Answers › UV-resistant plastics

What plastic should I use for outdoor parts that sit in the sun?

Reviewed by the JCH tooling team · Updated

Pick a resin whose chemistry resists UV, then protect it. For opaque parts that means ASA instead of ABS, polypropylene or polyethylene with a HALS package, or any of them in black with fine carbon black. Clear parts need UV-stabilized polycarbonate, often hard-coated. Rank candidates with ASTM G154 or G155 tests, not datasheet claims.

What the sun actually does to a plastic part

Outdoor failure is mostly a chemistry problem, not a strength problem. When a polymer absorbs ultraviolet energy, chemical bonds break and leave behind free radicals. Those radicals react with oxygen and make more radicals, and the chain reaction keeps cutting polymer chains shorter. Shorter chains mean lower molecular weight, and lower molecular weight shows up as fading, chalking, a dull surface, and eventually brittleness. Chemical-additive makers call the whole process photo-oxidation, and it is why a part that passed every drop test on day one can snap in your hand after a few summers.

The damage starts at the surface. The outer skin takes the light, cracks first, and those small surface cracks then act as notches that let an impact or a flex load break the full wall. That's why outdoor parts often look only slightly faded right up to the moment they fail: the surface layer is gone, the core is mostly fine, but the notch is already there.

Cross-section of a molded wall in sunlight: UV breaks bonds in a thin surface layer, a UV absorber soaks up light below the surface, HALS mops up radicals at the surface, and carbon black blocks light at the very top Where UV does its damage in a molded wall sunlight (UV part does the damage) surface layer: bonds break, radicals form, chains shorten bulk of the wall: mostly untouched if the surface is protected wall thickness, e.g. 2.5 mm (not to scale) HALS: traps radicals near the surface and regenerates UV absorber: turns UV into heat before it reaches deeper layers Carbon black (black parts only): screens light at the very surface

Some resins are far more exposed than others because of what is in their backbone. ABS gets its toughness from polybutadiene rubber, and that rubber has carbon-carbon double bonds that react readily with UV and oxygen. ASA swaps the butadiene for an acrylate rubber with a saturated backbone, so the main photo-oxidation route that eats ABS isn't there. Polypropylene is especially sensitive to UV in its natural state. Polycarbonate yellows and loses impact strength outdoors unless it carries a UV absorber.

The three ways to protect a part

1. UV absorbers

A UV absorber soaks up ultraviolet energy and dumps it as a small amount of heat before it can break bonds. Because it works by absorbing light, it protects best through the depth of the wall and is weakest right at the surface, where there is little material in front of the light. In polycarbonate, UV absorbers of the benzotriazole and hydroxyphenyl-triazine classes are the normal route.

2. Hindered amine light stabilizers (HALS)

HALS don't absorb UV at all. They step in after radicals form and trap them, then regenerate and trap more, so a small loading keeps working for a long time. Stabilizer makers usually pair HALS with a UV absorber: the absorber protects the deeper layers, the HALS protects the surface. One catch matters for material choice: most HALS (N-H and N-R types) are basic amines, and in polycarbonate they speed up hydrolysis, so they are not recommended there. Conventional N-H type HALS can also be sensitive to acidic environments; non-basic N-OR types are the usual choice if the part sees agricultural chemicals or acidic cleaners.

3. Pigment, especially carbon black

Carbon black absorbs and screens the damaging wavelengths right at the surface and also slows the oxidation chemistry. For polyethylene, carbon-black makers put the loading for optimum UV protection at about 2 to 2.5%, and they stress particle size: smaller primary particles present more surface to absorb UV, which is why polyethylene pipe standards call for an average primary particle size under 25 nm. Dispersion matters too: clumps of black leave unprotected resin between them, and a poorly dispersed black misses its weathering performance whatever grade it is. It's a big part of why so many outdoor parts are black.

How the usual candidates compare

ResinWeak point outdoorsUsual fixNotes
ABSButadiene rubber reacts with UV and oxygen; color shift and embrittlementSwitch to ASA, cap with ASA, or paintFine for parts that live under a cover or indoors
ASALower heat resistance (HDT about 75 to 95 °C at 1.82 MPa for standard grades)Pick a UV-boosted grade for harsh exposureDistributor data: over 80% impact retained after 2,000 h xenon arc; comparable ABS degrades within 500 to 600 h
PolycarbonateYellows and loses impact strength without protectionUV-stabilized grade (UV absorber, not HALS); hard coat for clear glazingCheck sunscreen, fuel and solvent contact; stress cracking is a separate risk
PolypropyleneEspecially UV-sensitive when unstabilizedHALS package, or carbon black for black partsAsk which HALS and at what loading the grade carries
PolyethyleneEmbrittles without protectionCarbon black at about 2 to 2.5%, or HALSBlack is the most robust option

The ASA hour figures come from xenon-arc testing under ASTM G155, and they are a comparison under one set of lab conditions, not a promise of outdoor years. Use them to rank materials, not to predict service life.

Steel mold plate with a large machined triangular cavity, a lifting eye bolt at the top and cooling-line ports along the side
The finish given to a cavity like this sets the part's starting gloss. Outdoors, a dull, chalky surface is one of the early visible signs of UV damage, which is why gloss retention is worth measuring alongside color change in weathering tests.

Worked example: a black lid versus a gray lid

Take a hypothetical utility-box lid, 2.5 mm wall, that sits flat on top of a post in full sun. Two versions are on the table.

Version A, black polypropylene. The molder colors natural PP with a black masterbatch. If the masterbatch carries 40% carbon black and the target in the part is 2.5% carbon black (the top of the 2 to 2.5% range carbon-black makers give as optimum), the let-down is 2.5 ÷ 40 = 6.25% masterbatch by weight. That's well above a typical color-only dose, so it has to be written down; a molder told only "black" may run a lower dose that looks just as black but protects far less. Add a HALS-stabilized base grade and the lid has two independent layers of protection.

Version B, mid gray. A UV-level carbon-black loading (2 to 2.5%) is off the table for a mid-gray part, so the protection has to come from the resin and the stabilizer package. ABS would be the wrong call here: its butadiene phase is the known weak spot. ASA in the same gray is the straightforward swap. But check heat: a dark or mid-gray lid in direct sun runs hot, and standard ASA's heat deflection temperature of roughly 75 to 95 °C at 1.82 MPa leaves less margin than you might assume for a part carrying a load or a snap-fit preload. If the lid also has to survive a hard impact in cold weather, a UV-stabilized polycarbonate or a PC blend may be worth the extra material cost; run the thermal expansion calculator too, because a long lid that heats and cools every day moves more than people expect against a metal frame.

The decision comes down to color. If the brand can live with black, black PP or PE with the right loading of fine carbon black is hard to beat. If it can't, you're buying weathering through resin choice and additives, and you should test.

Testing: what G154 and G155 can and can't tell you

Two accelerated methods cover most plastic parts. ASTM G154 uses fluorescent UV lamps; the UVA-340 lamp it specifies in several cycles most closely matches the short-wave UV in noon summer sunlight. Most G154 cycles alternate 4 or 8 h of light, typically at 60 °C, with 4 h of dark condensation at 50 °C, so the samples get both UV and wet surfaces. ASTM G155 uses filtered xenon-arc lamps, which reproduce the full sunlight spectrum including visible light, and is the better choice when color fade is the main question.

Both are practices for running the equipment, not pass-fail specifications. Neither defines how many hours equal a year outdoors, and no honest lab will give you a single conversion factor. What they do well is rank: run your candidate grade and a known-good reference side by side, measure color change (ΔE), gloss and impact retention at intervals, and compare. If you need an hours number on a drawing, agree the test cycle, the hours and the property limits with the resin supplier first.

What goes wrong in practice

Decision checklist

  1. How much direct sun does the part get: full exposure, partial shade, or behind glass?
  2. Can the part be black or dark? If yes, specify carbon black type and loading.
  3. Is it clear or translucent? Then it needs a UV-absorber grade, and probably a coating.
  4. What else does it touch outdoors: salt spray, fuel, sunscreen, fertilizer, acidic cleaners?
  5. What's the thinnest load-bearing feature, and what happens if it cracks?
  6. Which test (G154 or G155, which cycle, how many hours) and which pass limits (ΔE, gloss, impact retained) will you use to compare candidates?
  7. Is the exact grade, color and colorant supplier written on the drawing?

When the answer changes

If the part lives under a cover, behind tinted glass, or is replaced every season, a standard ABS or PP may be perfectly adequate, and the stabilized grade is wasted spend. If the part is in salt air on a boat, UV is only one of several attacks; our marine and boat parts page covers corrosion, water and hardware choices. And if the part has to carry a flame rating as well, the UV and flame-retardant packages have to coexist in one grade, which narrows the options to grades that list both.

Common questions

Is ABS OK for outdoor use?

Not unprotected in direct sun. The polybutadiene rubber that makes ABS tough contains double bonds that react with UV and oxygen, so it fades and turns brittle. It works outdoors if it is painted, capped with an ASA layer, or kept under a cover. For an exposed molded part, ASA is the usual drop-in swap.

Does black plastic really last longer in the sun?

Usually, if the black is carbon black at the right loading. Carbon black screens UV at the surface and slows oxidation. Carbon-black makers give about 2 to 2.5% of a fine-particle black as the optimum loading for polyethylene. A black made from a small dose of colorant may look the same but protect much less.

How many hours of QUV testing equal one year outdoors?

There is no fixed conversion, and ASTM G154 and G155 do not claim one. Climate, part color, orientation and the property you measure all change the answer. Use the tests to rank a candidate against a reference material that has a known outdoor record, and agree pass limits for color change, gloss and impact retention.

Can I use HALS in polycarbonate?

Stabilizer suppliers advise against it. Most HALS (N-H and N-R types) are basic amine compounds, and in polycarbonate they accelerate hydrolysis, which cuts molecular weight and toughness. Polycarbonate grades for outdoor use rely on UV absorbers such as benzotriazole or hydroxyphenyl-triazine types instead, and clear glazing often adds a hard coat as well.

Will a UV-stabilized grade stop the color from fading?

It slows damage to the polymer, but color fade also depends on the pigments. Some organic pigments fade quickly in sunlight even in a well-stabilized resin. Ask the color supplier for light-fastness data on the specific pigments in your color, and test the colored part, not a natural plaque.

Sources

Send the part file and the quantity you expect to run, and we'll review it before you commit to tooling. NDA first if you want one.

Send a part for reviewBook a 30-minute call