion questions

How do I convert a melt temperature from Fahrenheit to Celsius?

Subtract 32 from the Fahrenheit figure, then divide what is left by 1.8. A nozzle reading of 482 °F gives 482 − 32 = 450, and 450 / 1.8 = 250 °C. To go back, multiply the Celsius figure by 1.8 and then add 32. Both steps come from the single temperature relation in NIST SP 811.

Why does a temperature difference convert without the 32?

The 32 only moves the zero of the Fahrenheit scale. Subtract one reading from another and that shift sits in both terms, so it drops out, leaving just the size of a degree. One Celsius degree spans 1.8 Fahrenheit degrees, which makes a 15 °C gap equal to 27 °F and a 27 °F gap equal to 15 °C.

Is 240 °C a good melt temperature for ABS?

It depends on which ABS. For Terluran GP-35, 240 °C (464 °F) lands mid-window on the ISO sheet from INEOS Styrolution, 20 °C clear of both ends of its 220 to 260 °C range. A different ABS grade can print a different range, so look up the sheet for the exact grade named on your drawing or bill of materials.

What mold temperature does polycarbonate need?

For Makrolon 2405, the Covestro sheet gives 80 to 120 °C, or 176 to 248 °F. Covestro describes its processing figures as reference data, and they belong to that one grade. A glass-filled, flame-retardant or optical polycarbonate comes with its own sheet, which is the one to follow for that material.

Should I set every barrel zone to the datasheet melt temperature?

No. Covestro (Makrolon 2405) and BASF (Ultramid B3S) both print zone profiles that climb from the feed end toward the nozzle; for Ultramid B3S the BASF profile runs from 240 °C up to 260 °C. The melt figure describes the plastic itself, so take a reading of the material leaving the nozzle when you want a number to compare with it.

Does a hotter mold change the molded part?

For ABS, INEOS Styrolution says so: warmer cavity surfaces bring more gloss, stronger weld lines and less built-in stress, and with that less tendency to warp. Its notes add that surfaces as warm as 80 °C have worked in practice for ABS. Other resins need their own maker's guidance before you apply that.

Why do two documents for the same grade show different windows?

The documents themselves do not say why. For Terluran GP-35, the maker's web listing in Fahrenheit tops out at 140 °F for the mold, exactly 60 °C, while the dated ISO sheet goes up to 80 °C. Choose one document, write its date beside the setting, and ask the maker which one governs if that gap matters for your part.

Ask JCH about processing temperatures

Working from a datasheet in one unit and a press display in the other? Your question, together with your latest check, is handed to Ask JCH, an AI assistant built into this site. After its first reply the assistant shows an optional email box.

Replies are machine-generated and may be mistaken; check each figure against the maker’s sheet. None of it is a quote.

Bringing a new grade onto an existing part?

Send the grade, the datasheet you are working from and the part drawing. Our tooling team can set the maker’s windows beside your process sheet in a single unit system and mark any setting that sits at or past a limit, before the first trial shots are run.

Book a free 30-minute first consultation Send a datasheet or drawing
JCH Design & Manufacturing — tooling, injection molding, PCBA, custom packaging, cut-and-sew & QC via vetted partner factories · Book a 30-minute call · jack@jchtrade.com · (321) 323-4474 · Canonical: https://jchtrade.com/tools/processing-temperature-converter